    • 3. 发明申请
    • Two-stage conversion treatment
    • 两阶段转化处理
    • US20070017602A1
    • 2007-01-25
    • US11450933
    • 2006-06-09
    • Alina KochMarian PawlikHeike QuellhorstPatrick Droniou
    • Alina KochMarian PawlikHeike QuellhorstPatrick Droniou
    • C23C22/34
    • C23C22/83C23C22/34C23C22/44C23C22/73
    • The invention relates to a chromium-free, corrosion prevention treatment for steel, zinc or zinc alloys, aluminum, magnesium or alloys thereof in which the metal surfaces are contacted in a first step with a first aqueous solution having a pH of 1.5 to 5 which contains Ti and/or Zr and/or Si ions and at least such a quantity of fluoride that the atomic ratio of Ti to F and/or Zr to F and/or Si to F is in the range from 1:1 to 1:6 and then, optionally after rinsing with water, and thereafter in a second step are contacted with a second aqueous solution having a pH of 1.5 to 5 which contains Ti and/or Zr and/or Si ions and at least such a quantity of fluoride that the atomic ratio of Ti to F and/or Zr to F and/or Si to F is in the range from 1:1 to 1:6, and which additionally contains such a quantity of soluble anions of oxo acids of Mo (VI) and/or W (VI) that the total concentration of molybdenum and/or tungsten is in the range from 5 to 1500 mg/l.
    • 本发明涉及一种钢,锌或锌合金,铝,镁或其合金的无铬防锈处理,其中金属表面在第一步骤中与pH为1.5至5的第一水溶液接触, 含有Ti和/或Zr和/或Si离子,并且至少一定量的氟化物,Ti与F和/或Zr与F和/或Si与F的原子比在1:1至1:5的范围内。 然后,任选地在用水冲洗后,然后在第二步中与含有Ti和/或Zr和/或Si离子的pH为1.5〜5的第二水溶液接触,并且至少含有这样的氟化物 Ti与F和/或Zr与F和/或Si与F的原子比在1:1至1:6的范围内,并且还含有如下量的可溶性阴离子的Mo(VI )和/或W(VI),钼和/或钨的总浓度在5至1500mg / l的范围内。