    • 1. 发明授权
    • Artificial pigment and method for preparing the same
    • 人造颜料及其制备方法
    • US06750297B2
    • 2004-06-15
    • US10182438
    • 2002-07-29
    • Seung-Uk YeuHo-Yeul ChoiChang-Sun HanWan-Sik Cha
    • Seung-Uk YeuHo-Yeul ChoiChang-Sun HanWan-Sik Cha
    • C08F222
    • D21H19/42C08F285/00C08F212/08
    • The present invention relates to an artificial pigment and a method of preparing the same, specifically, to an artificial pigment with excellent dry pick resistance and to a method of preparing the same. In order to accomplish the present invention, there is provided an artificial pigment of inverted core-shell structure comprising: a) a shell of butadiene polymer including: i) a seed of butadiene polymer having glass transition temperature of −10 to 50° C.; and ii) a seed covering of butadiene polymer having a glass transition temperature of −10 to 20° C.; and b) a core of styrene polymer having a glass transition temperature of 40 to 120° C. Also provided is method of preparing artificial pigment comprising: a) preparing a shell of butadiene polymer; and b) preparing a core of styrene polymer on the inner side of said shell of step a). The coating color comprising the artificial pigment of the present invention can make coated paper having excellent dry pick resistance anti high paper gloss and printing gloss as well as stiffness.
    • 人造颜料及其制备方法技术领域本发明涉及一种人造颜料及其制备方法,具体涉及具有优良抗干性的人造颜料及其制备方法。 为了实现本发明,提供了一种倒置的核 - 壳结构的人造颜料,其包括:a)丁二烯聚合物的壳,包括:i)具有-10至50℃的玻璃化转变温度的丁二烯聚合物的种子 ; 和ii)玻璃化转变温度为-10〜20℃的丁二烯聚合物种子覆盖物; 和b)玻璃化转变温度为40〜120℃的苯乙烯聚合物的核心。还提供了制备人造颜料的方法,包括:a)制备丁二烯聚合物的壳; 和b)在步骤a)的所述壳的内侧制备苯乙烯聚合物的芯。 包含本发明的人造颜料的涂料颜色可以使具有优异抗干性能的涂布纸具有高的纸张光泽和印刷光泽度以及刚度。