    • 1. 发明授权
    • Method and apparatus for treating pulp with oxygen and storing the
treated pulp
    • 用氧处理纸浆并储存经处理的纸浆的方法和设备
    • US4295927A
    • 1981-10-20
    • US48917
    • 1979-06-15
    • Jozef M. BentvelzenMichael D. MeredithHenry BeppleLouis O. TorregrossaHoward R. BattanDennis H. Justice
    • Jozef M. BentvelzenMichael D. MeredithHenry BeppleLouis O. TorregrossaHoward R. BattanDennis H. Justice
    • D21B1/16D21B1/34D21C9/00D21C9/10D21D1/30D21D5/28
    • D21C9/004D21B1/16D21B1/342D21C9/1068D21D1/30
    • A wood pump slurry is treated with oxygen in a mill with little change to the process or structure of the mill. No special pressure tanks are required. The consistency of the pulp need not be altered for the treatment step. It may be treated at the usual process consistency of the pulp; e.g., it may be treated at the usual consistency of the pulp leaving a washer or subsequent steam mixer without additional dewatering or additional dilution.The oxygen is added into a closed section of the system so that it cannot immediately vent to the atmosphere. Alkali should also be present when the oxygen is mixed with the slurry. The mixing should occur near to the point of oxygen addition.The oxygen is inserted into the pulp slurry and mixed with the pulp slurry between a washer and the subsequent storage tank.The mixing occurs in a relatively small mixter that intensively mixes the slurry and gas. The mixer has a mixing zone with a swept area of 10,000 to 1,000,000 square meters per metric ton of oven-dry pulp. A preferred range is 25,000 to 150,000 square meters per metric ton of oven-dry pulp and an optimum range of around 65,400 square meters per metric ton of oven-dry pulp.Other systems and specific mixer designs are also disclosed.
    • 在磨机中用氧气处理木浆泵浆料,对轧机的工艺或结构几乎没有变化。 不需要特殊的压力罐。 对于处理步骤,不需要改变纸浆的稠度。 可以按照纸浆的通常工艺一致性进行处理; 例如,可以以离开洗涤器或随后的蒸汽混合器的纸浆的通常稠度进行处理,而无需额外的脱水或额外的稀释。 将氧气加入系统的封闭部分,使其不能立即排放到大气中。 当氧气与浆料混合时,碱也应存在。 混合应发生在加氧附近。 将氧气插入纸浆中并与浆料在洗涤器和随后的储罐之间混合。 混合发生在相当小的混合器中,其密集地混合浆料和气体。 混合器具有混合区,扫地面积为10,000至100万平方米,每公吨烘干纸浆。 每公吨烘干纸浆的优选范围是25,000至15万平方米,每公吨干燥纸浆的最佳范围约为65,400平方米。 还公开了其他系统和特定混合器设计。
    • 3. 发明授权
    • Method and apparatus for treating pulp with oxygen in a multi-stage
bleaching sequence
    • 在多阶段漂白顺序中用氧处理纸浆的方法和设备
    • US4298426A
    • 1981-11-03
    • US48936
    • 1979-06-15
    • Louis O. TorregrossaJozef M. BentvelzenGerald D. CrosbyMichael D. MeredithHenry Bepple
    • Louis O. TorregrossaJozef M. BentvelzenGerald D. CrosbyMichael D. MeredithHenry Bepple
    • D21C9/10D21C9/12D21C9/14D21C9/16D21D5/28
    • D21C9/1068
    • A wood pulp slurry is treated with oxygen in a mill with little change to the process or structure of the mill. No special pressure tanks are required. The consistency of the pulp need not be altered for the treatment step. It may be treated at the usual process consistency of the pulp; e.g., it may be treated at the usual consistency of the pulp leaving a washer or subsequent steam mixer without additional dewatering or additional dilution.The oxygen is added into a closed section of the system so that it cannot immediately vent to the atmosphere. Alkali should also be present when the oxygen is mixed with the slurry. The mixing should occur near to the point of oxygen addition.The mixing occurs in a relatively small mixer that intensively mixes the slurry and gas. The mixer has a mixing zone with a swept area of 10,000 to 1,000,000 square meters per metric ton of oven-dry pulp. A preferred range is 25,000 to 150,000 square meters per metric ton of oven-dry pulp and an optimum range of around 65,400 square meters per metric ton of oven-dry pulp.The pulp is treated several times during a sequence. Some sequences are O-X-O and O-O-X-O in which X may be chlorine, chlorine dioxide, a combination of chlorine and chlorine dioxide - mixture of chlorine and chlorine dioxide, C.sub.D, D.sub.c -, hypochlorite, peroxide and ozone. The sequence may be followed by a D stage.Other systems and specific mixer designs are also disclosed.
