    • 2. 发明授权
    • Method for producing an (meth)acrylate syrup
    • (甲基)丙烯酸酯糖浆的制造方法
    • US07700704B2
    • 2010-04-20
    • US11268734
    • 2005-11-08
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • C08F12/00
    • C08F220/14
    • The present invention provides a method for producing an (meth)acrylate syrup by bulk polymerization which is characterized by: a) using (meth)acrylate ester monomer; and b) using 2,4-diphenyl-4methyl-1-pentenol singly or together with a thiol chain transfer agent as a chain transfer agent, c) initiating polymerization by adding an initiator having the half-life of up to 30 minutes at 55-80° C. of initial reaction temperature, so as to maintain the peak reactor temperature below 95° C. and the reactor conversion rate as 5-50 weight %. The method for producing an (meth)acrylate syrup of the present invention has such advantages that reaction runaway does not occur, the control of molecular weight and conversion rate is possible even at low exothermic temperature without stirring failure, and a partially polymerized (meth)acrylate syrup can also be prepared therefrom.
    • 本发明提供通过本体聚合制备(甲基)丙烯酸酯糖浆的方法,其特征在于:a)使用(甲基)丙烯酸酯单体; 和b)使用2,4-二苯基-4-甲基-1-戊烯醇单独或与硫醇链转移剂一起作为链转移剂,c)通过在55℃下加入具有长达30分钟的半衰期的引发剂来引发聚合 -80℃的初始反应温度,以保持峰值反应器温度低于95℃,反应器转化率为5-50重量%。 本发明的(甲基)丙烯酸酯浆料的制造方法具有不发生反应失控的优点,即使在没有搅拌失效的低放热温度下也可以控制分子量和转化率,部分聚合的(甲基) 丙烯酸酯糖浆也可以由其制备。
    • 4. 发明申请
    • Method for producing an (meth)acrylate syrup
    • (甲基)丙烯酸酯糖浆的制造方法
    • US20060100407A1
    • 2006-05-11
    • US11268734
    • 2005-11-08
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • C08F118/02
    • C08F220/14
    • The present invention provides a method for producing an (meth)acrylate syrup by bulk polymerization which is characterized by: a) using (meth)acrylate ester monomer; and b) using 2,4-diphenyl-4methyl-1-pentenol singly or together with a thiol chain transfer agent as a chain transfer agent, c) initiating polymerization by adding an initiator having the half-life of up to 30 minutes at 55-80° C. of initial reaction temperature, so as to maintain the peak reactor temperature below 95° C. and the reactor conversion rate as 5-50 weight %. The method for producing an (meth)acrylate syrup of the present invention has such advantages that reaction runaway does not occur, the control of molecular weight and conversion rate is possible even at low exothermic temperature without stirring failure, and a partially polymerized (meth)acrylate syrup can also be prepared therefrom.
    • 本发明提供通过本体聚合制备(甲基)丙烯酸酯糖浆的方法,其特征在于:a)使用(甲基)丙烯酸酯单体; 和b)使用2,4-二苯基-4-甲基-1-戊烯醇单独或与硫醇链转移剂一起作为链转移剂,c)通过在55℃下加入具有长达30分钟的半衰期的引发剂来引发聚合 -80℃的初始反应温度,以保持峰值反应器温度低于95℃,反应器转化率为5-50重量%。 本发明的(甲基)丙烯酸酯浆料的制造方法具有不发生反应失控的优点,即使在没有搅拌失效的低放热温度下也可以控制分子量和转化率,部分聚合的(甲基) 丙烯酸酯糖浆也可以由其制备。
    • 5. 发明授权
    • Method for producing acryl syrup by bulk polymerization
    • 通过本体聚合制备丙烯酸树脂浆的方法
    • US07807767B2
    • 2010-10-05
    • US12232459
    • 2008-09-17
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • C08F12/00
    • C08F220/14
    • The present invention provides a method for producing acryl syrup by bulk polymerization, comprising a step of preparing a mixture comprising monomer component and 2,4-diphenyl-4methyl-1-pentene; a step of heating the mixture to the initial reaction temperature; and a step of adding an polymerization initiator having the half-life of not more than 30 minutes at 5-80° C., wherein the initial reaction temperature is controlled so that the polymerization initiator has the half-life of up to 30 minutes. The method of the present invention has such advantages that reaction runaway does not occur, the control of molecular weight and conversion rate is possible even at low exothermic temperature, and a partially polymerized acryl syrup can also be prepared therefrom.
    • 本发明提供了通过本体聚合制备丙烯酸树脂浆的方法,包括制备包含单体组分和2,4-二苯基-4-甲基-1-戊烯的混合物的步骤; 将混合物加热至初始反应温度的步骤; 以及在5-80℃下加入半衰期不超过30分钟的聚合引发剂的步骤,其中控制初始反应温度,使得聚合引发剂的半衰期长达30分钟。 本发明的方法具有不发生反应失控的优点,即使在低放热温度下也可以控制分子量和转化率,也可以由其制备部分聚合的丙烯酸树脂浆。
    • 6. 发明申请
    • Method for producing acryl syrup by bulk polymerization
    • 通过本体聚合制备丙烯酸树脂浆的方法
    • US20090018259A1
    • 2009-01-15
    • US12232459
    • 2008-09-17
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • No-ma KimJae-gwan LeeSuk-ky Chang
    • C08L33/12
    • C08F220/14
    • The present invention provides a method for producing acryl syrup by bulk polymerization, comprising a step of preparing a mixture comprising monomer component and 2,4-diphenyl-4methyl-1-pentene; a step of heating the mixture to the initial reaction temperature; and a step of adding an polymerization initiator having the half-life of not more than 30 minutes at 5-80° C., wherein the initial reaction temperature is controlled so that the polymerization initiator has the half-life of up to 30 minutes. The method of the present invention has such advantages that reaction runaway does not occur, the control of molecular weight and conversion rate is possible even at low exothermic temperature, and a partially polymerized acryl syrup can also be prepared therefrom.
    • 本发明提供了通过本体聚合制备丙烯酸树脂浆的方法,包括制备包含单体组分和2,4-二苯基-4-甲基-1-戊烯的混合物的步骤; 将混合物加热至初始反应温度的步骤; 以及在5-80℃下加入半衰期不超过30分钟的聚合引发剂的步骤,其中控制初始反应温度,使得聚合引发剂的半衰期长达30分钟。 本发明的方法具有不发生反应失控的优点,即使在低放热温度下也可以控制分子量和转化率,也可以由其制备部分聚合的丙烯酸树脂浆。