    • 6. 发明授权
    • Toner for developing electrostatic latent image and image forming method using the same
    • 用于显影静电潜像的调色剂和使用其的图像形成方法
    • US07575840B2
    • 2009-08-18
    • US11396389
    • 2006-03-31
    • Kouzou TeramotoYukinori NakayamaKousuke SatouHiroshi Mizuhata
    • Kouzou TeramotoYukinori NakayamaKousuke SatouHiroshi Mizuhata
    • G03G9/00
    • G03G9/0835G03G9/0837G03G9/0838
    • The toner of the present invention is characterized in that the charges rise up rapidly, the charge quantity is not insufficient nor excessive, the photoreceptor contamination is minimized and the toner is endurable under harsh conditions and against the high stress usage. The magnetic particle contained in the toner is of average particle size 0.01 μm through 0.50 μm, is of octahedron shape that is a convex polyhedron surrounded by eight triangles as a basis, each of vertexes and edges of the octahedron being in a curved surface shape and having a portion that can be taken as a straight line on the outer periphery of a projected image of said octahedron. The sphericity of the toner is 0.94 through 0.98. Here, the sphericity is defined by C2/C1, where C1 is a circumferential length of an image projected on a plane and C2 is a circumferential length of an assumed circle area as same as that of the projected image. Further, a number content of the toner of particle size 0.6 μm through 2.0 μm is smaller than 10%.
    • 本发明的调色剂的特征在于,电荷迅速上升,电荷量不足也不过量,感光体污染最小化,并且调色剂在恶劣条件下耐受并且抵抗高应力使用。 包含在调色剂中的磁性颗粒的平均粒度为0.01μm至0.50μm,为八面体形状,是以8个三角形围绕的凸面多面体为基准,八面体的顶点和边缘为曲面形状, 具有可以被视为所述八面体的投影图像的外周上的直线的部分。 调色剂的球形度为0.94至0.98。 这里,球形度由C2 / C1定义,其中C1是投影在平面上的图像的圆周长度,C2是与投影图像相同的假定圆形区域的圆周长度。 此外,粒径为0.6μm至2.0μm的调色剂的数量少于10%。
    • 7. 发明申请
    • Magnetic toner for two-component developer and image forming method using the developer
    • 用于双组分显影剂的磁性调色剂和使用显影剂的成像方法
    • US20060222983A1
    • 2006-10-05
    • US11394349
    • 2006-03-30
    • Yukinori NakayamaKousuke SatouKouzou TeramotoHiroshi Mizuhata
    • Yukinori NakayamaKousuke SatouKouzou TeramotoHiroshi Mizuhata
    • G03G9/083
    • G03G9/0835G03G9/0837G03G9/0838
    • The object is to provide a magnetic toner with which toner scattering, toner spent to carrier, development of scratch streaks by the magnetic brush on the photoreceptor drum can be prevented for a prolonged period and a good image characteristic (in image density and background fogging) can be maintained for a prolonged period, and an image forming method using the magnetic toner. A two-component developer comprising carriers and toner which contains magnetic particle at least in a binder resin thereof, the magnetic particle being of basically polyhedral shaped shape, vertexes and edges of said polyhedral shape being curved surfaces, said shape having peripheral parts taken as straight lines in a projected image thereof, saturation magnetization of said toner in a magnetic field of 79.6 kA/m being 4.0 to 15.0 Am2/kg, is prepared, and the toner retaining members (carriers) bearing at least said magnetic toner to which electric charge is injected are allowed to face a latent image retaining member and an electrostatic latent image on said latent image retaining member is developed with said magnetic toner.
    • 本发明的目的是提供一种磁性调色剂,其中调色剂飞散,用于载体的调色剂,感光鼓上的磁刷产生刮痕,可以延长时间并且具有良好的图像特性(图像浓度和背景雾化) 可以维持较长时间,以及使用该磁性调色剂的图像形成方法。 至少在其粘合剂树脂中含有磁性颗粒的载体和调色剂的双组分显影剂,所述磁性颗粒基本上是多面体形状,所述多面体形状的顶点和边缘是曲面,所述形状具有周边部分 在其投影图像中的线,在79.6kA / m的磁场中的所述调色剂的饱和磁化强度为4.0至15.0Am 2 / kg,并且调色剂保持构件(载体)承载于 允许注入电荷的至少所述磁性调色剂面对潜像保持部件,并且利用所述磁性调色剂使所述潜像保持部件上的静电潜像显影。
    • 10. 发明申请
    • Magnetic toner for two component developer and image forming method using the same
    • 用于双组分显影剂的磁性调色剂和使用其的成像方法
    • US20060216622A1
    • 2006-09-28
    • US11376623
    • 2006-03-15
    • Yukinori NakayamaKouzou TeramotoKousuke SatouHiroshi Mizuhata
    • Yukinori NakayamaKouzou TeramotoKousuke SatouHiroshi Mizuhata
    • G03G9/083
    • G03G9/0837G03G9/0819G03G9/0827G03G9/0835G03G9/0838
    • The two component developer comprises magnetic toners and the magnetic carriers which forms magnetic ears on the surface of the developing roller. The magnetic toner is of an average particle size 0.01 μm through 0.50 μm and is of octahedron shape that is a convex polyhedron surrounded by eight triangles as a basis, each of the vertexes and edges of the octahedron shape toner being in a curved surface shape and having a portion that can be taken as a straight line on the outer periphery of a projected image of the octahedron shape toner. The magnetic ears are electrically charged by the friction between the magnetic toner and the magnetic carriers and the magnetic ears on the developing roller are carried to the electrostatic latent image on the photoreceptor. The latent image is developed by the magnetic toners in the magnetic ears, in a small gap between the developing roller and the photoreceptor. Due to the two component developer, the toner charges are rapidly induced and moreover the toners are not excessively charged.
    • 双组分显影剂包括磁性调色剂和在显影辊表面上形成磁耳的磁性载体。 磁性调色剂的平均粒径为0.01μm至0.50μm,为八面体形状,是由八个三角形围绕的凸多面体的基础,八面体形状调色剂的顶点和边缘为曲面形状, 具有可以在八面体形状调色剂的投影图像的外周上被视为直线的部分。 磁性耳朵由磁性调色剂和磁性载体之间的摩擦带电,并且显影辊上的磁耳被承载在感光体上的静电潜像上。 潜影由磁性耳朵中的磁性调色剂在显影辊和感光体之间的小间隙中显影。 由于双组分显影剂,调色剂电荷迅速诱导,而且调色剂不会过度充电。