    • 在磨机中用氧气处理木浆浆料,对轧机的工艺或结构几乎没有变化。 不需要特殊的压力罐。 对于处理步骤,不需要改变纸浆的稠度。 可以按照纸浆的通常工艺一致性进行处理; 例如,可以以离开洗涤器或随后的蒸汽混合器的纸浆的通常稠度进行处理,而无需额外的脱水或额外的稀释。 将氧气加入系统的封闭部分,使其不能立即排放到大气中。 当氧气与浆料混合时,碱也应存在。 混合应发生在加氧附近。 混合发生在相当小的混合器中,其密集地混合浆料和气体。 混合器具有混合区,扫地面积为10,000至100万平方米,每公吨烘干纸浆。 每公吨烘干纸浆的优选范围是25,000至15万平方米,每公吨干燥纸浆的最佳范围约为65,400平方米。 在一个序列中纸浆被处理好几次。 一些序列是O-X-O和O-O-X-O,其中X可以是氯,二氧化氯,氯和二氧化氯的组合 - 氯和二氧化氯的混合物,CD,Dc-,次氯酸盐,过氧化物和臭氧。 该序列之后可以是D阶段。 还公开了其他系统和特定混合器设计。
    • 5. 发明授权
    • Method and apparatus for intimately mixing oxygen and pulp while using
an alkali to extract bleaching by-products
    • 在使用碱提取漂白副产物的同时,将氧和纸浆紧密混合的方法和装置
    • US4298427A
    • 1981-11-03
    • US48947
    • 1979-06-15
    • Jozef M. BentvelzenMichael D. MeredithLouis O. TorregrossaHenry Bepple
    • Jozef M. BentvelzenMichael D. MeredithLouis O. TorregrossaHenry Bepple
    • D21C9/10
    • D21C9/1068
    • A wood pulp slurry is treated with oxygen in a mill with little change to the process or structure of the mill. No special pressure tanks are rquired. The consistency of the pulp need not be altered for the treatment step. It may be treated at the usual process consistency of the pulp; e.g., it may be treated at the usual consistency of the pulp leaving a washer or subsequent steam mixer without additional dewatering or additional dilution.The oxygen is added into a closed section of the system so that it cannot immediately vent to the atmosphere. Alkali should also be present when the oxygen is mixed with the slurry. The mixing should occur near to the point of oxygen addition.An existing extraction stage within the system may be used as a source of alkali. In an existing extraction stage, the mixer and upstream oxygen line would be placed in the line between the steam mixer and the extraction tower.The mixing occurs in a relatively small mixer that intensively mixes the slurry and the gas. The mixer has a mixing zone with a swept area of 10,000 to 1,000,000 square meters per metric ton of oven-dry pulp. A preferred range is 25,000 to 150,000 square meters per metric ton of oven-dry pulp and an optimum range of around 65,400 square meters per metric ton of oven-dry pulp.Other systems and specific mixer designs are also disclosed.
    • 在磨机中用氧气处理木浆浆料,对轧机的工艺或结构几乎没有变化。 没有特殊的压力罐被打。 对于处理步骤,不需要改变纸浆的稠度。 可以按照纸浆的通常工艺一致性进行处理; 例如,可以以离开洗涤器或随后的蒸汽混合器的纸浆的通常稠度进行处理,而无需额外的脱水或额外的稀释。 将氧气加入系统的封闭部分,使其不能立即排放到大气中。 当氧气与浆料混合时,碱也应存在。 混合应发生在加氧附近。 系统内的现有萃取阶段可用作碱源。 在现有的萃取阶段,混合器和上游氧气管线将被置于蒸汽混合器和萃取塔之间的管线中。 混合发生在相当小的混合器中,其密集地混合浆料和气体。 混合器具有混合区,扫地面积为10,000至100万平方米,每公吨烘干纸浆。 每公吨烘干纸浆的优选范围是25,000至15万平方米,每公吨干燥纸浆的最佳范围约为65,400平方米。 还公开了其他系统和特定混合器设计。
    • 6. 发明授权
    • Low-consistency ozone delignification
    • 低稠度臭氧脱木质素
    • US4216054A
    • 1980-08-05
    • US836449
    • 1977-09-26
    • Jozef M. BentvelzenSteven L. BogartMaharaj K. GuptaWilliam T. McKeanMichael D. MeredithLouis O. Torregrossa
    • Jozef M. BentvelzenSteven L. BogartMaharaj K. GuptaWilliam T. McKeanMichael D. MeredithLouis O. Torregrossa
    • D21C9/10
    • D21C9/1073
    • A slurry of cellulosic fiber and water having a consistency in the range of 0.017-4.9% of the total ungassed weight of fiber and water is bleached with ozone. This is done without the usual addition of organic additives. The water can include impurities created by the bleaching process. Rapid reaction times under 8 minutes and preferably under 5 minutes are achieved.The reaction is enhanced in the consistency range of about 0.017-0.7%.The slurry is mixed using a mixing energy of 0.002-1.0 horsepower per cubic foot of gassed slurry. The mixing energy will determine whether the gas-liquid or liquid-solid interface will limit the speed of the reactions. The passage of ozone from the gas to a liquid phase will be the limiting factor below about 0.2 horsepower per cubic foot of gassed slurry. The increasing presence of ozone in the liquid as the horsepower increases from about 0.2 to about 0.4 horsepower per cubic foot of gassed slurry indicates this is a zone in which both the gas-liquid and the liquid-solid interface are limiting factors. Above about 0.4 horsepower per cubic foot of gassed slurry the liquid-solid interface will be the limiting factor.Superficial velocity of the ozone bearing gas is in a range of 200-3800 feet per hour. The ozone usually is 0.05-6% by weight of the total weight of the gas.
