    • 1. 发明授权
    • Polyurethane PSA
    • 聚氨酯PSA
    • US07160976B2
    • 2007-01-09
    • US10816277
    • 2004-04-01
    • Bernd LühmannPhilippe HesseSianty SunartoUwe SchümannKirstin WeilandCarsten Böhmer
    • Bernd LühmannPhilippe HesseSianty SunartoUwe SchümannKirstin WeilandCarsten Böhmer
    • C08G18/48
    • C08G18/4866C08G18/4812C08G18/755C08G2170/40C09J175/08Y10T428/31551
    • Pressure-sensitive adhesive based on polyurethane, characterized in that the polyurethane is composed of the following starting materials which are reacted with one another in the stated proportions: a) at least one aliphatic or alicyclic diisocyanate having in each case an asymmetrical molecular structure, b) a combination of at least one polypropylene glycol diol and at least one polypropylene glycol triol, the ratio of the number of hydroxyl groups in the diol component to the number of hydroxyl groups in the triol component being between 0.7 and 9.0, preferably between 1.5 and 2.5, additionally the ratio of the number of isocyanate groups to the total number of hydroxyl groups being between 0.9 and 1.1, preferably between 0.95 and 1.05, and the diols and triols alternatively being selected and combined in each case as follows: diols having a molecular weight of less than or equal to 1000 are combined with triols whose molecular weight is greater than 1000, preferably greater than or equal to 3000, diols having a molecular weight of greater than 1000 are combined with triols whose molecular weight is less than 1000.
    • 基于聚氨酯的压敏粘合剂,其特征在于,所述聚氨酯由以下起始原料组成,所述原料以规定的比例彼此反应:a)至少一种脂族或脂环族二异氰酸酯,在每种情况下均为不对称分子结构,b )至少一种聚丙二醇二醇和至少一种聚丙二醇三醇的组合,二醇组分中的羟基数与三醇组分中的羟基数之比为0.7至9.0,优选为1.5至 另外,异氰酸酯基数与羟基总数的比例在0.9和1.1之间,优选在0.95和1.05之间,二醇和三醇在各种情况下可以选择和组合,如下所示:具有分子 小于或等于1000的重量与分子量大于1000,优选大于o的三醇组合 r等于3000,分子量大于1000的二醇与分子量小于1000的三醇组合。
    • 6. 发明申请
    • Polyurethane PSA for sensitive surfaces
    • 聚氨酯PSA用于敏感表面
    • US20050027091A1
    • 2005-02-03
    • US10815894
    • 2004-04-01
    • Bernd LuhmannPhilippe HesseSianty SunartoUwe SchumannKirstin WeilandCarsten Bohmer
    • Bernd LuhmannPhilippe HesseSianty SunartoUwe SchumannKirstin WeilandCarsten Bohmer
    • C08G18/22C08G18/48C08G18/73C08G18/75C08G18/00
    • C08G18/4866C08G18/227C08G18/4808C08G18/4812C08G18/73C08G18/755C08G2170/40Y10T428/31551
    • Polyurethane-based pressure-sensitive adhesive, characterized in that the polyurethane is composed of the following starting materials which are reacted catalytically with one another in the stated proportions: a) at least one aliphatic or alicyclic polyisocyanate having a functionality of in each case less than or equal to three, b) a combination of at least one polypropylene glycol diol and at least one polypropylene glycol triol, the ratio of the number of hydroxyl groups in the diol component to the number of hydroxyl groups in the triol component being less than 10, preferably between 0.2 and 5, additionally the ratio of the number of isocyanate groups to the total number of hydroxyl groups being between 0.8 and 1.15, preferably between 0.95 and 1.05, more preferably between 1.0 and 1.05, the catalyst for the reaction to the polyurethane consisting of or comprising a bismuth carboxylate or bismuth carboxylate derivative, and the diols and triols alternatively being selected and combined in each case as follows: diols having a molecular weight of less than or equal to 1000 are combined with triols whose molecular weight is greater than or equal to 1000, preferably greater than or equal to 3000, diols having a molecular weight of greater than 1000 are combined with triols whose molecular weight is less than 1000.
    • 聚氨酯类压敏粘合剂,其特征在于,所述聚氨酯由以下起始材料组成,所述原料以规定的比例彼此催化反应:a)至少一种脂族或脂环族多异氰酸酯,其功能性在每种情况下小于 或等于3,b)至少一种聚丙二醇二醇和至少一种聚丙二醇三醇的组合,二醇组分中的羟基数与三醇组分中的羟基数之比小于10 优选在0.2和5之间,另外,异氰酸酯基数相对于羟基的总数的比例在0.8至1.15之间,优选在0.95和1.05之间,更优选在1.0和1.05之间,用于与聚氨酯反应的催化剂 由羧酸铋或铋酸铋衍生物组成或由其组成,二醇和三醇可以选择和共同使用 在每种情况下如下:分子量小于或等于1000的二醇与分子量大于或等于1000,优选大于或等于3000的三醇组合,分子量大于或等于3000的二醇 1000与分子量小于1000的三醇组合。
    • 7. 发明申请
    • Polyurethane PSA
    • 聚氨酯PSA
    • US20050019587A1
    • 2005-01-27
    • US10816277
    • 2004-04-01
    • Bernd LuhmannPhilippe HesseSianty SunartoUwe SchumannKirstin WeilandCarsten Bohmer
    • Bernd LuhmannPhilippe HesseSianty SunartoUwe SchumannKirstin WeilandCarsten Bohmer
    • C08G18/48C08G18/75C09J175/08B32B27/40C08L75/04
    • C08G18/4866C08G18/4812C08G18/755C08G2170/40C09J175/08Y10T428/31551
    • Pressure-sensitive adhesive based on polyurethane, characterized in that the polyurethane is composed of the following starting materials which are reacted with one another in the stated proportions: a) at least one aliphatic or alicyclic diisocyanate having in each case an asymmetrical molecular structure, b) a combination of at least one polypropylene glycol diol and at least one polypropylene glycol triol, the ratio of the number of hydroxyl groups in the diol component to the number of hydroxyl groups in the triol component being between 0.7 and 9.0, preferably between 1.5 and 2.5, additionally the ratio of the number of isocyanate groups to the total number of hydroxyl groups being between 0.9 and 1.1, preferably between 0.95 and 1.05, and the diols and triols alternatively being selected and combined in each case as follows: diols having a molecular weight of less than or equal to 1000 are combined with triols whose molecular weight is greater than 1000, preferably greater than or equal to 3000, diols having a molecular weight of greater than 1000 are combined with triols whose molecular weight is less than 1000.
    • 基于聚氨酯的压敏粘合剂,其特征在于,所述聚氨酯由以下起始原料组成,所述原料以规定的比例彼此反应:a)至少一种脂族或脂环族二异氰酸酯,在每种情况下均为不对称分子结构,b )至少一种聚丙二醇二醇和至少一种聚丙二醇三醇的组合,二醇组分中的羟基数与三醇组分中的羟基数之比为0.7至9.0,优选为1.5至 另外,异氰酸酯基数与羟基总数的比例在0.9和1.1之间,优选在0.95和1.05之间,二醇和三醇在各种情况下可以选择和组合,如下所示:具有分子 小于或等于1000的重量与分子量大于1000,优选大于o的三醇组合 r等于3000,分子量大于1000的二醇与分子量小于1000的三醇组合。