    • Hwei-ling YauChristine J. Landry-ColtrainLinda M. Franklin
    • Hwei-ling YauChristine J. Landry-ColtrainLinda M. Franklin
    • G03C176
    • G03C1/7614G03C11/08G03C2001/7635G03C2200/47Y10S430/162
    • The present invention is an imaged photographic element having a protective overcoat thereon. The protective overcoat is formed by providing a photographic element having at least one silver halide light-sensitive emulsion layer. A first coating of hydrophobic polymer particles having an average size of 0.01 to 1 microns, a melting temperature of from 55 to 200 ° C. at a weight percent of 30 to 95, and one or more hydrophilic polymers at a total weight percent of 5 to 70 is applied to form a first layer over the silver halide light-sensitive emulsion layer. A second coating of abrasion resistant particles having an average size of from 0.01 to 1 microns is applied to form a second layer over the first layer. The coatings are dried at temperatures not exceeding the melting point of the particles used in the first coating, or of the glass transition temperature of the abrasion resistant particles used in the second coating, whichever is the lowest. After photoprocessing, the first and second layers can be fused to form a protective overcoat. The photographic element is developed to provide an imaged photographic element.
    • 本发明是在其上具有保护性外涂层的成像照相元件。 保护性外涂层通过提供具有至少一种卤化银感光乳剂层的照相元件形成。 平均尺寸为0.01至1微米,熔化温度为55至200℃,重量百分比为30至95的疏水性聚合物颗粒和一种或多种总重量百分比为5的亲水性聚合物的第一涂层 施加到70以形成卤化银感光乳剂层上的第一层。 施加平均尺寸为0.01至1微米的耐磨颗粒的第二涂层以在第一层上形成第二层。 涂层在不超过第一涂层中使用的颗粒的熔点或第二涂层中使用的耐磨性颗粒的玻璃化转变温度的温度下进行干燥,以最低者为准。 在光处理之后,第一层和第二层可以熔合以形成保护性外涂层。 照相元件被显影以提供成像的照相元件。
    • 10. 发明授权
    • Ink jet printing method
    • 喷墨打印方式
    • US06464351B1
    • 2002-10-15
    • US09627052
    • 2000-07-27
    • Christine Landry-ColtrainDavid M. TeegardenChristopher R. HoffmanLinda M. Franklin
    • Christine Landry-ColtrainDavid M. TeegardenChristopher R. HoffmanLinda M. Franklin
    • B41J201
    • B41M5/52B41M5/5218B41M5/5227B41M5/5236B41M5/5254
    • An ink jet printing method, comprising the steps of: A) providing an ink jet printer that is responsive to digital data signals; B) loading the printer with an ink jet recording element comprising a support having thereon an image-receptive layer capable of accepting an ink jet image comprising an open-pore membrane of a mixture of a water-insoluble polymer and a water-absorbent polymer, the mixture containing at least about 25% by weight of the water-absorbent polymer, the image-receiving layer being made by dissolving the mixture of polymers in a solvent mixture, the solvent mixture comprising at least one solvent which is a good solvent for the water-insoluble polymer and at least one poor solvent for the water-insoluble polymer, the poor solvent having a higher boiling point than the good solvent, coating the dissolved mixture on the support, and then drying to remove approximately all of the solvents to obtain the open-pore membrane; C) loading the printer with an ink jet ink composition; and D) printing on the ink jet recording element using the ink jet ink in response to the digital data signals.
    • 一种喷墨打印方法,包括以下步骤:A)提供响应于数字数据信号的喷墨打印机; B)使用喷墨记录元件装载打印机,该喷墨记录元件包括其上具有能够接受的图像接受层的支撑 包括水不溶性聚合物和吸水性聚合物的混合物的开孔膜的喷墨图像,所述混合物含有至少约25重量%的吸水性聚合物,所述图像接收层被制成 通过将聚合物的混合物溶解在溶剂混合物中,溶剂混合物包含至少一种作为水不溶性聚合物的良溶剂的溶剂和用于不溶于水的聚合物的至少一种不良溶剂,不良溶剂具有较高的沸点 比溶剂好,将溶解的混合物涂在载体上,然后干燥除去大部分溶剂,得到开孔膜; C)用喷墨油墨组合装载打印机 ; 和D)响应于数字数据信号,使用喷墨油墨在喷墨记录元件上进行打印。