    • 4. 发明授权
    • Cuprous pyrophosphate glasses
    • 焦磷酸铜眼镜
    • US5529961A
    • 1996-06-25
    • US367465
    • 1994-12-30
    • Bruce G. AitkenGeorge H. BeallJames E. Dickinson, Jr.
    • Bruce G. AitkenGeorge H. BeallJames E. Dickinson, Jr.
    • C03C3/16C03C3/17C03C3/19C03C3/21
    • C03C3/16
    • The subject invention is directed at glasses wherein either a portion of the ZnO or alkali metals, or both, is replaced by Cu.sub.2 O, i.e., monovalent copper. Specifically, the present invention is directed at a glass consisting essentially of, expressed in terms of mole percent on the oxide basis, 28-42% P.sub.2 O.sub.5, 15-30% Cu.sub.2 O, 10-30% R.sub.2 O, wherein R.sub.2 O is selected from the group consisting of 0-15% Li.sub.2 O, 0-20% Na.sub.2 O, and 0-10% K.sub.2 O, and up to a total of 45% of optional ingredients in the indicated proportions selected from the group consisting of 0-10% Al.sub.2 O.sub.3, 0-15% MgO, 0-20% CaO, 0-20% SrO, 0-20% BaO, 0-25% MgO+CaO+SrO+BaO, 0-35% ZnO, 0-10% MnO, 0-2% CeO.sub.2, 0-2% Ln.sub.2 O.sub.3, 0-10 Al.sub.2 O.sub.3 0-10% B.sub.2 O.sub.3, 0-10 Fe.sub.2 O.sub.3 0-10% Al.sub.2 O.sub.3 +B.sub.2 O.sub.3 +Fe.sub.2 O.sub.3, 0-7% MoO.sub.3 0-7% WO.sub.3 0-7% MoO.sub.3 +WO.sub.3, and 0-8% F, the latter as analyzed in weight percent. In addition, it is necessary that the predominate proportion of the copper in the glass is present in the cuprous or Cu.sup.+ oxidation state. These inventive glasses exhibit a transition temperature normally below about 300.degree. C., a working temperature below about 400.degree. C., while, at the same time, exhibiting excellent resistance to attack by water.
    • 本发明涉及其中一部分ZnO或碱金属或两者都被Cu 2 O替代的玻璃,即一价铜。 具体地说,本发明涉及基本上由以氧化物为基准的摩尔百分数表示的玻璃,28-42%的P2O5,15-30%的Cu2O,10-30%的R2O,其中R2O选自 由0-15%的Li 2 O,0〜20%的Na 2 O和0〜10%的K 2 O组成,最多可以以指定的比例选择总量为45%的选自0-10%的Al 2 O 3, 15%MgO,0-20%CaO,0-20%SrO,0-20%BaO,0-25%MgO + CaO + SrO + BaO,0-35%ZnO,0-10%MnO,0-2% CeO2,0-2%Ln2O3,0-10Al2O3 0-10%B2O3,0-10Fe2O3 0-10%Al2O3 + B2O3 + Fe2O3,0-7%MoO3 0-7%WO3 0-7%MoO3 + WO3, 和0-8%F,后者以重量百分比分析。 此外,玻璃中铜的主要比例必须以亚铜或Cu +氧化态存在。 这些本发明的玻璃的转变温度通常低于约300℃,工作温度低于约400℃,同时表现出优异的耐水侵蚀性。
    • 5. 发明授权
    • Cuprous metaphosphate glasses
    • 亚硫酸偏磷酸盐眼镜
    • US5529960A
    • 1996-06-25
    • US367466
    • 1994-12-30
    • Bruce G. AitkenGeorge H. BeallJames E. Dickinson, Jr.
    • Bruce G. AitkenGeorge H. BeallJames E. Dickinson, Jr.
