    • 1. 发明申请
    • Thermoplastic resin composition and resin molded product
    • 热塑性树脂组合物和树脂模塑制品
    • US20110009538A1
    • 2011-01-13
    • US12923341
    • 2010-09-15
    • Makoto NakamuraHiroshi NakanoKiyoji TakagiKouji Iwaki
    • Makoto NakamuraHiroshi NakanoKiyoji TakagiKouji Iwaki
    • C08K3/34C08K5/49C08K5/54
    • C08K9/08C08K3/34C08K5/524C08K9/04C08L55/02C08L67/02C08L69/00C08L2666/02C08L2666/18
    • The present invention relates to a thermoplastic resin composition comprising an aromatic polycarbonate resin (component A) [which may comprise an aromatic polycarbonate resin (component A1) and a thermoplastic resin other than the aromatic polycarbonate resin (component A2)], a granular talc (component B) having a bulk density of 0.4 to 1.5 g/mL which is obtained by granulating a talc having an average particle size of 0.1 to 10 μm, a rubber polymer (component C; optional component), a flame retardant (component E; optional component) and a fluorinated polyolefin (component F; optional component), wherein the granular talc (component B) has a particle size in which a proportion of a 500 μm-mesh screen residue thereof is not less than 55% by weight; as well as a resin molded product obtained by molding the thermoplastic resin composition. The thermoplastic resin composition and the resin molded product are excellent in extrusion moldability, rigidity, flame retardant, impact resistance and thermal stability, and exhibit an excellent balance between these properties.
    • 本发明涉及包含芳族聚碳酸酯树脂(组分A)[其可以包含芳族聚碳酸酯树脂(组分A1)和除芳族聚碳酸酯树脂(组分A2)之外的热塑性树脂)]的热塑性树脂组合物,颗粒滑石( 成分B),其通过造粒平均粒度为0.1〜10μm的滑石,橡胶聚合物(C成分,任意成分),阻燃剂(E成分)而得到的堆积密度为0.4〜1.5g / 任选组分)和氟化聚烯烃(组分F;任选组分),其中所述颗粒滑石(组分B)具有其500μm筛网残余物的比例不小于55重量%的粒径; 以及通过模塑该热塑性树脂组合物获得的树脂模制产品。 热塑性树脂组合物和树脂成型体的挤出成型性,刚性,阻燃性,耐冲击性和热稳定性优异,在这些特性之间表现出极好的平衡。
    • 3. 发明申请
    • THERMOPLASTIC RESIN COMPOSITION AND RESIN MOLDED PRODUCT
    • 热塑性树脂组合物和树脂模制产品
    • US20090215934A1
    • 2009-08-27
    • US12281733
    • 2007-02-28
    • Makoto NakamuraHiroshi NakanoKiyoji TakagiKouji Iwaki
    • Makoto NakamuraHiroshi NakanoKiyoji TakagiKouji Iwaki
    • C08K3/34C08K5/49C08K5/09
    • C08K9/08C08K3/34C08K5/524C08K9/04C08L55/02C08L67/02C08L69/00C08L2666/02C08L2666/18
    • The present invention relates to a thermoplastic resin composition comprising an aromatic polycarbonate resin (component A) [which may comprise an aromatic polycarbonate resin (component A1) and a thermoplastic resin other than the aromatic polycarbonate resin (component A2)], a granular talc (component B) having a bulk density of 0.4 to 1.5 g/mL which is obtained by granulating a talc having an average particle size of 0.1 to 10 μm, a rubber polymer (component C; optional component), a flame retardant (component E; optional component) and a fluorinated polyolefin (component F; optional component), wherein the granular talc (component B) has a particle size in which a proportion of a 500 μm-mesh screen residue thereof is not less than 55% by weight; as well as a resin molded product obtained by molding the thermoplastic resin composition. The thermoplastic resin composition and the resin molded product are excellent in extrusion moldability, rigidity, flame retardant, impact resistance and thermal stability, and exhibit an excellent balance between these properties.
    • 本发明涉及包含芳族聚碳酸酯树脂(组分A)[其可以包含芳族聚碳酸酯树脂(组分A1)和除芳族聚碳酸酯树脂(组分A2)之外的热塑性树脂)]的热塑性树脂组合物,颗粒滑石( 组分B),其通过使平均粒度为0.1〜10微米的滑石粉,橡胶聚合物(组分C,任选的组分),阻燃剂(组分E;成分E)制成,其堆积密度为0.4〜1.5g / 任选的组分)和氟化聚烯烃(组分F;任选组分),其中所述颗粒状滑石(组分B)具有其500μm筛网残余物的比例不小于55重量%的粒径; 以及通过模塑该热塑性树脂组合物获得的树脂模制产品。 热塑性树脂组合物和树脂成型体的挤出成型性,刚性,阻燃性,耐冲击性和热稳定性优异,在这些特性之间表现出极好的平衡。
    • 5. 发明申请
    • Thermoplastic resin composition
    • 热塑性树脂组合物
    • US20070117901A1
    • 2007-05-24
    • US11635798
    • 2006-12-08
    • Masami SuzukiMorio TsunodaHajime OhyamaMakoto NakamuraKiyoji Takagi
    • Masami SuzukiMorio TsunodaHajime OhyamaMakoto NakamuraKiyoji Takagi
    • C08K3/34
    • C08L77/02C08K3/34C08L23/0861C08L29/04C08L53/00C08L53/02C08L53/025C08L77/00C08L77/06C08L2205/02C08L2205/035C08L2666/02C08L2666/04C08L2666/24
    • The present invention relates to a thermoplastic resin composition which excels in impact resistance, dimension stability and rigidity, and also excels in appearance, fluidity and paint film adhesion property, and further which is very useful as manufacturing materials for exterior parts of automobile. A thermoplastic resin composition comprising component (A): a polyamide resin; component (B): a hydrogenated product of block copolymer comprising vinyl aromatic polymer block (a) and conjugated diene based polymer block (b), and/or ethylene-α-olefin based block copolymer; component (C): a modified hydrogenated product of block copolymer comprising the vinyl aromatic polymer block (a) and the conjugated diene based polymer block (b), which hydrogenated product is modified by addition of an unsaturated acid and/or derivative thereof; component (D): a plate-like and/or needle-like inorganic filler; and component (F): an ethylene-vinyl alcohol copolymer and/or a partial saponified product of ethylene-vinyl acetate copolymer.
