    • 1. 发明授权
    • Light-conversion flexible polymer material and use thereof
    • 光转换柔性聚合物材料及其用途
    • US09068077B2
    • 2015-06-30
    • US13496548
    • 2010-09-15
    • Zhiguo XiaoYing ChangYulong SuiYuening WuMaolong Li
    • Zhiguo XiaoYing ChangYulong SuiYuening WuMaolong Li
    • C08L83/00C08K3/24C08K3/34C08K3/30H01L33/00F21V9/10C08L83/04C09K11/02C08G77/04H01L33/50
    • C08L83/04C08G77/04C08K3/24C09K11/02H01L33/501H01L33/505C08L83/00
    • A light-conversion flexible polymer material consists of an organic silicone rubber (bi-component addition thermal vulcanizing liquid silicone rubber, 20.0-75.0%), a diluting agent (silicone oil, 10.0-20.0%), a luminescent material (one or more of aluminate, silicate, siliconitride and oxysulfide luminescent materials, 15.0-65.0%) and auxiliary. The polymer material can be bent randomly as required. The polymer material is made by mixing raw materials uniformly in a blending container, inpouring the obtained mixture into a mold and thermal-curing. The polymer material is used on the surface of a blue-light LED and the luminescent material in the light-conversion flexible polymer material can be excitated by light emitted from the blue light LED to give out light, which is combined with residual blue light into white light. The polymer material can be widely used in light-source devices such as lamp, nixie tube and backlight.
    • 光转换柔性聚合物材料由有机硅橡胶(双组分加成热硫化液硅橡胶,20.0-75.0%),稀释剂(硅油,10.0-20.0%),发光材料(一种或多种) 的铝酸盐,硅酸盐,硅氮化物和氧硫化物发光材料,15.0-65.0%)和辅助剂。 聚合物材料可以根据需要随机弯曲。 聚合物材料通过将原料均匀地混合在共混容器中,将所得混合物浸入模具中并热固化而制成。 聚合物材料用于蓝光LED的表面,并且光转换柔性聚合物材料中的发光材料可以被从蓝色LED发出的光激发,以发出与剩余蓝色光合并的光 白光。 聚合物材料可广泛用于灯具,数码管和背光源等光源装置中。
    • 3. 发明申请
    • WATERPROOF SELF-LUMINESCENT SPRAY-PAINTED FILM
    • 防水自发光喷涂膜
    • US20120058322A1
    • 2012-03-08
    • US13266679
    • 2010-04-28
    • Zhiguo XiaoMaolong LiYingying LiKuiwu ShaoHongwei Zhang
    • Zhiguo XiaoMaolong LiYingying LiKuiwu ShaoHongwei Zhang
    • B32B7/02B05D3/02B05D1/28B05D1/42B05D1/18B05D5/00B05D1/02
    • B41M5/508B41M5/52B41M5/5218B41M5/5227B41M5/5245B41M5/5254Y10T428/24975
    • The invention provides a waterproof self-luminescent spray-painted film with a thickness of 0.150-1.560 mm. The film has, from top to bottom, ink reception layer (1), connection layer (2) and light-storing photo-luminescent film (3); wherein the ink reception layer (1) is prepared by mixing inorganic filler, adhesive, color fixing agent, coupling agent, surfactant, cross-linking agent, fluorescent whitening agent and water at a ratio. The film has good waterproof property, rapid ink-drying, clear image after being ink-jet printed, and high color density. The film is self-luminescent after absorbing external visible light, and is visible and has the illumination function of low lighting intensity in darkness after a pattern or character is printed on the surface of the film. The film can be widely used in various occasions, such as home decoration, hotels, corridors, office buildings, cinemas, warehouses, ship cabins, underpasses and the places in need of large scale printing and high-precision patterns.
