    • 10. 发明授权
    • Method for producing borosilicate glasses
    • 硼硅酸盐玻璃的制造方法
    • US07490486B2
    • 2009-02-17
    • US10480183
    • 2002-06-07
    • Karin NaumannChristof KassFranz Ott
    • Karin NaumannChristof KassFranz Ott
    • C03B5/16C03B5/00C03C3/091C03C3/093
    • C03C1/004C03C3/091
    • The process of producing a refined borosilicate glass includes preparing a glass batch with a composition in wt. % on the basis of oxide content of SiO2, 65-82; Al2O3, 2-8; B2O3, 5-13; MgO+CaO+SrO +BaO+ZnO, 0-7; ZrO2, 0-2; and Li2O+Na2O+K2O, 3-10; adding 0.05 wt. % to 0.6 wt. % of sulfate(s) expressed as SO3 to the glass batch as the refining agent; melting the glass batch including the refining agent to form melted glass; and then hot-shaping the borosilicate glass. The refining agent may also include from 0.01 wt. % to 0.6 wt. % of F− or from 0.015 wt. % to 0.6 wt. of Cl−. The sulfate is preferably an alkali metal and/or alkaline earth metal sulfate or sulfates.
    • 制备精制硼硅酸盐玻璃的方法包括制备具有重量百分比的组合物的玻璃批料。 基于SiO2的氧化物含量%,65-82; Al2O3,2-8; B2O3,5-13; MgO + CaO + SrO + BaO + ZnO,0-7; ZrO2,0-2; 和Li2O + Na2O + K2O,3-10; 加入0.05wt。 %至0.6wt。 作为澄清剂的以SO 3表示的硫酸盐的量为玻璃批料; 熔化包括澄清剂的玻璃料以形成熔融玻璃; 然后热成型硼硅酸盐玻璃。 澄清剂还可以包括0.01wt。 %至0.6wt。 %的F-或0.015wt。 %至0.6wt。 的Cl-。 硫酸盐优选为碱金属和/或碱土金属硫酸盐或硫酸盐。