    • 1. 发明授权
    • Partially alloyed galvanize product
    • 部分合金镀锌产品
    • US4125679A
    • 1978-11-14
    • US818796
    • 1977-07-25
    • George M. MinoDonald L. Dustin
    • George M. MinoDonald L. Dustin
    • C23C2/06C23C2/28C23C1/02
    • C23C2/28C23C2/06Y10T428/12799
    • A partially alloyed galvanized ferrous strand and a method for its production. The method is characterized by the steps of immersing a clean and oxide-free ferrous strand in a molten zinc galvanizing bath to produce on the strand a coating weight of between 0.2 and 0.5 oz. per square foot. After immersion, the zinc-coated ferrous strand is heat treated and cooled to produce a galvanized coating on said ferrous strand, which coating has a duplex structure characterized by an iron-zinc intermetallic layer consisting essentially of the zeta phase, an overlay of free zinc, and an average iron content between about 2 and less than 4% by weight.
    • 部分合金镀锌铁线及其制造方法。 该方法的特征在于将清洁和无氧化的铁线浸入熔融镀锌浴中以在该股线上产生0.2-0.5盎司的涂层重量的步骤。 每平方英尺 在浸渍之后,对锌涂层的铁线材进行热处理和冷却,以在所述亚铁股线上产生镀锌涂层,该涂层具有双相结构,其特征在于基本上由ζ相组成的铁 - 锌金属间化合物层,游离锌 ,平均铁含量在约2%且小于4%(重量)之间。
    • 2. 发明授权
    • Partially alloyed galvanize product and method
    • 部分合金镀锌产品及方法
    • US4059711A
    • 1977-11-22
    • US686961
    • 1976-05-14
    • George M. MinoDonald L. Dustin
    • George M. MinoDonald L. Dustin
    • C23C2/06C23C2/28C23C1/02
    • C23C2/28C23C2/06Y10T428/12799
    • A partially alloyed galvanized ferrous strand and a method for its production. The method is characterized by the steps of immersing a clean and oxide-free ferrous strand in a molten zinc galvanizing bath to produce on the strand a coating weight of between 0.2 and 0.5 oz. per square foot. After immersion, the zinc-coated ferrous strand is heat treated and cooled to produce a galvanized coating on said ferrous strand, which coating has a duplex structure characterized by an iron-zinc intermetallic layer consisting essentially of the zeta phase, an overlay of free zinc, and an average iron content between about 2 and less than 4% by weight.
    • 部分合金镀锌铁线及其制造方法。 该方法的特征在于将清洁和无氧化的铁线浸入熔融镀锌浴中以在该股线上产生0.2-0.5盎司的涂层重量的步骤。 每平方英尺 在浸渍之后,对锌涂层的铁线材进行热处理和冷却,以在所述亚铁股线上产生镀锌涂层,该涂层具有双相结构,其特征在于基本上由ζ相组成的铁 - 锌金属间化合物层,游离锌 ,平均铁含量在约2%且小于4%(重量)之间。