    • 3. 发明授权
    • UV-radiation absorbing glass with reduced absorption of visible light and methods of making and using same
    • 具有减少可见光吸收的紫外线吸收玻璃及其制造和使用方法
    • US07375043B2
    • 2008-05-20
    • US10861822
    • 2004-06-04
    • Joerg FechnerAndreas ReisseFranz OttBrigitte Hueber
    • Joerg FechnerAndreas ReisseFranz OttBrigitte Hueber
    • C03C3/091C03C3/093
    • C03C3/091C03C3/089C03C3/093C03C4/085
    • The method for making UV-absorbing glass, which transmits in a visible range, includes melting raw materials to form a melt and producing the melt under oxidative conditions. The UV-absorbing glass is free of PbO and has the following composition (in % by weight): SiO2, 55-79; B2O3, 3-25; Al2O3, 0-10; Li2O, 0-10; Na2O, 0-10; K2O, 0-10; MgO, 0-2; CaO, 0-3; SrO, 0-3; BaO, 0-3; ZnO, 0-3; ZrO2, 0-3; CeO2, 0-1; Fe2O3, 0-1; WO3, 0-3; Bi2O3, 0-3; MoO3, 0-3; with Σ Li2O+Na2O+K2O=0.5 to 16 and Σ MgO+CaO+SrO+BaO+ZnO=0-10. The melt composition is characterized by including 0.1 to 10 % TiO2 and from 0.01-10 % As2O3. The glass made by the method and its properties are also disclosed. The glass is useful in lamps, LCD displays, monitors and glass-to-metal seals with molybdenum, tungsten and Fe—Co—Ni alloys.
    • 制造在可见光范围内透射的紫外线吸收玻璃的方法包括熔化原料以形成熔体并在氧化条件下生产熔体。 UV吸收玻璃不含PbO,具有以下组成(重量%):SiO 2,55-79; B 2 O 3,3-25; Al 2 O 3,0-10; Li 2 O,0-10; Na 2 O,0-10; K 2 O,0-10; MgO,0-2; CaO,0-3; SrO,0-3; 宝,0-3; ZnO,0-3; ZrO 2,0-3; CeO 2,0-1; Fe 2 O 3,0-1; WO 3,O 3; Bi 2 O 3,O 3; MoO 3,0-3; 与Sigma Li 2 O + Na 2 O + K 2 O = 0.5至16和Sigma MgO + CaO + SrO + BaO + ZnO = 0-10。 熔融组合物的特征在于包含0.1至10%的TiO 2和0.01至10%的As 2 O 3 3。 还公开了通过该方法制造的玻璃及其性质。 该玻璃可用于灯,LCD显示屏,显示器和具有钼,钨和Fe-Co-Ni合金的玻璃 - 金属密封。
    • 8. 发明申请
    • UV-absorbing borosilicate glass for a gas discharge lamp, process for manufacturing same and gas discharge lamp made with same
    • 用于气体放电灯的紫外线吸收硼硅酸盐玻璃,其制造方法和用其制造的气体放电灯
    • US20060009343A1
    • 2006-01-12
    • US11178793
    • 2005-07-11
    • Joerg FechnerFranz OttBrigitte Hueber
    • Joerg FechnerFranz OttBrigitte Hueber
    • C03C3/089C03C3/091
    • C03C3/091C03C3/089C03C4/085H01J61/302
    • Glass for gas discharge tubes, which are used in fluorescent lamps, EEFL lamps, LCD displays, computer monitors, telephone displays and TFT displays, and a process for making it are described. The glass contains, in % by weight based on oxide content: SiO2, 60-75; B2O3, >25-35; Al2O3, 0-10; Li2O, 0-10; Na2O, 0-20; K2O, 0-20; MgO, 0-8; CaO, 0-20; SrO, 0-5; BaO, 0-5; ZnO, 0-3; ZrO2, 0-5; TiO2, 0-10; Fe2O3, 0-0.5; CeO2 0-0.5; MnO2, 0-1.0; Nd2O3, 0-1; WO3, 0-2; Bi2O3, 0-5; MoO3, 0-5; As2O3, 0-1; Sb2O3, 0-1; SO42−, 0-2 C−, 0-2 and F−, 0-2, wherein ΣLi2O+Na2O+K2O=0-25% by weight; ΣMgO+CaO+SrO+BaO=0-20; ΣFe2O3+CeO2+TiO2+PbO+As2O3+Sb2O3 is at least 0-10; and ΣPdO+PtO3+PtO2+PtO+RhO2+Rh2O3+IrO2+Ir2O3 is from 0.00001-0.1.
