会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 6. 发明授权
    • Use of LNA in mass spectrometry
    • 在质谱中使用LNA
    • US06436640B1
    • 2002-08-20
    • US09528705
    • 2000-03-18
    • Adrian SimmonsClifford Smith
    • Adrian SimmonsClifford Smith
    • C12Q168
    • C12Q1/6827C12Q2565/627C12Q2525/113
    • DNA and RNA diagnostics based on mass spectrometry, e.g. Matrix-Assisted Laser Desorption/Ionisation Time-of-Flight (MALDI-TOF) mass spectrometry, Electrospray (ES) mass spectrometry, Ion Cyclotron Resonance (ICR) mass spectrometry, Fourier Transform mass spectrometry, or combinations thereof, where fully or partially LNA modified DNA probes are used in order to enhance stability and resolution. The invention in particular relates to a process for detecting a target nucleic acid sequence of a nucleic acid molecule or for detecting a mutation in a nucleic acid sequence of a nucleic acid molecule, wherein (a) the nucleic acid molecule or (b) a part of the nucleic acid molecule or (c) an oligonucleotide complementary to the sequence or at least a sub-sequence of the nucleic acid molecule is analysed by mass spectrometry in order to obtain direct or indirect information about the target nucleic acid sequence or mutation, and wherein the process involves the hybridisation of an LNA modified oligonucleotide to the nucleic acid molecule.
    • 基于质谱的DNA和RNA诊断,例如 基质辅助激光解吸/电离飞行时间(MALDI-TOF)质谱,电喷雾(ES)质谱,离子回旋共振(ICR)质谱,傅立叶变换质谱或其组合,其中全部或部分LNA 使用修饰的DNA探针以增强稳定性和分辨率。 本发明特别涉及用于检测核酸分子的靶核酸序列或检测核酸分子的核酸序列中的突变的方法,其中(a)核酸分子或(b)部分 的核酸分子或(c)通过质谱分析与核酸分子的序列或至少子序列互补的寡核苷酸,以获得关于靶核酸序列或突变的直接或间接信息,以及 其中所述方法涉及LNA修饰寡核苷酸与核酸分子的杂交。
    • 10. 发明申请
    • Composite tool coating system
    • 复合工具涂装系统
    • US20050025893A1
    • 2005-02-03
    • US10798768
    • 2004-03-11
    • Clifford Smith
    • Clifford Smith
    • C23C4/02C23C4/18B05D1/36
    • C23C4/02C23C4/18
    • My invention is a sequentially applied composite coating process that combines plate coating and spray coating techniques into an integrated system. A component, or part, is plated with a suitable material to build up surfaces of the part to a desired prepared specification. The part is then coated with a second molten material sprayed on, integrally bonding the spray-coating material into the plated-coating material layer of the part, to achieve the final spray coated composite material. Final grinding and/or polishing finish preparation may follow. Various materials and/or blends of materials known to the field of each individual art may be used in the plating stage and the spraying stage. In this fashion a relatively thick coating of highly durable material may be applied with superior bonding properties than achievable through currently practiced methods.