    • 1. 发明申请
    • COATED SUBSTRATES AND PACKAGES PREPARED THEREFROM
    • 涂层基材和其制备的包装
    • US20120094563A1
    • 2012-04-19
    • US13377917
    • 2010-07-16
    • Maria Isabel Arroyo VillanAngels DomenechKarl Zuercher
    • Maria Isabel Arroyo VillanAngels DomenechKarl Zuercher
    • B32B5/02
    • B32B27/12B32B5/022B32B5/024B32B7/02B32B7/12B32B27/08B32B27/32B32B2262/0253B32B2270/00B32B2307/30B32B2307/31B32B2307/50B32B2307/558B32B2307/72B32B2307/7246B32B2439/06B32B2439/46Y10T442/20
    • The invention provides a coated substrate comprising at least the following: i) a first layer formed from a first composition that has a melting point, Tm1, and comprising at least one ethylene-based interpolymer; ii) a second layer formed from a second composition comprising the following: a) at least one propylene-based polymer, and b) at least one ethylene-based polymer, and iii) a woven web formed from at least one olefin-based polymer with a melting point of Tm2a and/a or nonwoven web formed from at least one olefin-based polymer with a melting point of Tm2b; and wherein and Tm1 is less than, or equal to, “Tm2a −20° C.”, and/or less than, or equal to, “Tm2b −20° C.” The invention also provides a coated substrate comprising at least the following: i) a first layer is formed from a first composition that has a melting point, Tm1; and ii) a woven web formed from at least one olefin-based polymer with a melting point of Tm2a and/or a nonwoven web formed from at least one olefin-based polymer with a melting point of Tm2b; and wherein and the first composition comprises at least one propylene-based polymer with a MFR from 15 to 35 g/10 min, and wherein Tm1 is less than, or equal to, “Tm2a −20° C.”, and/or less than, or equal to, “Tm2b −20° C.”
    • 本发明提供了至少包括以下的涂层基材:i)由具有熔点Tm1并且包含至少一种基于乙烯的互聚物的第一组合物形成的第一层; ii)由第二组合物形成的第二层,所述第二组合物包含以下物质:a)至少一种基于丙烯的聚合物,和b)至少一种基于乙烯的聚合物,和iii)由至少一种基于烯烃的聚合物 熔点为Tm2a和/ a或由至少一种熔点为Tm2b的烯烃基聚合物形成的非织造纤维网; 并且其中和Tm1小于或等于“Tm2a -20℃”和/或小于或等于“Tm2b -20℃”。本发明还提供一种涂覆基材,其包含至少 以下:i)第一层由熔点为Tm1的第一组合物形成; 和ii)由至少一种熔点为Tm2a的烯烃基聚合物和/或由至少一种熔点为Tm2b的烯烃基聚合物形成的非织造纤维网形成的织造网; 并且其中第一组合物包含至少一种MFR为15-35g / 10min的基于丙烯的聚合物,其中Tm1小于或等于“Tm2a -20℃”和/或更少 大于或等于“Tm2b -20℃”
    • 2. 发明授权
    • Coated substrates and packages prepared therefrom
    • 涂布的基材和包装
    • US09162430B2
    • 2015-10-20
    • US13377917
    • 2010-07-16
    • Maria Isabel Arroyo VillanAngels DomenechKarl Zuercher
    • Maria Isabel Arroyo VillanAngels DomenechKarl Zuercher
    • B32B3/00B32B27/32B32B27/04B32B27/12B32B7/02
    • B32B27/12B32B5/022B32B5/024B32B7/02B32B7/12B32B27/08B32B27/32B32B2262/0253B32B2270/00B32B2307/30B32B2307/31B32B2307/50B32B2307/558B32B2307/72B32B2307/7246B32B2439/06B32B2439/46Y10T442/20
    • The invention provides a coated substrate comprising at least the following: i) a first layer formed from a first composition that has a melting point, Tm1, and comprising at least one ethylene-based interpolymer; ii) a second layer formed from a second composition comprising the following: a) at least one propylene-based polymer, and b) at least one ethylene-based polymer, and iii) a woven web formed from at least one olefin-based polymer with a melting point of Tm2a and/a or nonwoven web formed from at least one olefin-based polymer with a melting point of Tm2b; and wherein and Tm1 is less than, or equal to, “Tm2a −20° C.”, and/or less than, or equal to, “Tm2b −20° C.” The invention also provides a coated substrate comprising at least the following: i) a first layer is formed from a first composition that has a melting point, Tm1; and ii) a woven web formed from at least one olefin-based polymer with a melting point of Tm2a and/or a nonwoven web formed from at least one olefin-based polymer with a melting point of Tm2b; and wherein and the first composition comprises at least one propylene-based polymer with a MFR from 15 to 35 g/10 min, and wherein Tm1 is less than, or equal to, “Tm2a −20° C.”, and/or less than, or equal to, “Tm2b −20° C.”
