    • 1. 发明授权
    • Optical coupling device having KBBF group crystal coupled with prisms and method for manufacturing same
    • 具有与棱镜耦合的KBBF组晶体的光耦合器件及其制造方法
    • US08773750B2
    • 2014-07-08
    • US14115261
    • 2012-03-21
    • Chuangtian ChenYong ZhuFeidi FanXiaoyang WangRukang Li
    • Chuangtian ChenYong ZhuFeidi FanXiaoyang WangRukang Li
    • G02F1/355
    • G02F1/3501G02B1/02G02B5/04G02F1/353G02F1/3551G02F2001/3503
    • The present invention relates to a KBBF family nonlinear optical crystal-prism coupler and its method of fabrication. The coupler comprises: a KBBF family crystal with two smooth surfaces; transition layers each of which is deposited on respective one of the two smooth surfaces of the KBBF family crystal; and a pair of prisms each of which optically contacts with respective one of the activated transition layers. The present invention further provides a KBBF family nonlinear optical crystal-prism coupler that comprises: a KBBF family crystal with two smooth surfaces; a pair of prisms each of which has a smooth surfaces; first transition layers each of which is deposited on respective one of the two smooth surfaces of the KBBF family crystal; and second transition layers each of which is deposited on a smooth surface of respective one of the pair of prisms, wherein the first and second transition layers are integral by optical contact. The coupling between the KBBF family crystal and the prisms is achieved by optical contact through transition layers to improve bonding strength.
    • 本发明涉及KBBF系列非线性光学晶体 - 棱镜耦合器及其制造方法。 耦合器包括:具有两个光滑表面的KBBF系列晶体; 过渡层各自沉积在KBBF族晶体的两个平滑表面的相应一个上; 以及一对棱镜,每个棱镜与相应的一个激活的过渡层光学接触。 本发明还提供一种KBBF系列非线性光学晶体 - 棱镜耦合器,其包括:具有两个平滑表面的KBBF族晶体; 一对棱镜具有光滑的表面; 第一过渡层分别沉积在KBBF族晶体的两个光滑表面的相应一个上; 以及第二过渡层,每个过渡层沉积在该对棱镜中的相应一个棱镜的光滑表面上,其中第一和第二过渡层通过光学接触而成一体。 KBBF系列晶体与棱镜之间的耦合是通过过渡层的光学接触来实现的,以提高结合强度。
    • 2. 发明申请
    • FLUOROBERYLLIUM BORATE NON-LINEAR OPTICAL CRYSTALS AND THEIR GROWTH AND APPLICATIONS
    • 氟硼酸盐非线性光学晶体及其生长和应用
    • US20100142032A1
    • 2010-06-10
    • US12376559
    • 2006-09-15
    • Chuangtian ChenXiaohong WenRukang LiChengqian Zhang
    • Chuangtian ChenXiaohong WenRukang LiChengqian Zhang
    • G02F1/355G02F1/37G02F1/39H01S3/06C30B15/30
    • C30B9/12C30B15/00C30B29/12G02F1/3551
    • A beryllium borate fluoride salt nonlinear optical crystal is represented by molecule formula Mbe2BO3F2, wherein M is Rb or Cs. The crystal is grown by melt salt method, comprising the following step, mixing beryllium borate fluoride salt with flux at appropriate ratio, rising to 750-800° C., and keeping at constant temperature, then cooling to 2-10° C. higher than saturated temperature to obtain a elevated solution; putting seed crystal on seed crystal pole into the elevated solution, rotating the seed crystal pole, cooling to saturated temperature, and then cooling slowly; raising the obtained crystal above liquid level and cooling to room temperature, then obtaining the present nonlinear optical crystal. The crystal has nonlinear optical effect, broad transmittance wave, adsorption edge of ultraviolet lower to 150 nm, doesn't deliquesce, isn't soluble to diluted hydrochloric acid and nitric acid, and has good chemical resistance. The present crystal satisfies ultraviolet laser frequency-conversion requirements, can be used to make nonlinear optical device, make the second, the third, the forth, the fifth, or the sixth harmonic output device of Nd:YAG realized, and also can be used to harmonic output devices of other laser, to output tunable coherent light equal or down to 266 nm.