    • 描述了用于荧光灯,EEFL灯,LCD显示器,计算机显示器,电话显示器和TFT显示器的气体放电管用玻璃及其制造方法。 玻璃含有以氧化物含量为基准的重量%:SiO 2,60-75; B 2 O 3,25-35; Al 2 O 3,0-10; Li 2 O,0-10; Na 2 O,0-20; K 2 O,0-20; MgO,0-8; CaO,0-20; SrO,0-5; BaO,0-5; ZnO,0-3; ZrO 2,0-5; TiO 2,0-10; Fe 2 O 3,0-0.5; CeO 2 0-0.5; MnO 2,0-1.0; Nd 2 O 3,0-1; WO 3,O 2; Bi 2 O 3,0-5; MoO 3,0-5; 作为2 3,0-1; Sb 2 O 3,0-1; 0-2,0-2,...,0-2,...,0-2,...,0-2, 其中SigmaLi 2 O + Na 2 O + K 2 O = 0-25重量%; SigmaMgO + CaO + SrO + BaO = 0-20; SigmaFe 2 O 3 + CeO 2 + TiO 2 + PbO + As 2 N 2 + O 3 + Sb 2 O 3 3至少为0-10; 和SigmaPdO + PtO 3 + PtO 2 + PtO + RhO 2 + Rh 2 O 3 3< 3> / O 2 + Ir 2 + 2 2 O 3 3从0.00001-0.1。
    • 9. 发明授权
    • UV-absorbing borosilicate glass for a gas discharge lamp and process for manufacturing same
    • 用于气体放电灯的紫外线吸收硼硅酸盐玻璃及其制造方法
    • US07598191B2
    • 2009-10-06
    • US11178793
    • 2005-07-11
    • Joerg FechnerFranz OttBrigitte Hueber
    • Joerg FechnerFranz OttBrigitte Hueber
    • C03C3/089C03C3/091
    • C03C3/091C03C3/089C03C4/085H01J61/302
    • Glass for gas discharge tubes, which are used in fluorescent lamps, EEFL lamps, LCD displays, computer monitors, telephone displays and TFT displays, and a process for making it are described. The glass contains, in % by weight based on oxide content: SiO2, 60-75; B2O3, >25-35; Al2O3, 0-10; Li2O, 0-10; Na2O, 0-20; K2O, 0-20; MgO, 0-8; CaO, 0-20; SrO, 0-5; BaO, 0-5; ZnO, 0-3; ZrO2, 0-5; TiO2, 0-10; Fe2O3, 0-0.5; CeO2 0-0.5; MnO2, 0-1.0; Nd2O3, 0-1.0; WO3, 0-2; Bi2O3, 0-5; MoO3, 0-5; As2O3, 0-1; Sb2O3, 0-1; SO42−, 0-2; Cl-, 0-2 and F−, 0-2, wherein ΣLi2O+Na2O+K2O=0-25% by weight; ΣMgO+CaO+SrO+BaO=0-20; ΣFe2O3+CeO2+TiO2+PbO+As2O3+Sb2O3 is at least 0-10; and ΣPdO+PtO3+PtO2+PtO+RhO2+Rh2O3+IrO2+Ir2O3 is from 0.00001-0.1.
