    • 2. 发明授权
    • Cutting element, electric shaver provided with a cutting element
    • 切割元件,电动剃须刀配有切割元件
    • US08806762B2
    • 2014-08-19
    • US12595249
    • 2008-04-16
    • Hubert Sjoerd Blaauw
    • Hubert Sjoerd Blaauw
    • B26B21/58
    • C23C8/38B26B19/044B26B19/141B26B21/60
    • The invention relates to a cutting element (10), such as used in an electric shaver. The cutting element is made from stainless steel with a hardened surface layer (14) over at least part of its surface, and is characterized, in that the cutting end face (11) of the element comprises a, surface layer of hardened steel at least over its cutting edge (12), the rest of the end face comprising the stainless steel. The cutting element has self-sharpening and wear adjustable characteristics. The invention also relates to a method for producing the cutting element, and to an electric shaver comprising at least one cutting element according to the invention.
    • 本发明涉及一种用于电动剃须刀的切割元件(10)。 切割元件由不锈钢制成,在其表面的至少一部分上具有硬化的表面层(14),其特征在于,元件的切割端面(11)至少包括硬化钢的表面层 在其切割边缘(12)上,其余的端面包括不锈钢。 切割元件具有自磨削和磨损可调特性。 本发明还涉及一种用于制造切割元件的方法以及包括根据本发明的至少一个切割元件的电动剃须刀。
    • 3. 发明申请
    • METHOD FOR MANUFACTURING A STAINLESS STEEL PRODUCT
    • 制造不锈钢产品的方法
    • US20090218011A1
    • 2009-09-03
    • US11917577
    • 2006-06-12
    • Hubert Sjoerd BlaauwMartin HommesLucius Theodorus Vinkenvleugel
    • Hubert Sjoerd BlaauwMartin HommesLucius Theodorus Vinkenvleugel
    • C23C8/26C22C38/00
    • C23C8/26C21D6/002C23C8/80
    • The invention relates to a method for making a thin finished product to be formed by deformation that combines strength with resistance to a highly corrosive environment. The method comprises forming a sheet of stainless steel with a microstructure consisting predominantly of ferrite, austenite, martensite or a mixture thereof, with a thickness of less than 3 mm, to a three dimensional semi finished product, treating said semi finished product with a nitrogen-containing atmosphere at a temperature of between 1000° C. and 1200° C. during a time and under a nitrogen pressure, sufficient to saturate the product through the thickness with a nitrogen content between a lower limit of 0.3 wt % and an upper limit that is provided by the beginning of nitride separation, cooling down said product at such a rate and nitrogen pressure that nitride separation is avoided, and subsequently machining the nitrogen saturated semi- finished product to the finished product. The invention further relates to a rotary shaving assembly prepared by the method of the invention.
    • 本发明涉及通过将强度与耐腐蚀性高的环境结合的变​​形来形成薄的成品的方法。 该方法包括以三维半成品形成具有主要由铁素体,奥氏体,马氏体或其混合物组成的微结构的不锈钢薄片至三维半成品,用氮气处理所述半成品 在氮气压力下的时间和氮气压力下,在1000℃和1200℃之间的温度下,使产品饱和,氮含量在0.3wt%的下限和上限之间 这是通过氮化物分离开始提供的,以这样的速度和氮气压力冷却所述产物,以避免氮化物分离,随后将氮饱和半成品加工成成品。 本发明还涉及通过本发明的方法制备的旋转剃须组件。
    • 5. 发明授权
    • Method for manufacturing a stainless steel product
    • 不锈钢制品的制造方法
    • US09382608B2
    • 2016-07-05
    • US11917577
    • 2006-06-12
    • Hubert Sjoerd BlaauwMartin HommesLucius Theodorus Vinkenvleugel
    • Hubert Sjoerd BlaauwMartin HommesLucius Theodorus Vinkenvleugel
    • C23C8/26C23C8/24C21D6/00C23C8/80
    • C23C8/26C21D6/002C23C8/80
    • The invention relates to a method for making a thin finished product to be formed by deformation that combines strength with resistance to a highly corrosive environment. The method comprises forming a sheet of stainless steel with a microstructure consisting predominantly of ferrite, austenite, martensite or a mixture thereof, with a thickness of less than 3 mm, to a three dimensional semi finished product, treating said semi finished product with a nitrogen-containing atmosphere at a temperature of between 1000° C. and 1200° C. during a time and under a nitrogen pressure, sufficient to saturate the product through the thickness with a nitrogen content between a lower limit of 0.3 wt % and an upper limit that is provided by the beginning of nitride separation, cooling down said product at such a rate and nitrogen pressure that nitride separation is avoided, and subsequently machining the nitrogen saturated semi- finished product to the finished product. The invention further relates to a rotary shaving assembly prepared by the method of the invention.
    • 本发明涉及通过将强度与耐腐蚀性高的环境结合的变​​形来形成薄的成品的方法。 该方法包括以三维半成品形成具有主要由铁素体,奥氏体,马氏体或其混合物组成的微结构的不锈钢薄片至三维半成品,用氮气处理所述半成品 在氮气压力下的时间和氮气压力下,在1000℃和1200℃之间的温度下,使产品饱和,氮含量在0.3wt%的下限和上限之间 这是通过氮化物分离开始提供的,以这样的速度和氮气压力冷却所述产物,以避免氮化物分离,随后将氮饱和半成品加工成成品。 本发明还涉及通过本发明的方法制备的旋转剃须组件。