    • 3. 发明授权
    • Well cementing material
    • 固井材料
    • US07892348B2
    • 2011-02-22
    • US12555859
    • 2009-09-09
    • Eric LecolierAlain Rivereau
    • Eric LecolierAlain Rivereau
    • C04B24/00
    • C09K8/473C04B28/02C04B38/10Y02W30/94Y10S106/01C04B14/04C04B18/146C04B20/008C04B24/26C04B2103/40C04B2103/0053C04B28/06C04B28/065C04B2103/0035C04B2103/0036
    • The present invention relates to a formulation of a high-performance foamed cement material, comprising: at least one hydraulic binder, microparticles whose grain size ranges between 0.1 and 30 μm, whose proportion ranges between 15% and 50% by mass in relation to the mass of hydraulic binder, mineral particles whose grain size ranges between 1 and 500 μm, whose proportion ranges between 10% and 35% by mass in relation to the mass of hydraulic binder, the proportion of particles being lower than the proportion of microparticles, a hydrosoluble polymer thinning agent whose proportion ranges between 0.1% and 8% by mass in relation to the mass of hydraulic binder, water whose proportion is at most 40% by mass in relation to the mass of hydraulic binder, a foaming agent whose proportion ranges between 0.1% and 10% by mass in relation to the mass of hydraulic binder.
    • 本发明涉及一种高性能泡沫水泥材料的配方,其包括:至少一种水硬性粘合剂,其颗粒尺寸范围为0.1至30μm的微粒,其比例范围为15%至50质量% 水硬性粘合剂的质量,粒度范围为1〜500μm的矿物颗粒,其比例相对于水硬性粘合剂的质量为10〜35质量%,颗粒的比例低于微粒的比例,a 水硬性聚合物稀释剂的比例相对于水硬性粘合剂的质量为0.1〜8质量%,相对于水硬性粘合剂的质量为比例为40质量%以下的水,发泡剂的比例范围为 相对于液压粘合剂的质量为0.1%和10质量%。
    • 8. 发明申请
    • WELL CEMENTING MATERIAL
    • 良好的成型材料
    • US20100010108A1
    • 2010-01-14
    • US12555859
    • 2009-09-09
    • Eric LECOLIERAlain RIVEREAU
    • Eric LECOLIERAlain RIVEREAU
    • C09K8/467
    • C09K8/473C04B28/02C04B38/10Y02W30/94Y10S106/01C04B14/04C04B18/146C04B20/008C04B24/26C04B2103/40C04B2103/0053C04B28/06C04B28/065C04B2103/0035C04B2103/0036
    • The present invention relates to a formulation of a high-performance foamed cement material, comprising: at least one hydraulic binder, microparticles whose grain size ranges between 0.1 and 30 μm, whose proportion ranges between 15 % and 50 % by mass in relation to the mass of hydraulic binder, mineral particles whose grain size ranges between 1 and 500 μm, whose proportion ranges between 10 % and 35 % by mass in relation to the mass of hydraulic binder, the proportion of particles being lower than the proportion of microparticles, a hydrosoluble polymer thinning agent whose proportion ranges between 0.1 % and 8 % by mass in relation to the mass of hydraulic binder, water whose proportion is at most 40 % by mass in relation to the mass of hydraulic binder, a foaming agent whose proportion ranges between 0.1 % and 10 % by mass in relation to the mass of hydraulic binder.
    • 本发明涉及一种高性能泡沫水泥材料的配方,其包括:至少一种水硬性粘合剂,其粒度范围为0.1至30μm的微粒,其比例相对于所述粘合剂的比例为15%至50质量% 水硬性粘合剂的质量,粒度范围为1〜500μm的矿物颗粒,其比例相对于水硬性粘合剂的质量为10〜35质量%,颗粒的比例低于微粒的比例,a 水硬性聚合物稀释剂的比例相对于水硬性粘合剂的质量为0.1〜8质量%,相对于水硬性粘合剂的质量为比例为40质量%以下的水,发泡剂的比例范围为 相对于液压粘合剂的质量为0.1%和10质量%。