    • 将纤维素纤维和水的浆液在纤维和水的总未脱气重量的0.017-4.9%的范围内与臭氧一起漂白。 没有通常添加有机添加剂就可以完成。 水可以包括由漂白过程产生的杂质。 8分钟以下,优选5分钟以下快速反应时间。 该反应在约0.017-0.7%的一致性范围内得到增强。 使用0.002-1.0马力/立方英尺充气浆料的混合能量将浆料混合。 混合能量将决定气液或液 - 固界面是否会限制反应的速度。 臭氧从气体通到液相将是每立方英尺充气浆料低于约0.2马力的限制因素。 臭氧在液体中的增加的存在随着马力从每立方英尺充气浆料的约0.2至约0.4马力的增加表明这是气液和液 - 固界面都是限制因素的区域。 高于约0.4马力/立方英尺的充气浆液液固界面将成为限制因素。 含臭氧气体的表观速度在每小时200-3800英尺的范围内。 臭氧通常为气体总重量的0.05-6重量%。
    • 8. 发明授权
    • Method and apparatus for treating pulp with oxygen
    • 用氧处理纸浆的方法和设备
    • US4295926A
    • 1981-10-20
    • US49001
    • 1979-06-15
    • Jozef M. BentvelzenMichael D. MeredithHenry BeppleLouis O. TorregrossaHoward R. BattanDennis H. Justice
    • Jozef M. BentvelzenMichael D. MeredithHenry BeppleLouis O. TorregrossaHoward R. BattanDennis H. Justice
    • D21B1/16D21B1/34D21C9/00D21C9/10D21D1/30D21D5/28
    • D21C9/004D21B1/16D21B1/342D21C9/1068D21D1/30
    • A wood pulp slurry is treated with oxygen in a mill with little change to the process or structure of the mill. No special pressure tanks are required. The consistency of the pulp need not be altered for the treatment step. It may be treated at the usual process consistency of the pulp; e.g., it may be treated at the usual consistency of the pulp leaving a washer or the subsequent steam mixer without additional dewatering or additional dilution.The oxygen is added into a closed section of the system so that it cannot immediately vent to the atmosphere. Alkali should also be present when the oxygen is mixed with the slurry. The mixing should occur near to the point of oxygen addition.The oxygen is inserted into the pulp slurry and mixed with the pulp slurry between a pair of washers. The second washer may be a vacuum, pressure or diffusion washer.The mixing occurs in a relatively small mixer that intensively mixes the slurry and gas. The mixer has a mixing zone with a swept area of 10,000 to 1,000,000 square meters per metric ton of oven-dry pulp. A preferred range is 25,000 to 150,000 square meters per metric ton of oven-dry pulp and an optimum range of around 65,000 square meters per metric ton of oven-dry pulp.Other systems and specific mixer designs are also disclosed.
    • 在磨机中用氧气处理木浆浆料,对轧机的工艺或结构几乎没有变化。 不需要特殊的压力罐。 对于处理步骤,不需要改变纸浆的稠度。 可以按照纸浆的通常工艺一致性进行处理; 例如,可以以离开洗涤器或随后的蒸汽混合器的纸浆的通常稠度进行处理,而无需额外的脱水或额外的稀释。 将氧气加入系统的封闭部分,使其不能立即排放到大气中。 当氧气与浆料混合时,碱也应存在。 混合应发生在加氧附近。 将氧气插入纸浆中并与纸浆在一对垫圈之间混合。 第二垫圈可以是真空,压力或扩散垫圈。 混合发生在相当小的混合器中,其密集地混合浆料和气体。 混合器具有混合区,扫地面积为10,000至100万平方米,每公吨烘干纸浆。 每公吨烘干纸浆的优选范围为25,000至15万平方米,每公吨烘干纸浆的最佳范围约为65,000平方米。 还公开了其他系统和特定混合器设计。