    • 4. 发明申请
    • POLYOXAMIDE RESIN HAVING EXCELLENT IMPACT RESISTANCE AND IMPACT-RESISTANT PART
    • 具有优异抗冲击性和耐冲击性的聚酰胺树脂
    • US20130172520A1
    • 2013-07-04
    • US13823828
    • 2011-09-15
    • Shuichi MaedaKouichiro KurachiHiroshi OkushitaYasunari HanaokaNaoyasu YabuTomoyuki Nakagawa
    • Shuichi MaedaKouichiro KurachiHiroshi OkushitaYasunari HanaokaNaoyasu YabuTomoyuki Nakagawa
    • C08G69/26
    • C08G69/26C08G69/265
    • Provided is a polyoxamide resin which has excellent impact resistance and is characterized in that the polyoxamide resin is obtained from a diamine in which the diamine component has 10 to 18 carbons and in that the polyoxamide resin has a relative viscosity (ηr) of 2.1 or greater as determined at 25° C. using 96% sulfuric acid as a solvent and a solution having a concentration of 1.0 g/dL, and also provided is an impact-resistant part comprising this resin. The polyoxamide resin has a higher molecular weight than a conventional polyoxamide resin, a large moldable temperature range as estimated from the difference between the melting point and the thermal decomposition temperature and therefore excellent molten moldability, and furthermore excellent impact resistance when compared to a conventional aliphatic polyoxamide resin without losing the low water absorbency, chemical resistance, hydrolysis resistance, high elasticity, and high strength seen with aliphatic straight-chain polyoxamide resins.
    • 本发明提供耐冲击性优异的聚酰胺树脂,其特征在于,所述聚酰胺树脂由二胺成分为10〜18个碳原子的二胺得到,所述聚酰胺树脂的相对粘度(etar)为2.1以上 使用96%硫酸作为溶剂和浓度为1.0g / dL的溶液在25℃下测定,并且还提供包含该树脂的耐冲击部件。 聚酰胺树脂具有比常规聚酰胺树脂更高的分子量,由熔点和热分解温度之间的差异估计的大的可成型温度范围,因此具有优异的熔融成型性,并且与常规的脂族化合物相比,具有优异的耐冲击性 聚酰胺树脂,而不损失脂肪族直链聚酰胺树脂所见的低吸水性,耐化学性,耐水解性,高弹性和高强度。
    • 5. 发明授权
    • Production method of polyamide resin
    • 聚酰胺树脂的生产方法
    • US09090738B2
    • 2015-07-28
    • US12532866
    • 2008-03-26
    • Hiroshi OkushitaKouichirou KurachiMasato Shimokawa
    • Hiroshi OkushitaKouichirou KurachiMasato Shimokawa
    • C08G69/28C08G69/26
    • C08G69/26C08G69/265C08G69/28
    • To provide a method for producing a polyoxamide resin by one-step polymerization without performing a pre-polycondensation step in a solvent, which is necessary in the conventional production of a polyoxamide resin. A method of mixing an oxalic acid diester and a diamine in a pressure-resistant vessel and subjecting the mixture to polymerization under pressure in the presence of an alcohol produced by a polycondensation reaction and then to melt polymerization at a temperature not lower than the melting point of the produced polymer preferably while extracting the alcohol, thereby producing a polyoxamide resin by one-step polymerization without using a solvent except for an alcohol that is produced by polycondensation of raw materials in the production process.
    • 提供通过一步聚合制备聚酰胺树脂的方法,而不需要在常规生产聚酰胺树脂中所需的溶剂中进行预缩聚步骤。 在耐压容器中混合草酸二酯和二胺的方法,在通过缩聚反应生成的醇的存在下,在压力下使混合物聚合,然后在不低于熔点的温度下熔融聚合 优选在提取醇的同时,通过一步聚合制备聚酰胺树脂,而不使用除了在生产过程中通过原料缩聚制备的醇之外的溶剂。
    • 7. 发明申请
    • PRODUCTION METHOD OF POLYAMIDE RESIN
    • 聚酰胺树脂的生产方法
    • US20100113737A1
    • 2010-05-06
    • US12532866
    • 2008-03-26
    • Hiroshi OkushitaKouichirou KurachiMasato Shimokawa
    • Hiroshi OkushitaKouichirou KurachiMasato Shimokawa
    • C08G69/28
    • C08G69/26C08G69/265C08G69/28
    • To provide a method for producing a polyoxamide resin by one-step polymerization without performing a pre-polycondensation step in a solvent, which is necessary in the conventional production of a polyoxamide resin. A method of mixing an oxalic acid diester and a diamine in a pressure-resistant vessel and subjecting the mixture to polymerization under pressure in the presence of an alcohol produced by a polycondensation reaction and then to melt polymerization at a temperature not lower than the melting point of the produced polymer preferably while extracting the alcohol, thereby producing a polyoxamide resin by one-step polymerization without using a solvent except for an alcohol that is produced by polycondensation of raw materials in the production process.
