    • 3. 发明申请
    • Optical fiber and optical transmission path
    • 光纤和光传输路径
    • US20030215201A1
    • 2003-11-20
    • US10437052
    • 2003-05-14
    • FUJIKURA LTD.
    • Shoji TanigawaShoichiro MatsuoKuniharu HimenoKoichi Harada
    • G02B006/16G02B006/22
    • G02B6/03694G02B6/02247G02B6/02285G02B6/03611G02B6/03627G02B6/03644G02B6/03666G02B6/29377
    • Under condition that a non-circularity ratio is 5% or lower and a thermal expansion coefficient of a glass which forms the core is null1 and a thermal expansion of a glass which forms the cladding is null2, the difference of coefficients is controlled such that a formula null2.5null10null7/null C.nullnull1nullnull2null1.0null10null7/null C. is satisfied so as to maintain a polarization mode dispersion to be 0.03 ps/km0.5 or lower. The difference of coefficients is further controlled such that a formula null1.5null10null7/null C.nullnull1nullnull2null0/null C. is satisfied so as to maintain a polarization mode dispersion to be 0.015 ps/km0.5 or lower. By doing this, birefringence is reduced by adjusting the thermal expansion coefficient in a core and a cladding; thus providing an optical fiber, and an optical transmission path using the optical fiber, having preferable PMD for high speed transmission.
    • 在非圆度比为5%以下,形成芯的玻璃的热膨胀系数为α1,形成包层的玻璃的热膨胀为α2的条件下,控制系数差,使得 满足公式-2.5×10 -7 /℃。<=α1-α2<= 1.0×10 -7 /℃,以便将偏振模色散维持在0.03ps / km <0.5>或更低 。 进一步控制系数的差异,使得满足公式-1.5×10 -7 /℃<=α1-α2<= 0 /℃,以便将偏振模色散维持为0.015ps / km <0.5>以下。 通过这样做,通过调节芯和包层中的热膨胀系数来减少双折射; 从而提供一种光纤,以及使用该光纤的光传输路径,具有优选用于高速传输的PMD。
    • 5. 发明申请
    • Optical fiber drawing die and drawing method therefor
    • 光纤拉丝模及其拉丝方法
    • US20030136340A1
    • 2003-07-24
    • US10313402
    • 2002-12-06
    • Fujikura Ltd.
    • Munehisa FujimakiTakahiro HamadaKoichi Harada
    • B29D011/00
    • B29D11/00663B29L2011/0075
    • An optical fiber coating die is made such that an interfacial shear rate of the optical fiber to the resin coat is calculated in accordance with a pressure value of resin inside a coating cup, and the interfacial shear rate is in a range of null1.5null105 to 0 secnull1. Also, an optical fiber drawing die is made such that the interfacial shear rate of the optical fiber to the resin coat is calculated in accordance with a diameter of a coating resin, and the interfacial shear rate is in a range of range of null3null105 to 2null105 secnull1. By doing this, an optical fiber drawing die which can be used in an optical fiber drawing method so as to realize stable resin coating operation even in high-speed drawing operation and high productivity can be realized.
    • 制造光纤涂层模具,使得光纤与树脂涂层的界面剪切速率根据涂覆杯内的树脂的压力值计算,并且界面剪切速率在-1.5×10 5〜 0秒-1。 此外,制造光纤拉伸模具,使得光纤与树脂涂层的界面剪切速率根据涂布树脂的直径计算,并且界面剪切速率在-3×10 5〜 2x105秒-1。 通过这样做,可以实现即使在高速拉丝操作和高生产率下也能够用于光纤拉伸方法以实现稳定的树脂涂布操作的光纤拉伸模。