    • 本发明提供了一种厚度为0.150-1.560mm的防水自发光喷涂膜。 该墨水从上到下具有墨水接收层(1),连接层(2)和储光光致发光膜(3)。 其中所述油墨接收层(1)通过以一定比例混合无机填料,粘合剂,着色剂,偶联剂,表面活性剂,交联剂,荧光增白剂和水来制备。 该胶片具有良好的防水性能,快速的油墨干燥,喷墨打印后的图像清晰,色彩浓度高。 在吸收外部可见光之后,该膜是自发光的,并且在图案或字符被印刷在膜的表面上之后,在黑暗中具有低照明强度的照明功能。 该电影可广泛应用于家居装饰,酒店,走廊,办公楼,电影院,仓库,船舱,地下通道等需要大型印刷和高精度图案的场合。
    • 5. 发明申请
    • SILICATE PHOSPHOR AND ITS MANUFACTURE METHOD AS WELL AS LIGHT-EMITTING DEVICE USING THE SAME
    • 硅酸盐及其制造方法作为使用其的发光装置
    • US20080031797A1
    • 2008-02-07
    • US11754432
    • 2007-05-29
    • Wei XiaJing XuGuangxu LinXifeng WangZhiguo Xiao
    • Wei XiaJing XuGuangxu LinXifeng WangZhiguo Xiao
    • C01F17/00
    • C09K11/774C09K11/7734C09K11/7792C09K11/7796C09K11/7797Y02B20/181
    • The invention relates to an ultraviolet to green light region silicate phosphor capable of being excited by radiation light source and its manufacturing method, particularly to white and multicolor systems light-emitting device. The material has luminous color in the range from blue to red color system. The essential composition of the phosphor is aMO.bM′O.SiO2.cR:xEu.yLn.zLv.δLm, wherein M is an element or a combination of elements selected from the group consisting of Sr, Ca, Ba and Zn; M′ is an element or a combination of elements selected from the group consisting of Mg, Cd and Be; R is one or two of B2O3 and P2O5; Ln is an element or a combination of elements selected from the group consisting of Nd, Dy, Ho, Tm, La, Ce, Er, Pr, Bi, Sm, Sn, Y, Lu, Ga, Sb, Tb, Mn and Pb; Lv is an element or a combination of elements selected from the group consisting of Cl, F, Br, I and S; Lm is an element or a combination of elements selected from the group consisting of Li, Na and K
    • 本发明涉及能够被辐射光源激发的紫外至绿光区域硅酸盐荧光体及其制造方法,特别涉及白色和多色系统的发光装置。 该材料具有从蓝色到红色系统范围内的发光颜色。 荧光体的基本组成是M 1,M 2 SiO 2,cR:xEu.yLn.zLv.deltaLm,其中M是元素或选自Sr ,Ca,Ba和Zn; M'是选自Mg,Cd和Be的元素或元素的组合; R是B 2 O 3和P 2 O 5 5中的一个或两个; Ln是选自Nd,Dy,Ho,Tm,La,Ce,Er,Pr,Bi,Sm,Sn,Y,Lu,Ga,Sb,Tb,Mn和Pb中的元素或元素的组合 ; Lv是选自Cl,F,Br,I和S的元素或元素的组合; Lm是选自Li,Na和K的元素或元素的组合
    • 8. 发明授权
    • Silicate phosphor and its manufacture method as well as light-emitting device using the same
    • 硅酸盐荧光粉及其制造方法以及使用其的发光装置
    • US07998364B2
    • 2011-08-16
    • US11754432
    • 2007-05-29
    • Wei XiaJing XuGuangxu LinXifeng WangZhiguo Xiao
    • Wei XiaJing XuGuangxu LinXifeng WangZhiguo Xiao
    • C09K11/59C09K11/63C09K11/73C09K11/55C09K11/54
    • C09K11/774C09K11/7734C09K11/7792C09K11/7796C09K11/7797Y02B20/181
    • The invention relates to an ultraviolet to green light region silicate phosphor capable of being excited by radiation light source and its manufacturing method, particularly to white and multicolor systems light-emitting device. The material has luminous color in the range from blue to red color system. The essential composition of the phosphor is aMO.bM′O.SiO2.cR:xEu.yLn.zLv.δLm, wherein M is an element or a combination of elements selected from the group consisting of Sr, Ca, Ba and Zn; M′ is an element or a combination of elements selected from the group consisting of Mg, Cd and Be; R is one or two of B2O3 and P2O5; Ln is an element or a combination of elements selected from the group consisting of Nd, Dy, Ho, Tm, La, Ce, Er, Pr, Bi, Sm, Sn, Y, Lu, Ga, Sb, Tb, Mn and Pb; Lv is an element or a combination of elements selected from the group consisting of Cl, F, Br, I and S; Lm is an element or a combination of elements selected from the group consisting of Li, Na and K.
    • 本发明涉及能够被辐射光源激发的紫外至绿光区域硅酸盐荧光体及其制造方法,特别涉及白色和多色系统的发光装置。 该材料具有从蓝色到红色系统范围内的发光颜色。 荧光体的基本组成是M,SbMO,SiO 2,cR:xEu.yLn.zLv.δLm,其中M是选自Sr,Ca,Ba和Zn的元素或元素的组合; M'是选自Mg,Cd和Be的元素或元素的组合; R是B2O3和P2O5中的一种或两种; Ln是选自Nd,Dy,Ho,Tm,La,Ce,Er,Pr,Bi,Sm,Sn,Y,Lu,Ga,Sb,Tb,Mn和Pb中的元素或元素的组合 ; Lv是选自Cl,F,Br,I和S的元素或元素的组合; Lm是选自Li,Na和K的元素或元素的组合。