    • Single-bake two-layer enamelling with electrostatic powder coating
    • 单烤双层搪瓷与静电粉末涂料
    • US4265929A
    • 1981-05-05
    • US96368
    • 1979-11-21
    • Gebhard WagnerWerner Joseph
    • Gebhard WagnerWerner Joseph
    • A01B43/00C03C8/02C03C8/04C03C8/06C23D5/04B05D1/06
    • C23D5/04C03C8/02C03C8/04C03C8/06C03C2207/02C03C2207/04
    • In a two-layer enamelling process in which the ground coat and surface coat powders are electrostatically applied to metallic substrates and subsequently baked together, the improvement which comprises employing a ground coat powder having an electrical resistivity of about 10.sup.10 to 10.sup.14 ohm. cm and a surface coat powder having an electrical resistivity of about 10.sup.14 to 10.sup.16 ohm. cm. Advantageously the surface tension of the ground coat amounts to at least about 0.280 N/m and the surface tension of the surface coat to at most about 0.260 N/m, the difference between the surface tensions of the ground coat and surface amounts to at least about 0.050 N/m, the ground coat powder has an electrical resistivity 10.sup.12 to 10.sup.14 ohm. cm and at least about 10.sup.2 ohm. cm lower than that of the surface coat powder, the ground coat powder contains at least one of an alkaline earth metal, zinc, manganese or iron oxide in a total concentration of about 20 to 30% by weight, the zinc oxide content not exceeding about 12% by weight and the manganese oxide plus iron oxide content not exceeding about 9% by weight, about 3 to 5% by weight of finely divided iron oxide is added to the ground coat powder before adjustment of its electrical resistivity, and the ground coat powder is applied in such a quantity that, after baking, the ground coat has a layer thickness of about 0.02 to 0.03 mm.
    • 在其中将地面涂层和表面涂层粉末静电施加到金属基底上并随后烘烤在一起的两层搪瓷方法中,其改进包括使用电阻率为约1010至1014欧姆的底涂粉末。 cm和表面涂层粉末,其电阻率为约1014至1016欧姆。 厘米。 有利地,地面涂层的表面张力至少为约0.280N / m,表面涂层的表面张力至多为约0.260N / m,底涂层和表面的表面张力之间的差异至少等于 约0.050N / m,底涂层粉末的电阻率为1012至1014欧姆。 cm至少约102欧姆。 cm以下,底涂粉末含有总量为20〜30重量%的碱土金属,锌,锰或氧化铁中的至少一种,氧化锌含量不超过约 12重量%,氧化锰加氧化铁含量不超过约9重量%,约3-5重量%的细碎铁氧化物在调节其电阻率之前加入到底漆中,并将研磨的涂层 粉末的施加量使得在烘烤后,底涂层的层厚度为约0.02至0.03mm。