    • 9. 发明授权
    • Fine grained sintered cemented carbide, process for manufacturing and use thereof
    • 细晶粒烧结硬质合金,其制造及使用方法
    • US07179319B2
    • 2007-02-20
    • US10759478
    • 2004-01-16
    • Hans-Wilm HeinrichDieter SchmidtManfred Wolf
    • Hans-Wilm HeinrichDieter SchmidtManfred Wolf
    • C22C29/08
    • C22C29/08B22F2005/001B22F2998/10C22C1/053C22C29/067Y10T428/12007B22F9/04B22F3/02B22F3/10C23C14/00C23C16/00
    • The invention proposes a fine grained sintered cemented carbide containing chromium and based on WC and a binder based on Co or CoNiFe, and having at least one additional phase comprising at least one carbide or mixed carbide of tantalum. For improving the high-temperature properties while simultaneously maintaining a good trade-off between hardness and bending strength, it is proposed that the sintered cemented carbide contains approximately 0.3 to 4% Ta, as related to the total mass of the sintered cemented carbide, that the WC has a grain size of between 0.1 and 1.3 μm, that the binder phase contains the metals W, Cr and Ta, dissolved in solid solution, and that the at least one additional phase comprises a TaC phase visible by optical microscopy. The invention further relates to a powder-metallurgical process for manufacturing the sintered cemented carbide and to the use of the sintered cemented carbide for manufacturing cutting tools having improved high-temperature properties.
    • 本发明提出了一种包含铬并基于WC的细晶粒烧结硬质合金和基于Co或CoNiFe的粘合剂,并且具有至少一个包含至少一种碳化物或钽的混合碳化物的附加相。 为了提高高温性能同时保持硬度和弯曲强度之间的良好折衷,提出烧结硬质合金含有约0.3至4%的Ta,与烧结硬质合金的总质量相关, WC的粒径为0.1〜1.3μm,粘结相含有溶解在固溶体中的金属W,Cr和Ta,并且至少一个附加相包括通过光学显微镜可见的TaC相。 本发明还涉及用于制造烧结硬质合金的粉末冶金方法,以及使用烧结硬质合金制造具有改进的高温性能的切削工具。