    • 硼酸铍氟化物盐非线性光学晶体由分子式Mbe2BO3F2表示,其中M是Rb或Cs。 通过熔盐法生长晶体,包括以下步骤:将硼酸铍硼酸盐与助熔剂以适当的比例混合,升至750-800℃,保持恒温,然后冷却至2-10℃。 比饱和温度得到升高的溶液; 将种子晶种放入晶体柱中,将晶圆旋转,冷却至饱和温度,然后缓慢冷却; 将得到的晶体升高到液面以上并冷却至室温,得到本发明的非线性光学晶体。 该晶体具有非线性光学效应,宽透光率波长,紫外线吸附边缘低至150nm,不潮解,不溶于稀盐酸和硝酸,具有良好的耐化学性。 本发明的晶体满足紫外激光变频要求,可用于制造非线性光学器件,实现Nd:YAG的第二,第三,第四,第五或第六谐波输出器件,也可以使用 到其他激光器的谐波输出装置,输出等于或低于266nm的可调谐相干光。
    • 5. 发明申请
    • OPTICAL COUPLING DEVICE HAVING KBBF GROUP CRYSTAL COUPLED WITH PRISMS AND METHOD FOR MANUFACTURING SAME
    • 具有KBBF组合晶体的光耦合装置及其制造方法
    • US20140071519A1
    • 2014-03-13
    • US14115261
    • 2012-03-21
    • Chuangtian ChenYong ZhuFeidi FanXiaoyang WangRukang Li
    • Chuangtian ChenYong ZhuFeidi FanXiaoyang WangRukang Li
    • G02F1/35G02F1/355
    • G02F1/3501G02B1/02G02B5/04G02F1/353G02F1/3551G02F2001/3503
    • The present invention relates to a KBBF family nonlinear optical crystal-prism coupler and its method of fabrication. The coupler comprises: a KBBF family crystal with two smooth surfaces; transition layers each of which is deposited on respective one of the two smooth surfaces of the KBBF family crystal; and a pair of prisms each of which optically contacts with respective one of the activated transition layers. The present invention further provides a KBBF family nonlinear optical crystal-prism coupler that comprises: a KBBF family crystal with two smooth surfaces; a pair of prisms each of which has a smooth surfaces; first transition layers each of which is deposited on respective one of the two smooth surfaces of the KBBF family crystal; and second transition layers each of which is deposited on a smooth surface of respective one of the pair of prisms, wherein the first and second transition layers are integral by optical contact. The coupling between the KBBF family crystal and the prisms is achieved by optical contact through transition layers to improve bonding strength.
    • 本发明涉及KBBF系列非线性光学晶体 - 棱镜耦合器及其制造方法。 耦合器包括:具有两个光滑表面的KBBF系列晶体; 过渡层各自沉积在KBBF族晶体的两个平滑表面的相应一个上; 以及一对棱镜,每个棱镜与相应的一个激活的过渡层光学接触。 本发明还提供一种KBBF系列非线性光学晶体 - 棱镜耦合器,其包括:具有两个平滑表面的KBBF族晶体; 一对棱镜具有光滑的表面; 第一过渡层分别沉积在KBBF族晶体的两个光滑表面的相应一个上; 以及第二过渡层,每个过渡层沉积在该对棱镜中的相应一个棱镜的光滑表面上,其中第一和第二过渡层通过光学接触而成一体。 KBBF系列晶体与棱镜之间的耦合是通过过渡层的光学接触来实现的,以提高结合强度。
    • 6. 发明授权
    • Fluoroberyllium borate non-linear optical crystals and their growth and applications
    • 硼酸氟硼酸盐非线性光学晶体及其生长和应用
    • US08023180B2
    • 2011-09-20
    • US12376559
    • 2006-09-15
    • Chuangtian ChenXiaohong WenRukang LiChengqian Zhang
    • Chuangtian ChenXiaohong WenRukang LiChengqian Zhang
    • G02F1/35C30B15/14
    • C30B9/12C30B15/00C30B29/12G02F1/3551
    • A fluoroberyllium borate non-linear optical single crystal is represented by a molecular formula of MBe2BO3F2, wherein M is Rb or Cs. The crystal can be grown by the flux method comprising the steps of mixing a fluoroberyllium borate compound and a flux in proportion, heating the mixture up to 750-800° C., keeping at this temperature and then cooling it to the temperature of 2-10° C. above the saturating point to obtain a fluoroberyllium borate solution at high temperature; putting the seed crystal fixed on the end of a crystal hanging bar into the fluoroberyllium borate solution at high temperature, rotating the crystal hanging bar, cooling the melt solution to its saturating point, then cooling it again slowly, pulling the obtained crystal out of the solution surface, cooling it to room temperature, then obtaining the present fluoroberyllium borate non-linear optical crystal. The crystal has nonlinear optical effect, broad transmittance wave and UV cut-off edge at 150 nm; neither deliquesces nor dissolves in dilute hydrochloric acid or dilute nitric acid; and has good chemical stability. The present crystal is applicable to the need of harmonic generations in the UV range and can be used to make nonlinear optical devices, achieve the output device for the second, third, fourth, fifth or sixth harmonic generations of Nd:YAG laser. They can be also used in harmonic generation devices of other laser wavelength and to generate coherent light with wavelength at or less than 266 nm.
