    • Method for producing a moulded part
    • 用于制造模制件的方法
    • US20060192323A1
    • 2006-08-31
    • US10533560
    • 2003-07-30
    • Gebhard ZoblWolfgang GlatzWolfgang KrausslerRobert Oberbreyer
    • Gebhard ZoblWolfgang GlatzWolfgang KrausslerRobert Oberbreyer
    • C04B35/64
    • B22F3/164B22F3/02B22F5/00B22F2998/00B22F2998/10H01M8/0208H01M8/0215H01M8/0247Y02E60/50C22C33/0207H01M8/02B22F3/10
    • The invention relates to a process for producing a molding, comprising a disk-like or plate-like basic body —5— having a large number of knob-like and/or web-like elevations —4—3— which merge into the basic body —5— with inclined side surfaces, by means of pressing and sintering powdery raw materials close to the final shape. According to the invention, the pressing is carried out in a two-stage pressing operation. In the first stage the boundary surfaces of the basic body —5— are pressed to at least the approximate final shape as far as the transition regions of the elevations —3—4— and, at the same time, the elevations —3—4— are pressed to an oversize. The projection h′ of the elevations —3—4— from the basic body —5— is greater by 10%-150% as compared with the projection h from the basic body —5— in the finally pressed state. Their side surfaces form an angle of inclination α′ in the range from 90°-150° with the respectively adjacent boundary surface of the basic body —5—. In the second stage, the elevations —3—4— are pressed to at least approximately the final shape, the angle of inclination α′ being enlarged to a value α which lies in the range from 95°-170°.
    • 本发明涉及一种用于生产模制件的方法,该方法包括具有大量旋钮状和/或网状高度4-3的盘状或板状基体5,它们合并成基本 主体5 - 具有倾斜的侧面,通过压制和烧结接近最终形状的粉末状原料。 根据本发明,在两级压制操作中进行压制。 在第一阶段,基体5的边界表面至少压缩到近似最终形状,直到高度3-4的过渡区域,同时,高度3-4 - 被迫超大。 与基体5的突起h相比,从基体5开始的高度3-4的投影h'比最终压制状态下的突起h'大10%-150%。 它们的侧表面与基体的相邻的边界表面形成了在90°-150°范围内的倾斜角α'5°。 在第二阶段,将3-4号高程按压至少近似于最终形状,将倾斜角α'扩大到一个α值在95°-170°的范围内。
    • 7. 发明授权
    • Process for producing a molding
    • 用于生产模制品的方法
    • US08173063B2
    • 2012-05-08
    • US10533560
    • 2003-07-30
    • Gebhard ZoblWolfgang GlatzWolfgang KrausslerRobert Oberbreyer
    • Gebhard ZoblWolfgang GlatzWolfgang KrausslerRobert Oberbreyer
    • B28B3/00
    • B22F3/164B22F3/02B22F5/00B22F2998/00B22F2998/10H01M8/0208H01M8/0215H01M8/0247Y02E60/50C22C33/0207H01M8/02B22F3/10
    • The invention relates to a process for producing a molding, comprising a disk-like or plate-like basic body -5- having a large number of knob-like and/or web-like elevations -4-3- which merge into the basic body -5- with inclined side surfaces, by means of pressing and sintering powdery raw materials close to the final shape.According to the invention, the pressing is carried out in a two-stage pressing operation. In the first stage the boundary surfaces of the basic body -5- are pressed to at least the approximate final shape as far as the transition regions of the elevations -3-4- and, at the same time, the elevations -3-4- are pressed to an oversize. The projection h′ of the elevations -3-4- from the basic body -5- is greater by 10%-150% as compared with the projection h from the basic body -5- in the finally pressed state. Their side surfaces form an angle of inclination α′ in the range from 90°-150° with the respectively adjacent boundary surface of the basic body -5-. In the second stage, the elevations -3-4- are pressed to at least approximately the final shape, the angle of inclination α′ being enlarged to a value α which lies in the range from 95°-170°.
    • 本发明涉及一种用于制造模制件的方法,该方法包括具有大量旋钮状和/或网状凸起-4-3的盘状或板状基体5,它们合并成基本 体5具有倾斜的侧面,通过压制和烧结接近最终形状的粉末状原料。 根据本发明,在两级压制操作中进行压制。 在第一阶段中,基体-5的边界表面被按压到至少大致最终形状,直到高度-34-的过渡区域,并且同时,高度-34 - 被迫超大。 与最终按压状态下的基体-5的突起h相比,从基体5的高度-3-4-的突起h'大10%-150%。 它们的侧表面与基体的相邻的边界面形成90°-150°的倾角α'。 在第二阶段中,将高度-34-压制成至少近似于最终形状,倾斜角度α'被扩大到位于95°-170°范围内的值α。