    • The invention relates to an austenitic nickel-chromium-molybdenum alloy having high resistance to general corrosion, crevice, pitting and stress crack corrosion and also intercrystalline corrosion, consisting of (in % by weight):carbon: up to 0.01%silicon: up to 0.05%manganese: up to 0.50%phosphorus: up to 0.020%sulphur: up to 0.010%chromium: 14.0 to 18.0%molybdenum: 14.0 to 18.0%cobalt: up to 2.0%tungsten: up to 0.5%calcium 0.001 to 0.010%magnesium: 0.001 to 0.020%aluminium: 0.05 to 0.30%nitrogen: up to 0.02%iron: up to 3.0%copper: up to 0.5%titanium: up to 0.01%residue nickel and usual impurities due to melting, the sum of the contents (carbon+silicon+titanium) being limited to 0.05% at the most, and the sum of the elements (calcium+magnesium+aluminium) being adjusted within the limits 0.055 to 0.33%.
    • 本发明涉及一种具有高耐一般腐蚀,缝隙,点蚀和应力裂纹腐蚀以及晶间腐蚀的奥氏体镍铬钼合金,其由(以重量%计)组成:碳:高达0.01%的硅:直至 0.05%锰:高达0.50%的磷:高达0.020%的硫:高达0.010%的铬:14.0至18.0%的钼:14.0至18.0%的钴:至多2.0%的钨:高达0.5%的钙0.001至0.010%的镁 :0.001至0.020%铝:0.05至0.30%氮:至多0.02%铁:至多3.0%铜:至多0.5%钛:至多0.01%残留镍和由于熔化而导致的常见杂质,含量之和( 碳+硅+钛)限制在0.05%以下,元素(钙+镁+铝)之和调整在0.055〜0.33%的范围内。