    • 3. 发明授权
    • Iron-based sintered powder metal body, manufacturing method thereof and manufacturing method of iron-based sintered component with high strength and high density
    • 铁基烧结粉末金属体及其制造方法以及高强度,高密度的铁基烧结体的制造方法
    • US06514307B2
    • 2003-02-04
    • US09934428
    • 2001-08-21
    • Naomichi NakamuraSatoshi UenosonoShigeru UnamiMasashi FujinagaTakashi YoshimuraMitsumasa IijimaShin KoizumiHiroyuki AnmaYasuo Hatai
    • Naomichi NakamuraSatoshi UenosonoShigeru UnamiMasashi FujinagaTakashi YoshimuraMitsumasa IijimaShin KoizumiHiroyuki AnmaYasuo Hatai
    • C22C3302
    • C22C33/0264B22F3/1007B22F2998/10B22F2999/00C22C33/02B22F3/02B22F3/10C22C33/0207B22F1/0096
    • An sintered iron-based powder metal body with outstandingly lower re-compacting load and having a high density and a method of manufacturing an iron-based sintered component with fewer pores of a sharp shape and having high strength and high density, the method comprising mixing, an iron-based metal powder containing at most about 0.05% of carbon, at most about 0.3% of oxygen, at most about 0.010% of nitrogen, with at least about 0.03% and at most about 0.5% of graphite powder and a lubricant, preliminarily compacting the mixture into a preform, the density of which is about 7.3 Mg/m3 or more, and preliminarily sintering the preform in a non-oxidizing atmosphere in which a partial pressure of nitrogen is about 30 kPa or less at a temperature of about 1000° C. or higher and about 1300° C. or lower, thereby forming a sintered iron-based powder metal body with outstandingly lower re-compacting load and having high deformability, the density of which is about 7.3 Mg/m3 or more and which contains at least about 0.10% and at most about 0.50 of carbon, at most about 0.010% of oxygen and at most about 0.010% of nitrogen, and which comprises at most about 0.02% of free carbon, and, further applying re-compaction and re-sintering and/or heat treatment thereby forming a sintered component, as well as the method alternatively comprising applying preliminary sintering in an atmosphere with no restriction of the nitrogen partial pressure and then annealing instead of the sintering step, thereby obtaining a sintered iron-based powder metal body with the nitrogen content of at most about 0.010%.
    • 一种烧结铁基粉末金属体,具有显着降低的再压实载荷并具有高密度,并且制造具有较少的尖锐形状的孔并具有高强度和高密度的铁基烧结组分的方法,该方法包括混合 ,含有最多约0.05%的碳,至多约0.3%的氧,至多约0.010%的氮,至少约0.03%和至多约0.5%的石墨粉末和润滑剂的铁基金属粉末, 将混合物预先压实成预制件,其密度为约7.3Mg / m 3以上,并且在约10分钟的温度下在氮气分压为约30kPa以下的非氧化性气氛中预先烧结预成型体 1000℃以上约1300℃以下,从而形成烧结的铁基粉末金属体,具有显着降低的再压缩载荷,并具有高变形能力,其密度为约7.3Mg / m 3以上, 其中 至少约0.10%,至多约0.50碳,至多约0.010%的氧和至多约0.010%的氮,并且其包含至多约0.02%的游离碳,并且进一步应用再压实和 再烧结和/或热处理,从而形成烧结组分,以及所述方法或者包括在不限制氮分压的气氛中进行初步烧结,然后退火而不是烧结步骤,由此获得烧结的铁 - 含氮量最多为0.010%的粉末金属体。