    • Method of forming a fiber preform to minimize shifts of the
zero-dispersion wavelength
    • 形成纤维预制件以使零色散波长的偏移最小化的方法
    • US5683486A
    • 1997-11-04
    • US358529
    • 1994-12-19
    • Hiroshi OyamadaGo OginoHideo Hirasawa
    • Hiroshi OyamadaGo OginoHideo Hirasawa
    • C03B37/012C03B37/014C03B37/027
    • C03B37/014C03B2203/22C03B2203/36C03B2207/70G02B6/02247
    • An improvement is proposed, in a method for the preparation of a step-index silica glass preform as a precursor of optical fibers by completing the cladding layer of the secondary preform by the outer deposition on and around a primary preform consisting of the center core and side core, to conduct the outer deposition for the cladding layer in such a way that the inequality .vertline.d.lambda..sub.0 /dk.vertline..ltoreq.500 nm is satisfied, in which k is the ratio of the diameter of the primary preform to the diameter of the secondary preform and .lambda..sub.0 is the zero-dispersion wavelength in nm of an optical fiber obtained by drawing the secondary preform, d.lambda..sub.0 /dk being the differential of a function held between .lambda..sub.0 and k determined beforehand from the distribution of the refractive index within the primary preform. When the outer deposition is performed in this way, a great improvement can be obtained in the uniformity of the zero-dispersion wavelength of the optical fiber prepared by drawing the preform.
    • 提出了一种改进方法,其中通过在由中心核心构成的初级预制件上和周围的外部沉积来完成二次预型体的包覆层来制备作为光纤前体的步进折射率石英玻璃预制件的方法,以及 以使得不等式|dλ0 / dk |≤500nm满足下述方式对包覆层进行外部沉积,其中k是初级预制棒的直径与直径的比率 次级预制件和λ0是通过拉制次级预制件获得的光纤的零色散波长(nm),dλ0 / dk是预先从折射率分布预先确定的λ0和k之间保持的函数的差分 初级预制件内的折射率。 当以这种方式进行外部沉积时,通过拉伸预制件制备的光纤的零色散波长的均匀性可以获得很大的改进。
    • 9. 发明授权
    • Optical fiber and method for manufacturing silica glass
    • 光纤及石英玻璃制造方法
    • US09025922B2
    • 2015-05-05
    • US13403983
    • 2012-02-24
    • Hiroshi Oyamada
    • Hiroshi Oyamada
    • G02B6/02C03C25/60
    • C03C25/607C03C2201/21C03C2201/22
    • A method for manufacturing deuterium-treated silica glass includes exposing silica glass to a deuterium-containing atmosphere for a predetermined period of time to diffuse deuterium molecules within the silica glass, maintaining the silica glass at 40° C. or higher, and cooling the silica glass to room temperature. The silica glass is a silica glass-based optical fiber having a core made of silica glass, where the core is positioned at a center of the optical fiber and contains at least germanium, and a clad made of silica glass, where the clad surrounds the core and has a lower refractive index than the core. A surface of the silica glass is covered with a resin coating.