    • 本发明涉及耐冲击性,尺寸稳定性和刚性优异的外观,流动性和漆膜附着性优异的热塑性树脂组合物,进一步作为汽车用外装件的制造材料非常有用。 一种热塑性树脂组合物,其包含组分(A):聚酰胺树脂; 组分(B):包含乙烯基芳族聚合物嵌段(a)和共轭二烯基聚合物嵌段(b)的嵌段共聚物的氢化产物和/或乙烯-α-烯烃基嵌段共聚物; 组分(C):包含乙烯基芳族聚合物嵌段(a)和共轭二烯基聚合物嵌段(b)的嵌段共聚物的改性氢化产物,该加氢产物通过加入不饱和酸和/或其衍生物进行改性; 组分(D):板状和/或针状无机填料; 和组分(F):乙烯 - 乙烯醇共聚物和/或乙烯 - 乙酸乙烯酯共聚物的部分皂化产物。
    • 6. 发明授权
    • Thermoplastic resin composition
    • 热塑性树脂组合物
    • US08193282B2
    • 2012-06-05
    • US11635798
    • 2006-12-08
    • Masami SuzukiMorio TsunodaHajime OhyamaMakoto NakamuraKiyoji Takagi
    • Masami SuzukiMorio TsunodaHajime OhyamaMakoto NakamuraKiyoji Takagi
    • C08K3/04C08K3/34C08L53/02C08L77/00
    • C08L77/02C08K3/34C08L23/0861C08L29/04C08L53/00C08L53/02C08L53/025C08L77/00C08L77/06C08L2205/02C08L2205/035C08L2666/02C08L2666/04C08L2666/24
    • The present invention relates to a thermoplastic resin composition which excels in impact resistance, dimension stability and rigidity, and also excels in appearance, fluidity and paint film adhesion property, and further which is very useful as manufacturing materials for exterior parts of automobile.A thermoplastic resin composition comprising component (A): a polyamide resin; component (B): a hydrogenated product of block copolymer comprising vinyl aromatic polymer block (a) and conjugated diene based polymer block (b), and/or ethylene-α-olefin based block copolymer; component (C): a modified hydrogenated product of block copolymer comprising the vinyl aromatic polymer block (a) and the conjugated diene based polymer block (b), which hydrogenated product is modified by addition of an unsaturated acid and/or derivative thereof; component (D): a plate-like and/or needle-like inorganic filler; and component (F): an ethylene-vinyl alcohol copolymer and/or a partial saponified product of ethylene-vinyl acetate copolymer.
    • 本发明涉及耐冲击性,尺寸稳定性和刚性优异的外观,流动性和漆膜附着性优异的热塑性树脂组合物,进一步作为汽车外用部件的制造材料非常有用。 一种热塑性树脂组合物,其包含组分(A):聚酰胺树脂; 组分(B):包含乙烯基芳族聚合物嵌段(a)和共轭二烯基聚合物嵌段(b)的嵌段共聚物的氢化产物和/或乙烯-α-烯烃基嵌段共聚物; 组分(C):包含乙烯基芳族聚合物嵌段(a)和共轭二烯基聚合物嵌段(b)的嵌段共聚物的改性氢化产物,该加氢产物通过加入不饱和酸和/或其衍生物进行改性; 组分(D):板状和/或针状无机填料; 和组分(F):乙烯 - 乙烯醇共聚物和/或乙烯 - 乙酸乙烯酯共聚物的部分皂化产物。
    • 9. 发明授权
    • Process for producing amorphous thermoplastic resin composition
    • 无定型热塑性树脂组合物的制造方法
    • US5672679A
    • 1997-09-30
    • US566319
    • 1995-12-01
    • Kiyoji TakagiKoji NishidaMegumi Kojima
    • Kiyoji TakagiKoji NishidaMegumi Kojima
    • B29B7/84C08J3/00C08F6/10
    • C08J3/005B29B7/84C08J3/00
    • In a process for producing an amorphous thermoplastic resin composition comprising melt-kneading at least one amorphous thermoplastic resin, an improvement comprising melt-kneading the amorphous thermoplastic resin in the presence of not less than 1% by weight, based on the amorphous thermoplastic resin, of an organic solvent in a kneader having a vent hole(s) while maintaining at least one vent hole of the kneader under reduced pressure by means of an evacuator to remove the organic solvent so as to reduce the organic solvent content in the final composition to less than 1% by weight. Thermal deterioration of the resin during melt-kneading can be inhibited to provide a resin composition having well-balanced impact resistance and heat resistance and excellent hue.
    • 在制造熔融捏合至少一种无定形热塑性树脂的无定形热塑性树脂组合物的方法中,包括以不小于1重量%的非晶态热塑性树脂的存在下熔融捏合无定形热塑性树脂的改进, 在具有通气孔的捏合机中,通过抽气机在减压下保持捏合机的至少一个通气孔以除去有机溶剂,从而将最终组合物中的有机溶剂含量降低至 小于1重量%。 可以抑制熔融捏合过程中的树脂的热劣化,提供具有良好平衡的耐冲击性和耐热性以及优异的色调的树脂组合物。