    • 2. 发明授权
    • Process for the manufacture of .beta.-isobutyrylaminocrotonic acid amide
    • 制备β-异丁酰氨基巴豆酸酰胺的方法
    • US4242276A
    • 1980-12-30
    • US99778
    • 1979-12-03
    • Bernd Schilling
    • Bernd Schilling
    • C07C67/00C07C231/00C07C231/04C07C231/12C07C237/16C07C237/22C07C97/16
    • C07C231/00
    • A process for the manufacture of .beta.-isobutyrylaminocrotonic acid amide by reacting .beta.-aminocrotonic acid amide with dimethylketene in the liquid or gaseous state without the application of external heat at temperatures in the range of from room temperature to 70.degree. C. The dispersion medium used is an organic solvent having a boiling point above 40.degree. C. that may contain up to 0.1 mole of water and 0.2 to 2 moles of a carboxylic acid having 1 to 4 carbon atoms per mole of .beta.-aminocrotonic acid amide. If the dimethylketene is added undiluted the reaction is carried out in the absence of oxygen and in the presence of a protective gas atmosphere. The .beta.-isobutyrylaminocrotonic acid amide is obtained in the form of two stereoisomers (Z- and E-forms), which differ as regards their melting point and their solubility in organic solvents. On heating to 40.degree. C., the E-form is converted into the Z-form.
    • 通过使β-氨基巴豆酸酰胺与液体或气态的二甲基烯酮反应制备β-异丁酰氨基巴豆酸酰胺的方法,而不需要在室温至70℃的温度范围内施加外界热。使用的分散介质 是沸点高于40℃的有机溶剂,其可含有至多0.1摩尔水和0.2至2摩尔每摩尔β-氨基巴豆酸酰胺具有1至4个碳原子的羧酸。 如果未稀释地加入二甲基烯酮,则反应在不存在氧的情况下和在保护气体气氛存在下进行。 β-二异丁酰氨基巴豆酸酰胺以两种立体异构体(Z-和E-型)的形式获得,它们的熔点和它们在有机溶剂中的溶解度不同。 加热至40℃时,将E型转化成Z型。
    • 4. 发明授权
    • Process for the manufacture of 2-isopropyl-4-methyl-6-hydroxypyrimidine
    • 制备2-异丙基-4-甲基-6-羟基嘧啶的方法
    • US4585863A
    • 1986-04-29
    • US641329
    • 1984-08-16
    • Wolfgang DeinhammerBernd Schilling
    • Wolfgang DeinhammerBernd Schilling
    • C07D239/34C07D239/36C07D239/02
    • C07D239/36
    • An improved process for the manufacture of 2-isopropyl-4-methyl-6-hydroxypyrimidine, starting from 3-aminocrotonic acid amide and an acylating agent, without isolating the intermediately formed 3-isobutyrylaminocrotonic acid amide. In a first process step, the acylation is carried out with excess isobutyric acid anhydride in the presence of an alkali metal salt of isobutyric acid at temperatures of from 50.degree. to 120.degree. C. and in the absence of a solvent. In a second process step, the cyclization is carried out in the resulting reaction mixture by the addition of an aqueous alkali metal hydroxide solution at temperatures of from 80.degree. to 105.degree. C., and then the hydroxypyrimidine is isolated in known manner. The total quantities of alkali metal hydroxide added in the second process step are such that they are sufficient both for the neutralization of the isobutyric acid present in the reaction mixture and also for the cyclization. Less than 1 mole of alkali metal hydroxide per mole of the 3-aminocrotonic acid amide originally used is used for the cyclization itself.
