    • 1. 发明授权
    • Method of producing hardmetal-bonded metal component
    • 生产硬质合金金属成分的方法
    • US06756009B2
    • 2004-06-29
    • US10321593
    • 2002-12-18
    • Dong Sub SimKyung Woon KimKeun Chul SongJung Hwan Cho
    • Dong Sub SimKyung Woon KimKeun Chul SongJung Hwan Cho
    • B22F704
    • C23C26/00
    • A method is provided of producing a hardmetal-bonded metal component with an enhanced bond strength. The method comprises the steps of providing an iron-based metal body, mixing and compressing raw material powder of hardmetal and binder powder containing nickel, silicon and boron into a preform, heating and sintering the preform, and applying heat to the sintered body and the iron-based metal body under a state that the sintered body is brought into contact with the iron-based metal body, to thereby cause the sintered body to be bonded to the iron-based metal body. The sintered body and the iron-based metal body are thermally treated at a temperature of 1,000 to 1,200° C. for 30 or more minutes so that boron present in the sintered body is infiltrated into grain boundaries of the iron-based metal body to form a plurality of boride spikes in a bonding interface.
    • 提供了一种生产具有增强的粘结强度的硬金属粘合的金属组分的方法。 该方法包括以下步骤:提供铁基金属体,将含有镍,硅和硼的硬质合金和粘合剂粉末的原料粉末混合并压缩到预成型体中,加热和烧结预成型体,并向烧结体施加热量, 铁基金属体在烧结体与铁基金属体接触的状态下,从而使烧结体与铁基金属体接合。 将烧结体和铁基金属体在1000〜1200℃的温度下热处理30分钟以上,使烧结体中存在的硼渗入铁基金属体的晶界,形成 在接合界面中的多个硼化物尖峰。