    • 1. 发明申请
    • Method for local application of diffusion aluminide coating
    • 局部应用扩散铝化物涂层的方法
    • US20070009660A1
    • 2007-01-11
    • US10552719
    • 2005-08-08
    • Akiko SasakiNarihito OhiShigekazu MunedaHideo Takahashi
    • Akiko SasakiNarihito OhiShigekazu MunedaHideo Takahashi
    • B05D3/00C23C16/00
    • F01D5/005C23C10/02C23C10/04C23C10/18C23C10/30C23C10/48F01D5/288F05D2230/80F05D2230/90F05D2300/611
    • A method includes a component preparation step 10 of exposing local areas (damaged areas of an existing coating) of a base material of a metal component 1 to be coated, and roughening a surface of the base material to a desired surface roughness, a slurry preparation step 12 of preparing a coating slurry that contains a halide activator, a water soluble organic binder, and powder of an aluminum-containing intermetallic compound 3, an application and drying step 14 of applying the coating slurry to the damaged areas of the metal component, and then drying the areas, a packing step 16 of packing the metal component in a heat-resistant container filled with alumina powder, a diffusion treatment step 18 of retaining the heat-resistant container at high temperature in an inert atmosphere or a reducing atmosphere to diffuse aluminum onto the surface of the metal component, and a cleaning step 20 of taking out the metal component from the heat resistant container, and removing a slag from the surface of the metal component.
    • 一种方法包括:组分准备步骤10,其将要涂覆的金属组分1的基材的局部区域(现有涂层的损坏区域)暴露,并将基材的表面粗糙化至所需的表面粗糙度;浆料制备 制备包含卤化物活化剂,水溶性有机粘合剂和含铝金属间化合物3的粉末的涂料浆料的步骤12,将涂料浆料涂覆到金属组分的损坏区域的涂布和干燥步骤14, 然后干燥该区域,将填充氧化铝粉末的耐热容器中的金属成分填充的填充工序16,在惰性气氛或还原气氛中将耐热容器保持在高温下的扩散处理工序18 将铝扩散到金属部件的表面上,以及清洁步骤20,从耐热容器中取出金属成分,并从 金属部件的表面。