    • 1. 发明授权
    • Higher molecular weight arylene sulfide resin and process for its
preparation
    • 较高分子量的亚芳基硫醚树脂及其制备方法
    • US5110901A
    • 1992-05-05
    • US580720
    • 1990-09-11
    • Kenneth C. HooverEarl Clark, Jr.Roy E. RegerLacey E. ScogginsAfif M. Nesheiwat
    • Kenneth C. HooverEarl Clark, Jr.Roy E. RegerLacey E. ScogginsAfif M. Nesheiwat
    • C08G75/02
    • C08G75/0259
    • In a first embodiment, arylene sulfide resins are provided by contacting, in a polymerization mixture, during a polymerization process, reactants comprising: an alkali metal sulfide, an organic amide, an alkali metal carboxylate, water and a monomer source which comprises at least one dihaloaromatic compound. The amount of alkali metal carboxylate present during the polymerization process ranges from about 0.01 to about 0.03 mole per each mole of sulfur present in the resulting arylene sulfide resin. The total amount of water present during the polymerization process ranges from about 1.02 to about 2.1 moles per each mole of sulfur present in the resulting arylene sulfide resin.In a second embodiment, arylene sulfide resins are provided by contacting, in a polymerization mixture, during a polymerization process, reactants comprising: an alkali metal sulfide, an organic amide, an alkali metal carboxylate, water and a monomer source which comprises a mixture of at least one dihaloaromatic compound and at least one polyhaloaromatic compound having more than two halogen substituents per molecule. The ranges of the amount of alkali metal carboxylate present during the polymerization process and the total amount of water present during the polymerization process are identical to those amounts disclosed in the first embodiment. The amount of polyhaloaromatic compound initially present ranges from about 0.0001 to about 0.01 mole per each mole of dihaloaromatic compound present prior to the initiation of the polymerization process.
    • 在第一个实施方案中,亚芳基硫醚树脂通过在聚合反应过程中使聚合反应中的反应物与碱金属硫化物,有机酰胺,碱金属羧酸盐,水和单体源接触来提供,所述反应物包括至少一种 二卤化合物。 在聚合过程中存在的碱金属羧酸盐的量为所得亚芳基硫醚树脂中存在的每摩尔硫的约0.01至约0.03摩尔。 在聚合过程中存在的水的总量范围为所得亚芳基硫醚树脂中存在的每摩尔硫的约1.02至约2.1摩尔。 在第二个实施方案中,亚芳基硫醚树脂是通过在聚合反应过程中使聚合反应中的反应物与碱金属硫化物,有机酰胺,碱金属羧酸盐,水和单体来源接触来提供的, 至少一种二卤代芳族化合物和每分子具有多于两个卤素取代基的至少一种多卤芳族化合物。 在聚合过程中存在的碱金属羧酸盐的量的范围和在聚合过程中存在的水的总量与第一实施方案中公开的量相同。 在开始聚合过程之前,存在的每摩尔二卤代芳族化合物最初存在的多卤代芳族化合物的量为约0.0001至约0.01摩尔。