    • A roll and process for producing same are disclosed. This process includes the steps of: horizontally placing a core body made of a cast steel or a steel based Adamite containing from 0.5 to 2.5 %C, said core body having one or more circumferential grooves; feeding a consumable electrode wire into said groove or grooves, while rotating said core body, to thereby obtain according to an electro-slag welding process a deposited metal or metals filled in said groove or grooves, said deposited metal or metals containing from 1.5 to 2.5%C, from 0.2 to 1.0% Si, from 0.5 to 1.0% Mn, from 0.5 to 3.0 % Cr, from 0.2 to 3.0 % Mo, from 0 to 2.0 V, the balance being essentially Fe, and inevitable impurities; subjecting same to heat treatment at a temperature ranging from 500.degree. C to 700.degree. C; or feeding a consumable electrode wire into said groove or grooves, while rotating said core body, to thereby build-up a steel based Adamite deposited metal or metals over the surfaces of said groove or grooves to fill same according to an electro-slag welding process, the aforesaid Adamite deposited metal or metals containing from 1.5 to 2.5 % C and other suitable alloy elements and being built-up to a radial thickness ranging from 20 mm to 1/10 of the original diameter of said core body.
    • 公开了一种卷及其制造方法。 该方法包括以下步骤:水平放置由铸铁或含有0.5至2.5%C的钢基的矿物制成的芯体,所述芯体具有一个或多个圆周槽; 在将所述芯体旋转的同时,将可消耗电极线馈送到所述槽或槽中,从而根据电渣焊接工艺获得填充在所述槽或槽中的沉积金属或金属,所述沉积的金属或金属含有1.5至2.5 %C,0.2〜1.0%Si,0.5〜1.0%Mn,0.5〜3.0%Cr,0.2〜3.0%Mo,0〜2.0V,余量基本为Fe,不可避免的杂质; 在500〜700℃的温度下对其进行热处理; 或在将所述芯体旋转的同时将消耗性电极线供给到所述槽或槽中,从而在所述槽或槽的表面上积累钢基的Adamite沉积金属或金属,以根据电渣焊接工艺 ,上述Adamite沉积的金属或含有1.5至2.5%C的金属和其它合适的合金元素,并被构建成径向厚度为所述芯体原始直径的20至1/10。