    • Method of producing vapor grown carbon fibers using coal
    • 使用煤生产气相生长碳纤维的方法
    • US5846509A
    • 1998-12-08
    • US526169
    • 1995-09-11
    • Robert L. AligDavid J. Burton
    • Robert L. AligDavid J. Burton
    • D01F9/127D01F9/12
    • B82Y30/00D01F9/1272
    • A method of producing vapor grown carbon fibers is provided in which coal is utilized as a source of an iron catalyst, as a source of hydrocarbon and sulfur, or both. The method includes the steps of introducing pulverized coal into a furnace containing a gas selected from the group consisting of hydrogen, hydrocarbon, nitrogen, ammonia, helium, or mixtures thereof, and maintaining the gas at a temperature from about 1000.degree.-1175.degree. C. to form the fibers. The coal has a sulfur content of from 1 to 6% by weight and may comprise high volatile bituminous coal. The use of coal to produce vapor grown carbon fibers provides a significant cost advantage over other starting materials and also provides an environmentally safe use for high sulfur content coal.
    • 提供了生产气相生长碳纤维的方法,其中使用煤作为铁催化剂的来源,作为烃和硫的来源,或两者。 该方法包括以下步骤:将粉煤引入含有选自氢,烃,氮,氨,氦或其混合物的气体的炉中,并将气体保持在约1000-111℃的温度 形成纤维。 煤的硫含量为1至6重量%,可包含高挥发性烟煤。 使用煤来生产气相生长碳纤维比其他起始材料具有显着的成本优势,并且还为高硫含量煤提供了环境安全的用途。
    • 5. 发明授权
    • Adjustable linkage
    • 可调联动
    • US6164017A
    • 2000-12-26
    • US226365
    • 1999-01-06
    • David J. Burton
    • David J. Burton
    • E04H3/28F16C11/04
    • E04H3/28
    • A folding stage includes a spacing linkage that is adjustable. The spacing linkage locks the folding stage at its final use position. The linkage includes an adjustable link member having an adjustment device. The adjustment device provides for changing the length of the link. The adjustment device includes a housing having a block slidably mounted therein. The housing and the block both include transverse openings for receiving a pivot bolt. The end of the housing receives a bolt threadably connected to the sliding block. A nut on the exterior of the housing threadably connects to the bolt and positions the block relative to the end of the housing for adjusting the length of the link and the position of the spacing linkage.
    • 折叠台包括可调节的间隔连杆。 间隔连接将折叠台锁定在其最终使用位置。 联动装置包括具有调节装置的可调节连杆构件。 调整装置提供改变链接的长度。 调节装置包括具有可滑动地安装在其中的块的壳体。 壳体和块都包括用于接收枢转螺栓的横向开口。 壳体的端部接收螺纹连接到滑块的螺栓。 壳体外部的螺母可螺纹地连接到螺栓并且相对于壳体的端部定位该块,用于调节连杆的长度和间隔连杆的位置。
    • 6. 发明授权
    • Vapor grown carbon fibers with increased bulk density and method for
making same
    • 具有增加体积密度的气相生长碳纤维及其制造方法
    • US5594060A
    • 1997-01-14
    • US480246
    • 1995-06-07
    • Robert L. AligJason R. GuthDavid J. Burton
    • Robert L. AligJason R. GuthDavid J. Burton
    • C08K7/06D01F11/14C08K3/04B32B5/16
    • D01F11/14C08K7/06
    • Carbon fiber with increased bulk density comprising vapor grown carbon fiber is provided. The preferred method of increasing the carbon fiber bulk density comprises mixing a vapor grown carbon fiber with a diameter of less than about 1 .mu.m and an initial bulk density of less than about 0.2 lb/ft.sup.3 with an aqueous-based solution, blending the mixture under high shear conditions, and drying the blended mixture. Upon drying, the mixture forms a carbon fiber mass with an increased bulk density having a final bulk density of at least about 3 lb/ft.sup.3. The increased bulk density carbon fiber pellets are ideally suited for use as reinforcing materials in rubber, plastic and the like. Preferably, the aqueous-based solution is a latex containing solution and latex is deposited on the fibers.
    • 提供了包含气相生长碳纤维的具有增加的堆积密度的碳纤维。 增加碳纤维堆积密度的优选方法包括用水基溶液混合直径小于约1μm的初始堆积密度的小于或等于约0.2lb / ft 3的气相生长碳纤维,将混合物 在高剪切条件下干燥混合的混合物。 干燥后,混合物形成具有至少约3lb / ft 3的最终堆积密度的堆积密度增加的碳纤维块。 增加堆积密度的碳纤维颗粒理想地适合用作橡胶,塑料等中的增强材料。 优选地,水基溶液是含乳胶的溶液,并且胶乳沉积在纤维上。