会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 5. 发明申请
    • METHOD OF MANUFACTURING MAGNETIC RECORDING MEDIUM AND MAGNETIC RECORDING MEDIUM MANUFACTURED BY THE SAME
    • 制造磁记录介质的方法和由其制造的磁记录介质
    • US20090092857A1
    • 2009-04-09
    • US12244556
    • 2008-10-02
    • Ayako MATSUMOTOSatoshi Matsubaguchi
    • Ayako MATSUMOTOSatoshi Matsubaguchi
    • G11B5/842G11B5/68
    • G11B5/70G11B5/70678G11B5/714G11B5/842G11B5/845
    • The present invention relates to a method of manufacturing a magnetic recording medium comprising coating a magnetic layer coating liquid comprising a ferromagnetic hexagonal ferrite powder and a binder to form a coating film, subjecting the coating film to orientation processing while the coating film is still wet, and drying the coating film to form a magnetic layer. The magnetic layer coating liquid is prepared by subjecting a ferromagnetic hexagonal ferrite powder with an average plate diameter of 10 to 50 nm to a dry comminution step, subjecting the ferromagnetic hexagonal ferrite powder to a first dispersion step together with a binder to prepare a dispersion liquid, and sequentially subjecting the dispersion liquid obtained to a second dispersion step and a filtering step. The dispersion liquid obtained by the first dispersion step comprises a dry solid component in an amount, as measured after filtration, of 15 percent or less.
    • 磁记录介质的制造方法技术领域本发明涉及一种磁记录介质的制造方法,其特征在于,包括含有铁磁性六角铁氧体粉末和粘合剂的磁性层涂布液,形成涂膜,在涂膜仍然是湿的同时对涂膜进行取向处理, 并干燥涂膜以形成磁性层。 通过对平均板直径为10〜50nm的铁磁性六方晶系铁氧体粉末进行干式粉碎步骤,将铁磁六方铁氧体粉末与粘合剂一起进行第一分散工序,制备磁性层涂布液,制备分散液 依次对得到的分散液进行第二分散工序和过滤工序。 通过第一分散步骤获得的分散液含有在过滤后测得的干固体成分为15%或更低的量。
    • 7. 发明授权
    • Magnetic recording medium
    • 磁记录介质
    • US07005203B2
    • 2006-02-28
    • US10653932
    • 2003-09-04
    • Satoshi MatsubaguchiYuichiro Murayama
    • Satoshi MatsubaguchiYuichiro Murayama
    • G11B5/702
    • G11B5/7021G11B5/70G11B5/7023G11B5/725
    • Provided is a magnetic recording medium that exhibits excellent electromagnetic characteristics especially in recording and reproducing systems using an MR head, as well as has excellent long-term preservation property. The magnetic recording medium comprises a lower layer comprising a nonmagnetic powder or a ferromagnetic powder and a binder and at least one magnetic layer thereover comprising a ferromagnetic powder and a binder on a support. Said binder comprised in the lower layer and/or magnetic layer comprises a polyurethane, said polyurethane is polyurethane (1) prepared from a chain extending agent, an organic diisocyanate, and a polyester polyol which comprises a dibasic acid component and a diol component, wherein the dibasic acid component comprises an aliphatic dibasic acid component and 70 molar percent or more of the diol component is derived from a diol having an alkyl branched side chain comprising two or more carbon atoms without a ring structure, or said polyurethane is polyurethane (2) prepared from a chain extending agent which comprises an alkyl branched aliphatic diol comprising three or more of total carbon atoms in a branched side chain per molecule, an organic diisocyanate, and a polyester polyol which comprises a dibasic acid component and a diol component, wherein the dibasic acid component comprises an aliphatic dibasic acid component and 70 molar percent or more of the diol component is derived from an alkyl branched aliphatic diol having a branched side chain of which total carbon atoms per molecule is two or more, and magnitude of saturation magnetic flux density (φm) ranges from 150 to 400 G·μm.
    • 提供了一种磁记录介质,其特别是在使用MR磁头的记录和再现系统中具有优异的电磁特性,并且具有优异的长期保存性能。 磁记录介质包括由非磁性粉末或铁磁性粉末和粘结剂构成的下层,以及至少一个包含铁磁粉末和载体上的粘合剂的磁性层。 包含在下层和/或磁性层中的所述粘合剂包括聚氨酯,所述聚氨酯是由链增长剂,有机二异氰酸酯和包含二元酸组分和二醇组分的聚酯多元醇制备的聚氨酯(1),其中 二元酸组分包含脂族二元酸组分,并且70摩尔%或更多的二醇组分衍生自具有烷基支链侧链的二醇,其具有两个或多个没有环结构的碳原子,或者所述聚氨酯是聚氨酯(2) 由包含分子中支链侧链中总共碳原子数三个以上的烷基支链脂肪族二醇,有机二异氰酸酯和含有二元酸成分和二醇成分的聚酯多元醇构成的链延长剂制备,其中, 二元酸组分包含脂族二元酸组分,70摩尔%或更多的二元醇组分衍生自fr 具有每分子总碳原子数为2以上的支链侧链的烷基支链脂族二醇,饱和磁通密度(phim)的量级为150〜400Ggm。
    • 8. 发明授权
    • Magnetic recording medium
    • 磁记录介质
    • US5908683A
    • 1999-06-01
    • US844388
    • 1997-04-18
    • Masaki SuzukiHiroo InabaSatoshi MatsubaguchiHiroaki Takano
    • Masaki SuzukiHiroo InabaSatoshi MatsubaguchiHiroaki Takano
    • G11B5/70G11B5/733G11B5/738G11B5/708
    • G11B5/70G11B5/733G11B5/738Y10S428/90Y10T428/256Y10T428/257Y10T428/265
    • A magnetic recording medium comprises a non-magnetic substrate, a lower coating layer, which is overlaid upon the non-magnetic substrate and primarily contains a binder and inorganic particles dispersed in the binder, and a magnetic layer, which is overlaid upon the lower coating layer and is constituted of at least a single layer. The magnetic layer contains at least a binder and ferromagnetic metal particles dispersed in the binder. The thickness of the magnetic layer falls within the range of 0.05 .mu.m to 0.5 .mu.m. The surface roughness of a top magnetic layer is at most 3 nm. The lower coating layer contains a fatty acid. An increase in the number of small protrusions, which have a height of at least 30 nm, does not occur substantially on the surface of the magnetic layer after the magnetic recording medium has been stored for seven days under environmental conditions of a temperature of 60.degree. C. and a relative humidity of 90%.
    • 磁记录介质包括非磁性基底,下涂层,其覆盖在非磁性基底上并且主要包含分散在粘合剂中的粘合剂和无机颗粒以及覆盖在下涂层上的磁性层 层,并且由至少单层构成。 磁性层至少包含粘合剂和分散在粘合剂中的强磁性金属颗粒。 磁性层的厚度在0.05μm〜0.5μm的范围内。 顶层磁性层的表面粗糙度为3nm以下。 下涂层含有脂肪酸。 在磁记录介质已经在温度为60°的环境条件下储存了七天之后,磁性层的表面上基本上没有出现高度至少为30nm的小突起的数量的增加。 C.相对湿度为90%。