    • 2. 发明申请
    • SOLID ELECTROLYTE AND LITHIUM BASED BATTERY USING THE SAME
    • 使用固体电解质和锂离子电池
    • US20130157146A1
    • 2013-06-20
    • US13652807
    • 2012-10-16
    • LI WANGXIANG-MING HEJIAN-JUN LIJIAN GAOCHANG-YIN JIANG
    • LI WANGXIANG-MING HEJIAN-JUN LIJIAN GAOCHANG-YIN JIANG
    • H01M10/0565
    • C08F2/48C08F222/1006C08F2220/286H01M10/052H01M10/0565H01M2300/0082
    • A solid electrolyte includes an interpenetrating polymer network and a lithium salt dispersed in the interpenetrating polymer network. The interpenetrating polymer network includes CH2—CH2OH segments, and is formed by polymerizing a first monomer R1—OCH2—CH2—OHR2, a second monomer R3—OCH2—CH2—OmR4 and an initiator. Each “R1”, “R2” and “R3” includes —C═C— group or —C≡C— group. The “R4” includes an alkyl group or a hydrogen atom. The “m” and “n” are integer. Molecular weights of the first monomer and the second monomer are more than or equal to 100, and less than or equal to 800. The first monomer is less than or equal to 50% of the second monomer by weight. The lithium salt is less than or equal to 10% the second monomer by weight. A lithium based battery using the solid electrolyte is also provided.
    • 固体电解质包括互穿聚合物网络和分散在互穿聚合物网络中的锂盐。 互穿聚合物网络包括CHCH 2 -CH 2 O H H段,并且通过使第一单体R 1 -OCH 2 -CH 2 -OHRR 2,第二单体R 3 -OCH 2 -CH 2 -O·mR 4和引发剂 。 每个“R1”,“R2”和“R3”包括-C = C-基团或-C = C-基团。 “R4”包括烷基或氢原子。 “m”和“n”是整数。 第一单体和第二单体的分子量大于或等于100,小于或等于800.第一单体小于或等于第二单体重量的50%。 该锂盐的重量小于或等于第二单体的10%。 还提供了使用固体电解质的锂基电池。
    • 3. 发明申请
    • SOLID ELECTROLYTE AND LITHIUM BASED BATTERY USING THE SAME
    • 使用固体电解质和锂离子电池
    • US20130157144A1
    • 2013-06-20
    • US13652813
    • 2012-10-16
    • LI WANGXIANG-MING HEJIAN-JUN LIJIAN GAOCHANG-YIN JIANG
    • LI WANGXIANG-MING HEJIAN-JUN LIJIAN GAOCHANG-YIN JIANG
    • H01M10/056H01M10/0565H01M4/40
    • H01M10/0525H01M10/0565H01M10/4235H01M2300/0082H01M2300/0091Y02E60/122
    • A solid electrolyte includes an interpenetrating polymer network, a plasticizer and a lithium salt. The plasticizer and the lithium salt are dispersed in the interpenetrating polymer network. The interpenetrating polymer network includes CH2—CH2—On segments, and is formed by polymerizing a first monomer R1—OCH2—CH2—OnR2 with a second monomer R3—OCH2—CH2—OmR4 under an initiator. The “R1”, “R2” or “R3” respectively includes —C═C— group or —C≡C— group. The “R4” includes an alkyl group or a hydrogen atom. The “m” and “n” are integers. A molecular weight of the first monomer or a molecular weight of the second monomer is greater than or equal to 100, and less than or equal to 800. The first monomer is less than or equal to 50% of the second monomer by weight. The lithium salt is less than or equal to 10% the second monomer by weight. A lithium based battery using the solid electrolyte is also provided.
    • 固体电解质包括互穿聚合物网络,增塑剂和锂盐。 增塑剂和锂盐分散在互穿聚合物网络中。 互穿聚合物网络包括CHCH 2 -CH 2 -O-链段,并且通过将第一单体R 1 -OCH 2 -CH 2 -O·nR 2与第二单体R 3 -OCH 2 -CH 2 -O·mR 4聚合而形成, 一个发起者 “R1”,“R2”或“R3”分别包括-C = C-基团或-C = C-基团。 “R4”包括烷基或氢原子。 “m”和“n”是整数。 第一单体的分子量或第二单体的分子量大于或等于100,小于或等于800.第一单体小于或等于第二单体重量的50%。 该锂盐的重量小于或等于第二单体的10%。 还提供了使用固体电解质的锂基电池。
    • 4. 发明申请
    • METHOD FOR MAKING SOLID ELECTROLYTE
    • 制造固体电解质的方法
    • US20130157145A1
    • 2013-06-20
    • US13652824
    • 2012-10-16
    • LI WANGXIANG-MING HEJIAN-JUN LIJIAN GAOCHANG-YIN JIANG
    • LI WANGXIANG-MING HEJIAN-JUN LIJIAN GAOCHANG-YIN JIANG
    • H01M10/0565
    • C08F2/48C08F222/1006C08F299/024C08F2220/286H01M10/0565H01M2300/0082
    • A method for making a solid electrolyte includes the following steps. A first monomer, a second monomer, an initiator and a lithium salt are provided. Wherein the first monomer is R1—OCH2—CH2—OnR2, the second monomer is R3—OCH2—CH2—OmR4, each “R1”, “R2” and “R3” includes —C═C— group or —C≡C— group, “R4” is an alkyl group or a hydrogen (H), and “m” and “n” represents an integer number, molecular weights of the first and second monomers are greater than or equal to 100, and less than or equal to 800. The first and second monomers, the initiator and the lithium salt are mixed to form a mixture, and a weight ratio of the first monomer to the second monomer is less than or equal to 50%. The first and second monomers are polymerized to form an interpenetrating polymer network, and the lithium salt is transformed into a solid solution and dispersing in the interpenetrating polymer network.
    • 制备固体电解质的方法包括以下步骤。 提供第一单体,第二单体,引发剂和锂盐。 其中,第一单体为R 1 -OCH 2 -CH 2 -OOR n R 2,第二单体为R 3 -OCH 2 -CH 2 -OCl m R 4,每个“R1”,“R2”和“R3”包括-C = C - 基或-C = C-基,“R4”是烷基或氢(H),“m”和“n”表示整数,第一和第二单体的分子量大于或等于 至100,小于等于800.将第一和第二单体,引发剂和锂盐混合以形成混合物,并且第一单体与第二单体的重量比小于或等于50% 。 聚合第一和第二单体以形成互穿聚合物网络,并将锂盐转变成固溶体并分散在互穿聚合物网络中。