    • 3. 发明申请
    • FLAME RESISTANT RESIN COMPOSITION
    • 耐火树脂组合物
    • US20080262127A1
    • 2008-10-23
    • US12018099
    • 2008-01-22
    • Kuen-Yuan HwangAn-Pang TuGai-Chi ChenI-Cheng Hsu
    • Kuen-Yuan HwangAn-Pang TuGai-Chi ChenI-Cheng Hsu
    • C08K3/00C08K3/20C08K3/26
    • C08G59/3218C08G59/621C08K3/013C08L63/00C08L2666/54
    • A flame resistant resin composition is provided, which includes: (A) at least an epoxy resin having a biphenylic unit or a naphthalenic unit; (B) phenolic resins used as a curing agent, the phenolic resins include at least a phenolic resin having a biphenylic moiety and a polyphenolic moiety, wherein the the at least a phenolic resin having a biphenylic moiety and a polyphenolic moiety is in an amount of 30 to 100 wt % of the total weight of the curing agents; (C) a curing-promoting agent; and (D) an inorganic filler material. The resin composition includes an epoxy resin having a biphenylic unit or a naphthalenic unit and the phenolic resin having a biphenylic moiety and a polyphenolic moiety as a curing agent, such that excellent flame resistance can be achieved without adding flame resistant agents. The resin composition also has a higher glass transition temperature to improve the water absorption issue after curing, and increases heat stability. Therefore, the resin composition is particularly useful in composite materials, forming materials or semiconductor packaging materials.
    • 提供了一种阻燃树脂组合物,其包括:(A)至少一种具有联苯单元或萘单元的环氧树脂; (B)用作固化剂的酚醛树脂,酚醛树脂至少包括具有联苯部分和多酚部分的酚醛树脂,其中至少一种具有联苯部分和多酚部分的酚醛树脂的量为 30至100重量%的固化剂总重量; (C)固化促进剂; 和(D)无机填料。 树脂组合物包括具有联苯单元或萘单元的环氧树脂和具有联苯部分和多酚部分作为固化剂的酚醛树脂,使得可以在不添加阻燃剂的情况下实现优异的阻燃性。 树脂组合物还具有较高的玻璃化转变温度,以改善固化后的吸水问题,并且增加热稳定性。 因此,树脂组合物特别适用于复合材料,成型材料或半导体封装材料。
    • 7. 发明申请
    • METHOD FOR PREPARING MELAMINE SALT OF BIS(PENTAERYTHRITOL PHOSPHATE) PHOSPHORIC ACID
    • 磷酸二甲酯盐酸盐(PENTAERYTHRITOL PHOSPHICIC酸)的制备方法
    • US20080255353A1
    • 2008-10-16
    • US12020454
    • 2008-01-25
    • Kuen-Yuan HWANGAn-Pang TuGai-Chi Chen
    • Kuen-Yuan HWANGAn-Pang TuGai-Chi Chen
    • C07D251/12
    • C07D251/56C07D251/18
    • A method for producing a melamine salt of bis(pentaerythritol phosphate) phosphoric acid is proposed. The method includes the steps of reacting and mixing pentaerythritol and diphosphorous pentaoxide in an extruder to carry out esterification to produce bis(pentaerythritol phosphate) phosphoric acid; and mixing bis(pentaerythritol phosphate) phosphoric acid with melamine or a derivative thereof to carry out quaternization in the presence of a solvent, followed by removing water to obtain a melamine salt of bis(pentaerythritol phosphate) phosphoric acid. Diphosphorous pentaoxide is used in the method as a reactant, so that no hydrogen chloride is produced and it is not necessary to recollect trichlorophosphoric acid. Moreover, in the method of the present invention, such that esterification time can be shortened and a high pressure in a closed reaction system that causes explosion can be avoided.