    • Petroleum resistant coating and method of preparing same
    • 耐油涂层及其制备方法
    • US5010129A
    • 1991-04-23
    • US221035
    • 1988-07-18
    • Samir F. EliasDaryl K. Morrison
    • Samir F. EliasDaryl K. Morrison
    • C08K5/01C09D131/04
    • C08K5/01C09D131/04
    • A coating exhibiting superior resistance to petroleum products and an absence of known carcinogens as well as a method of preparing same is the subject of the present invention. The coating comprises a combination of a water slurry of filler material to which a latex polymer and coupling agent have been added together with a polyphenyl compound to which plasticizer and surfactant have been added. The water slurry comprises 40-60 weight percent water, 15-35 weight percent filler, 1-10 weight percent latex polymer, 0-2.0 weight percent coupling agent and up to 1 percent by weight colorant. The binder base comprises 10-50 weight percent tertiary or higher polyphenyls, 1-6 percent by weight compatible plasticizer, and 0.05 to 1.0 weight percent nonionic high molecular weight polyester surfactant and is heated. After heating, the binder base and water slurry are combined to form the composition of the invention. A thickener, adhesion promoter and bacteriostat may be added to the product.
    • 对石油产品具有优异的耐受性和不存在已知的致癌物质的涂层及其制备方法是本发明的主题。 该涂层包括填充材料的水浆料,胶乳聚合物和偶联剂与已加入增塑剂和表面活性剂的聚苯基化合物一起加入其中。 水浆料包含40-60重量%的水,15-35重量%的填料,1-10重量%的胶乳聚合物,0-2.0重量%的偶联剂和至多1重量%的着色剂。 粘合剂基质包含10-50重量%的三级或更高级的聚苯基,1-6%(重量)相容的增塑剂和0.05-1.0%的非离子高分子量的聚酯表面活性剂,并加热。 加热后,将粘合剂基料和水浆料结合形成本发明的组合物。 可以向产品中加入增稠剂,粘合促进剂和抑菌剂。