    • 提供通过一步聚合制备聚酰胺树脂的方法,而不需要在常规生产聚酰胺树脂中所需的溶剂中进行预缩聚步骤。 在耐压容器中混合草酸二酯和二胺的方法,在通过缩聚反应生成的醇的存在下,在压力下使混合物聚合,然后在不低于熔点的温度下熔融聚合 优选在提取醇的同时,通过一步聚合制备聚酰胺树脂,而不使用除了在生产过程中通过原料缩聚制备的醇之外的溶剂。
    • 8. 发明申请
    • POLYAMIDE RESIN
    • 聚酰胺树脂
    • US20100098893A1
    • 2010-04-22
    • US12518433
    • 2007-12-11
    • Hiroshi OkushitaKouichiro KurachiMasato ShimokawaShouichi Tanaka
    • Hiroshi OkushitaKouichiro KurachiMasato ShimokawaShouichi Tanaka
    • B32B1/08C08G69/26
    • C08G69/265C08L77/06Y10T428/139
    • There is provided a polyamide resin that can achieve a sufficiently high molecular weight compared to conventional polyamide 92, has a broad moldable temperature range or width estimated from a difference between melting point and thermal decomposition temperature, exhibits excellent melt moldability and has excellent chemical resistance and hydrolysis resistance compared to conventional aliphatic polyamide resins without impairing low water absorption property of an aliphatic linear polyoxamide resin. A polyamide resin in which the dicarboxylic acid component is oxalic acid and the diamine component is a diamine component composed of 1,9-nonanediamine and 2-methyl-1,8-octanediamine, with the molar ratio between 1,9-nonanediamine and 2-methyl-1,8-octanediamine being from 6:94 to 99:1.
    • 提供了与常规聚酰胺92相比可以获得足够高的分子量的聚酰胺树脂,具有从熔点和热分解温度之间的差异估计的宽的成型温度范围或宽度,显示出优异的熔融成型性,并且具有优异的耐化学性和 耐水解性与常规脂肪族聚酰胺树脂相比,而不损害脂族线型聚酰胺树脂的低吸水性。 一种聚酰胺树脂,其中二羧酸组分是草酸,二胺组分是由1,9-壬二胺和2-甲基-1,8-辛二胺组成的二胺组分,摩尔比为1,9-壬二胺和2 - 甲基-1,8-辛二胺为6:94至99:1。
    • 9. 发明申请
    • POLYETHER POLYAMIDE ELASTOMER
    • 聚醚多胺弹性体
    • US20090274913A1
    • 2009-11-05
    • US12305188
    • 2007-06-15
    • Hiroshi OkushitaShouichi Tanaka
    • Hiroshi OkushitaShouichi Tanaka
    • B32B27/08C08G73/02
    • C08G69/40B32B27/08B32B27/34B32B27/40B32B2437/02Y10T428/31562Y10T428/31725
    • Disclosed is a polyether polyamide elastomer particularly excellent in transparency while retaining properties such as dynamic physical properties, stiffness and bending-fatigue resistance. The polyether polyamide elastomer is produced by polymerizing (A) a polyamide-forming monomer selected from an aminocarboxylic acid compound (A1) represented by the following formula (1) and a lactam compound (A2) represented by the following formula (2), (B) a diamine compound comprising a triblock polyetherdiamine compound (B1) represented by the following formula (3) and at least one diamine compound (B2) selected from a branched saturated diamine having 6 to 22 carbon atoms, a branched alicyclic diamine having 6 to 16 carbon atoms and norbornanediamine, and (C) a dicarboxylic acid compound represented by the following formula (4), H2N—R1—COOH  (1) wherein R1 represents a linking group having a hydrocarbon chain, wherein R2 represents a linking group having a hydrocarbon chain, wherein x represents a number from 1 to 20, y represents a number from 4 to 50, and z represents a number from 1 to 20, HOOC—(R3)m—COOH  (4) wherein R3 represents a linking group having a hydrocarbon chain, and m represents 0 or 1.
    • 公开了一种特别优异的聚酯聚酰胺弹性体,同时保持诸如动态物理性能,刚度和抗弯曲疲劳性等性能。 聚醚聚酰胺弹性体是通过聚合(A)选自下式(1)表示的氨基羧酸化合物(A1)和由下式(2)表示的内酰胺化合物(A2)的聚酰胺形成性单体,( B)包含由下式(3)表示的三嵌段聚醚二胺化合物(B1)和至少一种选自具有6-22个碳原子的支化饱和二胺的二胺化合物(B2),支链脂环族二胺 16碳原子和降冰片烷二胺,(C)由下式(4)表示的二羧酸化合物,H 2 N-R 1 -COOH(1)其中R 1表示具有烃链的连接基团,其中R 2表示具有 烃链,其中x表示1至20的数,y表示4至50的数,z表示1-20的数,HOOC-(R3)m -COOH(4)其中R3表示具有 烃链,和 m表示0或1。