    • 2. 发明申请
    • SEALING RING AND PREPARATION METHOD THEREOF
    • 密封圈及其制备方法
    • US20120308430A1
    • 2012-12-06
    • US13585772
    • 2012-08-14
    • Xuemin CHENQingdong YEJimin YUANLiping HUMing YIN
    • Xuemin CHENQingdong YEJimin YUANLiping HUMing YIN
    • C22C21/00B22D27/00B22D23/00
    • F16J15/0806C22B34/12C22C21/00Y02P10/212
    • The present invention provides a sealing ring and a preparation method thereof. The sealing ring, based on percent by weight, includes 80%-85% of aluminum, 10%-15% of titanium, 0.1%-1% of scrap iron, and 4%-4.9% of potassium fluoroaluminate. Moreover, the present invention provides a method for preparing sealing ring, which includes the following steps: Step A: melting the aluminum in a medium-frequency induction furnace, adding the potassium fluoroaluminate to the medium-frequency induction furnace after melting the aluminum, melting and stirring the mixture evenly; Step B: adding titanium scrap or sponge titanium, and scrap iron to the mixture successively, melting and mixing the mixture totally at 800° C. to 1200° C., standing the mixture after stirring evenly; Step C: removing scum on the surface; Step D: casting into a mould to obtain a final sealing ring.
    • 本发明提供一种密封环及其制备方法。 密封圈以重量百分比计,包括80%-85%的铝,10%-15%的钛,0.1%-1%的废铁和4%-4.9%的氟铝酸钾。 此外,本发明提供一种制备密封圈的方法,其包括以下步骤:步骤A:在中频感应炉中熔化铝,将铝氟化铝加入到中频感应炉中,熔化铝,熔化 并均匀搅拌混合物; 步骤B:将钛废料或海绵钛和废铁依次加入混合物中,在800℃至1200℃下熔融混合,搅拌均匀后静置; 步骤C:去除表面浮渣; 步骤D:铸造成模具以获得最终密封环。