    • 从3-氨基巴豆酸酰胺和酰化剂制备2-异丙基-4-甲基-6-羟基嘧啶的改进方法,而不分离中间形成的3-异丁酰氨基巴豆酸酰胺。 在第一工艺步骤中,在50-120℃的温度和不存在溶剂的条件下,在异丁酸的碱金属盐存在下,用过量的异丁酸酐进行酰化。 在第二个工艺步骤中,通过在80℃至105℃的温度下加入碱金属氢氧化物水溶液在所得反应混合物中进行环化,然后以已知的方式分离出羟基嘧啶。 在第二工艺步骤中加入的碱金属氢氧化物的总量使得它们对于中和反应混合物中存在的异丁酸以及环化都是足够的。 最初使用的每摩尔3-氨基巴豆酸酰胺少于1摩尔碱金属氢氧化物用于环化本身。
    • 8. 发明授权
    • Vinylaromatic/1,3-diene copolymer stabilized with protective colloids as adhesives for porous substrates
    • 用保护胶体稳定的乙烯基芳烃/ 1,3-二烯共聚物作为多孔基材的粘合剂
    • US06656983B1
    • 2003-12-02
    • US09856538
    • 2001-08-01
    • Theo MayerThomas KohlerReinhard HarzschelHans-Peter WeitzelBernd Schilling
    • Theo MayerThomas KohlerReinhard HarzschelHans-Peter WeitzelBernd Schilling
    • C08L100
    • C09J125/10C08F236/10C08L2666/02C09J109/06
    • The invention provides mixed aromatic vinyl-1,3-diene polymers stabilized by a protective colloid and present in the form of aqueous polymer dispersions or polymer powders redispersible in water as adhesives for porous substrates. The polymer dispersions and the polymer powders are obtained by emulsion polymerization of a mixture containing: a) 20 to 80 percent by weight of one or more vinylaromatics; b) 19.9 to 79.9 percent by weight of one or more 1,3-dienes; c) 0.1 to 15 percent by weight of one or more comonomers from the group consisting of N-methylolacrylamide, N-methylolmethacrylamide and the N-(alkoxymethyl)-acrylamides and N-(alkoxymethyl)-methacrylamides with a C1 to C6-alkyl radical. The sum of the above percentages adds up to 100% by weight. Emulsion polymerization is carried out in the presence of one or more protective colloids and without emulsifiers, optionally followed by drying of the resulting aqueous polymer dispersion.
    • 本发明提供了由保护胶体稳定并以聚合物水分散体形式存在的混合芳族乙烯基-1,3-二烯聚合物或可再分散在水中的聚合物粉末作为多孔基材的粘合剂。 聚合物分散体和聚合物粉末通过混合物的乳液聚合获得,所述混合物包含:a)20至80重量%的一种或多种乙烯基芳烃; b)19.9至79.9重量%的一种或多种1,3-二烯; c)0.1至15重量%的来自由N-羟甲基丙烯酰胺,N-羟甲基甲基丙烯酰胺和N-(烷氧基甲基) - 丙烯酰胺和具有C 1至C 6 - 烷基的N-(烷氧基甲基) - 甲基丙烯酰胺组成的组中的一种或多种共聚单体 。 上述百分比的总和高达100重量%。 乳液聚合在一种或多种保护胶体和不含乳化剂的存在下进行,任选然后干燥所得的聚合物水分散体。
    • 9. 发明授权
    • Novel coating slips
    • 新型涂层滑
    • US4879336A
    • 1989-11-07
    • US272634
    • 1988-11-17
    • Bernd SchillingKarl-Ernst Fickert
    • Bernd SchillingKarl-Ernst Fickert
    • C08F216/06C08F8/12C08F16/02C08L29/02C09D5/00C09D129/04D21H19/60
    • D21H19/60
    • In a coating slip for coating flat surfaces comprising an aqueous dispersion, with a solids content of 8 to 65% by weight, of 100 parts by weight of a pigment, 3 to 30 parts by weight of synthetic high-molecular-weight binder based on copolymers of acrylates, styrene, butadiene and unsaturated carboxylic acid esters and 0.5 to 2 parts by weight of a cobinder the improvement comprising using a cobinder polymer containing a large degree of hydroxyl groups comprising (a) 50 to 95% by weight of vinyl alcohol units, (b) 5 to 50% by weight of 1-alkylvinyl alcohol units of 1 to 4 alkyl carbon atoms, (c) 0 to 20% by weight of vinyl acylate units, (d) 0 to 20% by weight of allyl alcohol units and (e) 0 to 5% by weight of other polymerizable monomers having improved pigment shock behavior and very good activity as an optical brightener support.
    • 在用于涂覆平坦表面的涂层滑动剂中,其包含含水分散体,固含量为8至65重量%,100重量份颜料,3至30重量份的合成高分子量粘合剂,基于 丙烯酸酯,苯乙烯,丁二烯和不饱和羧酸酯的共聚物和0.5至2重量份的椰子料,其改进包括使用含有大量羟基的椰子树脂聚合物,其包含(a)50至95重量%的乙烯醇单元 ,(b)5〜50重量%的1〜4个烷基碳原子的1-烷基乙烯醇单元,(c)0〜20重量%的乙烯基酰化物单元,(d)0〜20重量%的烯丙基醇 单元和(e)0至5重量%的具有改进的颜料冲击行为和作为荧光增白剂载体的非常好的活性的其它可聚合单体。