会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明授权
    • Method of manufacturing a contoured fluid-filled chamber with tensile structures
    • 制造具有拉伸结构的带轮廓流体填充室的方法
    • US08869430B2
    • 2014-10-28
    • US13049278
    • 2011-03-16
    • Kirvan L. ChaoFrederick J. DojanKlaas P. Hazenberg
    • Kirvan L. ChaoFrederick J. DojanKlaas P. Hazenberg
    • A43B13/20B29D35/14
    • A43B13/18A43B13/20B29D35/142
    • In one method of manufacturing a fluid-filled chamber, two polymer layers are located between two mold portions, the surfaces of the mold portions cooperatively defining a peripheral cavity with first and second regions, an inward extent of the first region exceeding an inward extent of the second region. A tensile structure may be positioned between the polymer layers and the mold portions may be compressed together. Part of a peripheral portion of the chamber may be formed by drawing first and second areas of the chamber against the first and second regions of the peripheral cavity, respectively. After pressurization, the first region of the peripheral cavity may have a greater extent of outward protrusion than the second region of the peripheral cavity. Accordingly, an asymmetric medio-lateral shape may be imparted to the chamber without the use of a tensile structure that is itself tapered or contoured.
    • 在制造流体填充室的一种方法中,两个聚合物层位于两个模具部分之间,模具部分的表面协作地限定具有第一和第二区域的外围空腔,第一区域的向内范围超过 第二个地区。 拉伸结构可以位于聚合物层之间,并且模具部分可以被压缩在一起。 腔室的周边部分的一部分可以通过分别将腔室的第一和第二区域分别抵靠周边空腔的第一和第二区域来形成。 在加压之后,周边空腔的第一区域可以具有比外围空腔的第二区域更大的向外突出的程度。 因此,不用使用本身呈锥形或轮廓的拉伸结构,可以向腔室施加不对称的中间 - 外侧形状。
    • 5. 发明申请
    • Method Of Manufacturing A Contoured Fluid-Filled Chamber With Tensile Structures
    • 制造具有拉伸结构的轮廓流体填充室的方法
    • US20120233880A1
    • 2012-09-20
    • US13049278
    • 2011-03-16
    • Kirvan L. ChaoFrederick J. DojanKlaas P. Hazenberg
    • Kirvan L. ChaoFrederick J. DojanKlaas P. Hazenberg
    • A43B13/20A43D8/00
    • A43B13/18A43B13/20B29D35/142
    • In one method of manufacturing a fluid-filled chamber, two polymer layers are located between two mold portions, the surfaces of the mold portions cooperatively defining a peripheral cavity with first and second regions, an inward extent of the first region exceeding an inward extent of the second region. A tensile structure may be positioned between the polymer layers and the mold portions may be compressed together. Part of a peripheral portion of the chamber may be formed by drawing first and second areas of the chamber against the first and second regions of the peripheral cavity, respectively. After pressurization, the first region of the peripheral cavity may have a greater extent of outward protrusion than the second region of the peripheral cavity. Accordingly, an asymmetric medio-lateral shape may be imparted to the chamber without the use of a tensile structure that is itself tapered or contoured.
    • 在制造流体填充室的一种方法中,两个聚合物层位于两个模具部分之间,模具部分的表面协作地限定具有第一和第二区域的外围空腔,第一区域的向内范围超过 第二个地区。 拉伸结构可以位于聚合物层之间,并且模具部分可以被压缩在一起。 腔室的周边部分的一部分可以通过分别将腔室的第一和第二区域分别靠着周边空腔的第一和第二区域而形成。 在加压之后,周边空腔的第一区域可以具有比外围空腔的第二区域更大的向外突出的程度。 因此,不用使用本身呈锥形或轮廓的拉伸结构,可以向腔室施加不对称的中间 - 外侧形状。