    • 本发明提供了至少包括以下的涂层基材:i)由具有熔点Tm1并且包含至少一种基于乙烯的互聚物的第一组合物形成的第一层; ii)由第二组合物形成的第二层,所述第二组合物包含以下物质:a)至少一种基于丙烯的聚合物,和b)至少一种基于乙烯的聚合物,和iii)由至少一种基于烯烃的聚合物 熔点为Tm2a和/ a或由至少一种熔点为Tm2b的烯烃基聚合物形成的非织造纤维网; 并且其中和Tm1小于或等于“Tm2a -20℃”和/或小于或等于“Tm2b -20℃”。本发明还提供一种涂覆基材,其包含至少 以下:i)第一层由熔点为Tm1的第一组合物形成; 和ii)由至少一种熔点为Tm2a的烯烃基聚合物和/或由至少一种熔点为Tm2b的烯烃基聚合物形成的非织造纤维网形成的织造网; 并且其中第一组合物包含至少一种MFR为15-35g / 10min的基于丙烯的聚合物,其中Tm1小于或等于“Tm2a -20℃”和/或更少 大于或等于“Tm2b -20℃”
    • 9. 发明授权
    • Medium density ethylene polymers, a process to prepare these polymers and use of carbonyl group containing chain transfer agents in this process
    • 中密度乙烯聚合物,在这个过程中制备这些聚合物的方法和使用含羰基的链转移剂
    • US06407191B1
    • 2002-06-18
    • US09600093
    • 2000-11-20
    • Juan Manuel MezquitaKarl ZuercherRonald Wevers
    • Juan Manuel MezquitaKarl ZuercherRonald Wevers
    • C08F428
    • C08F10/02C08F110/02C08F2/00C08F4/32C08F2/38C08F2500/08C08F2500/12C08F2500/26
    • The present invention relates to an ethylene homo or copolymer having a density of between 0.923 and 0.935 g/cm3, having a molecular weight distribution Mw/Mn of between 3 and 10, and comprising from 0.10 to 0.50 wt. percent of units derived from a carbonyl group containing compound, based on the total weight of the homo or copolymer. In addition, the invention relates to a free radical initiation polymerization process for the preparation of medium density ethylene polymers or copolymers, comprising reacting ethylene and optionally one or more comonomers at a high pressure, conveniently between 1600 and 4000 kg/cm2, and at temperatures of about 150-330° C. in a reactor system consisting of at least one autoclave reactor or of a combination of autoclave and tubular reactors, in the presence of free radical initiators and a carbonyl group containing compound. Finally, the invention relates to carbonyl group containing chain transfer agents to obtain improved polymer processing and performance properties in flat die extrusion processes and applications.
    • 本发明涉及密度为0.923至0.935g / cm3的乙烯均聚物或共聚物,其分子量分布Mw / Mn为3-10,并包含0.10至0.50wt。 基于含羰基化合物衍生的单元的百分比,基于均聚物或共聚物的总重量。 此外,本发明涉及用于制备中等密度乙烯聚合物或共聚物的自由基引发聚合方法,包括使乙烯和任选的一种或多种共聚单体在高压下,方便地在1600至4000kg / cm2之间和在温度 在由至少一个高压釜反应器或高压釜和管式反应器的组合组成的反应器系统中,在存在自由基引发剂和含羰基化合物的情况下为约150-330℃。 最后,本发明涉及含羰基的链转移剂,以获得改进的聚合物加工和在平模挤出工艺和应用中的性能。