    • 描述了用于荧光灯,EEFL灯,LCD显示器,计算机显示器,电话显示器和TFT显示器的气体放电管用玻璃及其制造方法。 该玻璃含有以氧化物含量为基准的重量%:SiO 2,60-75; B2O3,> 25-35; Al2O3,0-10; Li2O,0-10; Na2O,0-20; K2O,0-20; MgO,0-8; CaO,0-20; SrO,0-5; BaO,0-5; ZnO,0-3; ZrO2,0-5; TiO2,0-10; Fe2O3,0-0.5; CeO2 0-0.5; MnO2,0-1.0; Nd2O3,0-1.0; WO3,0-2; Bi2O3,0-5; MoO3,0-5; As2O3,0-1; Sb2O3,0-1; SO42-,0-2; Cl-,0-2和F-,0-2,其中SigmaLi2O + Na2O + K2O = 0-25%(重量); SigmaMgO + CaO + SrO + BaO = 0-20; SigmaFe2O3 + CeO2 + TiO2 + PbO + As2O3 + Sb2O3至少为0-10; 和SigmaPdO + PtO3 + PtO2 + PtO + RhO2 + Rh2O3 + IrO2 + Ir2O3为0.00001-0.1。
    • 10. 发明授权
    • Glass for an EEFL fluorescent lamp, process for making the glass and devices including articles made with the glass
    • 用于EEFL荧光灯的玻璃,用于制造玻璃的工艺和包括用玻璃制成的制品的装置
    • US07498731B2
    • 2009-03-03
    • US11178760
    • 2005-07-11
    • Joerg FechnerFranz OttBrigitte Hueber
    • Joerg FechnerFranz OttBrigitte Hueber
    • C03C3/091C03C3/093H01J5/00
    • C03C3/087C03C3/078C03C4/085
    • Glass for gas discharge tubes, which are used in fluorescent lamps, especially EEFL and miniaturized lamps, LCD displays, computer monitors, telephone displays and TFT displays, and a process for making it are described. The glass contains, in % by weight based on oxide content: SiO2, 60-85; B2O3, 0-10; Al2O3, 0-10; Li2O, 0-10; Na2O, 0-20; K2O, 0-20; MgO, 0-8; CaO, 0-20; SrO, 0-5; BaO, 0-5; ZnO, 0-8; ZrO2, 0-5; TiO2, 0-10; Fe2O3, 0-5; CeO2 0-5; MnO2, 0-5; Nd2O3, 0-1.0; WO3, 0-2; Bi2O3, 0-5; MoO3, 0-5; PbO, 0-5; As2O3, 0-1; Sb2O3, 0-1; SO42−, 0-2; Cl−, 0-2 and F−, 0-2, wherein Σ Li2O+Na2O+K2O=5-25% by weight; Σ MgO+CaO+SrO+BaO=3-20; Σ Fe2O3+CeO2+TiO2+PbO+As2O3+Sb2O3 is at least 0-10; and Σ PdO+PtO3+PtO2+PtO+RhO2+Rh2O3+IrO2+Ir2O3 is 0.1.
    • 用于荧光灯,特别是EEFL和小型化灯,LCD显示器,计算机显示器,电话显示器和TFT显示器的气体放电管用玻璃及其制造方法进行说明。 该玻璃含有以氧化物含量为基准的重量%:SiO 2,60-85; B2O3,0-10; Al2O3,0-10; Li2O,0-10; Na2O,0-20; K2O,0-20; MgO,0-8; CaO,0-20; SrO,0-5; BaO,0-5; ZnO,0-8; ZrO2,0-5; TiO2,0-10; Fe2O3,0-5; CeO2 0-5; MnO2,0-5; Nd2O3,0-1.0; WO3,0-2; Bi2O3,0-5; MoO3,0-5; PbO,0-5; As2O3,0-1; Sb2O3,0-1; SO42-,0-2; Cl-,0-2和F-,0-2,其中Sigma Li2O + Na2O + K2O = 5-25%重量; Sigma MgO + CaO + SrO + BaO = 3-20; Sigma Fe2O3 + CeO2 + TiO2 + PbO + As2O3 + Sb2O3至少为0-10; 并且Sigma PdO + PtO 3 + PtO 2 + PtO + RhO 2 + Rh 2 O 3 + IrO 2 + Ir 2 O 3为0.1。