    • 硼酸氟硼酸非线性光学单晶由MBe2BO3F2的分子式表示,其中M为Rb或Cs。 该晶体可以通过助熔剂法生长,该方法包括以下步骤:将氟硼酸铋化合物和助熔剂按比例混合,将混合物加热至750-800℃,保持该温度,然后冷却至2- 在饱和点以上10℃,在高温下得到硼酸氟硼酸盐溶液; 将晶体固定在晶体悬挂杆的末端,在高温下放入硼酸氟硼酸盐溶液中,旋转晶体悬挂杆,将熔融溶液冷却至饱和点,然后缓慢冷却,将得到的晶体从 溶液表面,冷却至室温,然后得到本发明的硼酸氟硼酸盐非线性光学晶体。 该晶体具有非线性光学效应,在150nm处具有宽透射波和UV截止边缘; 既不会溶解在稀盐酸或稀硝酸中; 并具有良好的化学稳定性。 本发明的晶体适用于紫外范围内谐波代的需要,可用于制造非线性光学器件,实现Nd:YAG激光二次,三次,四次,五次或六次谐波的输出装置。 它们也可用于其他激光波长的谐波发生装置,并产生波长在266nm以下的相干光。
    • 8. 发明申请
    • FLUOROBERYLLIUM BORATE NON-LINEAR OPTICAL CRYSTALS, THEIR GROWTH METHODS AND USES
    • 氟硼酸盐非线性光学晶体,其生长方法和用途
    • US20110222143A1
    • 2011-09-15
    • US13113613
    • 2011-05-23
    • Chuangtian ChenXiaohong WenRukang LiChengqian Zhang
    • Chuangtian ChenXiaohong WenRukang LiChengqian Zhang
    • G02F1/355
    • C30B9/12C30B15/00C30B29/12G02F1/3551
    • A fluoroberyllium borate non-linear optical single crystal is represented by a molecular formula of MBe2BO3F2, wherein M is Rb or Cs. The crystal can be grown by the flux method comprising the steps of mixing a fluoroberyllium borate compound and a flux in proportion, heating the mixture up to 750-800° C., keeping at this temperature and then cooling it to the temperature of 2-10° C. above the saturating point to obtain a fluoroberyllium borate solution at high temperature; putting the seed crystal fixed on the end of a crystal hanging bar into the fluoroberyllium borate solution at high temperature, rotating the crystal hanging bar, cooling the melt solution to its saturating point, then cooling it again slowly, pulling the obtained crystal out of the solution surface, cooling it to room temperature, then obtaining the present fluoroberyllium borate non-linear optical crystal. The crystal has nonlinear optical effect, broad transmittance wave and UV cut-off edge at 150 nm; neither deliquesces nor dissolves in dilute hydrochloric acid or dilute nitric acid; and has good chemical stability. The present crystal is applicable to the need of harmonic generations in the UV range and can be used to make nonlinear optical devices, achieve the output device for the second, third, fourth, fifth or sixth harmonic generations of Nd:YAG laser. They can be also used in harmonic generation devices of other laser wavelength and to generate coherent light with wavelength at or less than 266 nm.
    • 硼酸氟硼酸非线性光学单晶由MBe2BO3F2的分子式表示,其中M为Rb或Cs。 该晶体可以通过助熔剂法生长,该方法包括以下步骤:将氟硼酸铋化合物和助熔剂按比例混合,将混合物加热至750-800℃,保持该温度,然后冷却至2- 在饱和点以上10℃,在高温下得到硼酸氟硼酸盐溶液; 将晶体固定在晶体悬挂杆的末端,在高温下放入硼酸氟硼酸盐溶液中,旋转晶体悬挂杆,将熔融溶液冷却至饱和点,然后缓慢冷却,将得到的晶体从 溶液表面,冷却至室温,然后得到本发明的硼酸氟硼酸盐非线性光学晶体。 该晶体具有非线性光学效应,在150nm处具有宽透射波和UV截止边缘; 既不会溶解在稀盐酸或稀硝酸中; 并具有良好的化学稳定性。 本发明的晶体适用于紫外范围内谐波代的需要,可用于制造非线性光学器件,实现Nd:YAG激光二次,三次,四次,五次或六次谐波的输出装置。 它们也可用于其他激光波长的谐波发生装置,并产生波长在266nm以下的相干光。