    • 2. 发明授权
    • Process for producing superplastic aluminum alloy strips
    • 生产超塑性铝合金条的工艺
    • US4531977A
    • 1985-07-30
    • US483951
    • 1983-03-28
    • Ryoji MishimaHitoshi Miyamoto
    • Ryoji MishimaHitoshi Miyamoto
    • B22D11/00C22C21/00C22C21/06C22F1/00C22F1/047C22F1/04
    • C22C21/06C22F1/047Y10S420/902
    • Process for producing superplastic aluminum alloy strips comprising continuously casting and rolling a molten aluminum alloy containing 4.0 to 6.0% (by weight) of magnesium, 0.4 to 1.5% (by weight) of manganese, 0.05 to 0.2% (by weight) of chromium and less than 0.50% (by weight) of silicon, thereby preparing a cast strip of 3 to 20 mm in thickness, after subjecting the cast strip to annealing treatment at a temperature of 420.degree. to 530.degree. C., subjecting the annealed strip to the former step of cold rolling and intermediate annealing and then subjecting the intermediately annealed strip to the latter step of cold rolling until the reduction ratio reaches to a value of not less than 60%.
    • PCT No.PCT / JP82 / 00292 Sec。 371日期1983年3月28日 102(e)1983年3月28日PCT PCT。1982年7月28日PCT公布。 出版物WO83 / 00510 日期:1983年2月17日。生产超塑性铝合金带的方法,包括连续铸造和轧制含有4.0至6.0重量%的镁,0.4至1.5重量%的锰,0.05至0.2重量% (重量比)的铬和小于0.50%(重量)的硅,从而在420℃至530℃的温度下对铸造带进行退火处理之后,制备厚度为3-20mm的铸造带材。 对退火钢带进行冷轧和中间退火的前一步骤,然后对中间退火的钢带进行冷轧后续步骤,直到减速比达到不小于60%的值。