    • C03C3/17C03C3/21C03C3/16C03C3/19
    • C03C3/21C03C3/17
    • The subject invention is directed at wherein either a portion of the ZnO or alkali metals, or both, found in prior art glasses, is replaced by Cu.sub.2 O, i.e., cuprous or monovalent copper. In addition to the Cu.sub.2 O substitution, the inventive glass contains a required metal oxide constituent which is necessary to enhance durability. More specifically, the present invention discloses a glass consisting essentially of, expressed in terms of mole percent on the oxide basis, of about 42-54% P.sub.2 O.sub.5, 10-30% Cu.sub.2 O, 10-30% R.sub. O and 3-12% of a component selected from the group consisting of 0-7% MoO.sub.3, 0-10 Fe.sub.2 O.sub.3, 0-10% Al.sub.2 O.sub.3 and 0-7%WO.sub.3. In addition, the composition includes up to a total of 45% of optional ingredients in the indicated proportions selected from the group consisting of 0-15% MgO, 0-20% CaO, 0-20% SrO, 0-20% BaO, 0-25% MgO+CaO+SrO+BaO, 0-35% ZnO, 0-10% MnO, 0-2% CeO.sub.2, 0-10% B.sub.2 O.sub.3, 0-2% Ln.sub.2 O.sub.3 , 0-8% F, the latter as analyzed in weight percent. The R.sub.2 O constituent is selected from the group consisting of 0-15% Li.sub.2 O, 0-20% Na.sub.2 O, and 0-10% K.sub.2 O. Furthermore, the Al.sub.2 O.sub.3 +Fe.sub.2 O.sub.3 does not exceed 10% and the MoO.sub.3 +WO.sub.3 does not exceed 7%. One final requirement of the glass is that the predominate proportion of the copper is present in the Cu.sup.+ or monovalent oxidation state.
    • 本发明涉及其中在现有技术的玻璃中发现的ZnO或碱金属的一部分或两者的一部分被Cu 2 O替代,即亚铜或一价铜。 除了Cu2O的取代之外,本发明的玻璃还含有必要的金属氧化物成分,这是提高耐久性所必需的。 更具体地说,本发明公开了一种玻璃,其基本上由以氧化物为基准的摩尔百分数表示,约42-54%的P 2 O 5,10-30%的Cu 2 O,10-30%的RO和3-12%的 选自0-7%MoO 3,0-10 Fe 2 O 3,0-10%Al 2 O 3和0-7%WO 3的组分。 此外,该组合物包含至多总计45%的任选成分,所指定的比例选自0-15%MgO,0-20%CaO,0-20%SrO,0-20%BaO, 0-25%MgO + CaO + SrO + BaO,0-35%ZnO,0-10%MnO,0-2%CeO 2,0-10%B 2 O 3,0-2%Ln 2 O 3,0-8%F 按重量百分比分析。 R2O成分选自0-15%Li2O,0-20%Na2O和0-10%K2O。 此外,Al2O3 + Fe2O3不超过10%,MoO3 + WO3不超过7%。 玻璃的一个最终要求是铜的主要比例存在于Cu +或一价氧化态中。
    • 9. 发明授权
    • Molecular, inorganic glasses
    • 分子,无机眼镜
    • US06503859B1
    • 2003-01-07
    • US09894587
    • 2001-06-28
    • Bruce G. Aitken
    • Bruce G. Aitken
    • C03C332
    • C03C3/321C03C4/10
    • The invention resides in a molecular, inorganic glass and a method of making the glass, the glass being vitreous and resistant to devitrification, that is composed, in substantial part at least, of thermally-stable, zero-dimensional clusters or molecules, composed of four atoms of arsenic and three atoms of sulfur, the glass further containing up to 12 atomic percent of germanium, adjoining clusters being bonded to each other primarily by van der Waals forces, and at least 95% of the glass composition consisting of 42-60% arsenic, 37-48% sulfur plus selenium, the selenium being 0-14%.