    • 1. 发明授权
    • Method for coating a rubber wiper blade
    • 橡胶刮水片涂布方法
    • US06287642B1
    • 2001-09-11
    • US09424729
    • 2000-03-14
    • Wolfgang LeutschJohannes RauschnabelJeanne ForgetJohannes Voigt
    • Wolfgang LeutschJohannes RauschnabelJeanne ForgetJohannes Voigt
    • C23C16513
    • C23C14/22B60S2001/3829C23C14/027C23C16/029C23C16/50
    • In the process for coating the elastomeric rubber wiper a vaporous coating material is generated and activated by a plasma and/or laser; a protective coating is formed on a rubber wiper surface by exposing it to the vaporous coating material by CVD and/or PVD methods and process parameters for the coating process are controlled so that the protective coating includes at least three coating layers and has a total thickness of from 200 nm to 2 &mgr;m. The coating layers include at least one thicker softer elastic coating layer with elastomeric properties similar to those of the rubber wiper and other thinner harder coating layers having wear-resistant properties. The other thinner harder coating layers have respective hardness increasing from an inner most one to an outermost one of the other thinner harder coating layers.
    • 在用于涂覆弹性体橡胶擦拭器的过程中,通过等离子体和/或激光产生并激活蒸汽涂层材料; 通过用CVD和/或PVD方法将橡胶擦拭表面暴露于气态涂料上,形成保护涂层,并且控制用于涂覆过程的工艺参数,使得保护涂层包括至少三个涂层并具有总厚度 为200〜2μm。 涂层包括至少一个较软的较软的弹性涂层,其具有与橡胶擦拭器和具有耐磨性能的其它较薄的较硬的涂层相似的弹性体性质。 其他较薄的较硬的涂层具有相应的硬度从另一较薄的较硬的涂层中的最内层到最外层的硬度。
    • 2. 发明授权
    • Method and device for coating at least one wiper-blade element
    • 用于涂覆至少一个刮片元件的方法和装置
    • US06793978B2
    • 2004-09-21
    • US10049763
    • 2002-06-04
    • Kurt BurgerGuenter SchneiderKlaus BurghoffThomas WeberJeanne Forget-Funk
    • Kurt BurgerGuenter SchneiderKlaus BurghoffThomas WeberJeanne Forget-Funk
    • C23C1650
    • C23C16/458B60S2001/3829C23C16/0245C23C16/509
    • The invention is based on a method for coating at least one wiper blade element (10) made of an elastomer material, in which first, the surface of the wiper blade element (10) is cleaned and activated by means of a plasma, and then in a CVD process, a coating material is brought into a plasma state and at least one protective coating (64) forms on the surface of the wiper blade element (10), where a high-frequency voltage is applied to the region of the wiper blade element (10) oriented away from the protective layer (64) by means of an electrode (56). The invention proposes that before being brought into a treatment chamber (32, 34, 36, 38, 40, 74), the wiper blade element (10) be cut to a useful length (66) from a profiled band and placed on an electrode plate (56) so that its wiper lip (18) stands approximately perpendicular to the electrode plate (56), which extends to both sides of the wiper blade element (10), and is subjected to a plasma flow (50).
    • 本发明基于一种用于涂覆由弹性体材料制成的至少一个刮片元件(10)的方法,其中首先,通过等离子体清洁和激活刮水片元件(10)的表面,然后 在CVD工艺中,涂层材料进入等离子体状态,并且在刮片元件(10)的表面上形成至少一个保护涂层(64),其中高频电压被施加到擦拭器的区域 叶片元件(10)通过电极(56)远离保护层(64)。本发明提出在被带入处理室(32,34,36,38,40,74)之前,刮水器 叶片元件(10)从成型带切割成有用长度(66)并放置在电极板(56)上,使得其擦拭器唇缘(18)大致垂直于电极板(56),其延伸到两个 并且经受等离子体流(50)。
    • 4. 发明授权
    • Combination antiabrasion layer
    • 组合抗磨层
    • US06368717B1
    • 2002-04-09
    • US09403820
    • 2000-02-04
    • Johannes RauschnabelJeanne ForgetJohannes Voigt
    • Johannes RauschnabelJeanne ForgetJohannes Voigt
    • B32B904
    • B05D1/62C23C16/029C23C16/26C23C28/00Y10T428/24942Y10T428/24983Y10T428/31663
    • A combination wear protection film for components made of substrates susceptible to wear is described. The film has a wear-resistant surface film that contains one or more of the elements carbon, nitrogen, or boron, the proportion of this element—or, if more than one of these elements is present, the sum of the proportions of the elements present—is at least 30% by atomic weight, preferably at least 40% by atomic weight; and a support film, located between a substrate and the surface film and made of a plasma polymer, that exhibits a quasi-continuous transition in modulus of elasticity and optionally in hardness from a value of a base film to a value of the surface film. A method for producing a wear protection film of this kind, and objects equipped with the wear protection film is also described.
    • 描述了易受磨损的基材制成的组合磨损保护膜。 该膜具有含有碳,氮或硼中的一种或多种元素的耐磨表面膜,该元素的比例 - 或者如果存在这些元素中的一种以上,则元素的比例之和 为原子量至少为30%,优选为原子量的至少40%; 以及位于基板和表面膜之间并由等离子体聚合物制成的支撑膜,其显示出从基膜的值到表面膜的值的弹性模量和任选的硬度的准连续过渡。 还描述了一种用于制造这种耐磨保护膜的方法,以及配备有该磨损保护膜的物体。