    • LOW DIELECTRIC BROMINATED RESIN WITH A SYMMETRIC OR SATURATED HETEROCYCLIC ALPHATIC MOLECULAR STRUCTURE AND THE PREPARATION THEREOF
    • 具有对称或饱和杂环化合物分子结构的低介电自旋树脂及其制备方法
    • US20110245431A1
    • 2011-10-06
    • US12752450
    • 2010-04-01
    • Ming Jen TZOUChi Cheng ChenChih Hong Chen
    • Ming Jen TZOUChi Cheng ChenChih Hong Chen
    • C08L63/00C08G65/40
    • C08G59/08C08G59/1438
    • The present invention provides a brominated epoxy resin, which has a molecular segment of low polarity in the polymer chain, while the molecular segment of low polarity is attributed to the symmetric or saturated cyclic alphatic molecular structure with low “molecular dipole moment” characteristics; making a printed circuit board for high frequency signal transformation applications needs a proper copper clad laminate which processes the properties of a low dielectric constant and of a low dissipation factor; a copper clad laminate can meet above requirements by using the inventive resin as a laminate binder. The inventive resin is prepared by the following steps: 1. Reacting a 2,6-disubstituted mono-phenol compound (A) with an aldehyde or a cyclic diene compound (B), so as to obtain a bisphenol compound (C) having a high symmetry or saturated aliphatic heterocyclic structure; 2. Reacting the resultant symmetric or saturated cyclic diphenol compound (C) with epichlorohydrin for an epoxidation reaction to obtain an epoxy resin (D); and 3. Reacting the resultant epoxy resin (D) with a bromine-containing phenolic compound (E) to obtain the inventive novel brominated epoxy resin (F).
    • 本发明提供了一种溴化环氧树脂,其在聚合物链中具有低极性的分子链段,而低极性的分子链段归因于具有低“分子偶极矩”特性的对称或饱和环状脂肪分子结构; 制造用于高频信号转换应用的印刷电路板需要适当的覆铜层压板,其处理低介电常数和低损耗因子的性质; 通过使用本发明的树脂作为层压粘合剂,覆铜层压板可以满足上述要求。 本发明的树脂通过以下步骤制备:1.用醛或环二烯化合物(B)反应2,6-二取代的单酚化合物(A),以获得具有 高对称性或饱和脂肪杂环结构; 2.用环氧氯丙烷反应所得到的对称或饱和环状二酚化合物(C)进行环氧化反应得到环氧树脂(D); 和3.将得到的环氧树脂(D)与含溴酚化合物(E)反应,得到本发明的新型溴化环氧树脂(F)。
    • 2. 发明授权
    • Capacitive touch module and display having capacitive touch module
    • 电容式触摸模块和具有电容式触摸模块的显示器
    • US09007537B2
    • 2015-04-14
    • US13612886
    • 2012-09-13
    • Kyaw Kyaw TunChao-Chen WangChi-Cheng Chen
    • Kyaw Kyaw TunChao-Chen WangChi-Cheng Chen
    • G02F1/1335G06F3/044
    • G06F3/044
    • A capacitive touch module includes a first glass layer, a second glass layer, a liquid crystal layer, a first insulating layer, a second insulating layer, a plurality of first electrodes, second electrodes and third electrodes. The liquid crystal layer is arranged between the first glass layer and the second glass layer. The first insulating layer is formed between the first glass layer and the liquid crystal layer. The second insulating layer is formed between the liquid crystal layer and the second glass layer. The plurality of first electrodes are formed between the liquid crystal layer and the first insulating layer along a first axis. The plurality of second electrodes are formed between the second insulating layer and the second glass layer along the first axis. The plurality of third electrodes are formed between the first insulating layer and the first glass layer along a second axis.
    • 电容式触摸模块包括第一玻璃层,第二玻璃层,液晶层,第一绝缘层,第二绝缘层,多个第一电极,第二电极和第三电极。 液晶层布置在第一玻璃层和第二玻璃层之间。 第一绝缘层形成在第一玻璃层和液晶层之间。 第二绝缘层形成在液晶层和第二玻璃层之间。 多个第一电极沿着第一轴线形成在液晶层和第一绝缘层之间。 多个第二电极沿着第一轴线形成在第二绝缘层和第二玻璃层之间。 多个第三电极沿着第二轴线形成在第一绝缘层和第一玻璃层之间。
    • 3. 发明申请
    • VARNISH COMPOSITION WITH HIGH TEMPERATURE OF GLASS TRANSITION FOR GLASS FIBER LAMINATE
    • 玻璃纤维层压玻璃过渡温度变化组成
    • US20110306725A1
    • 2011-12-15
    • US13034896
    • 2011-02-25
    • MING-JEN TZOUCHI-CHENG CHENMEI-LING CHEN
    • MING-JEN TZOUCHI-CHENG CHENMEI-LING CHEN
    • C09D179/04
    • C09D179/04C08L61/06C08L61/22C08L61/28
    • A varnish composition includes (1) a benzoxazine resin having highly symmetric molecular structure; (2) at least one of naphthol type novolac resins, aniline type novolac resins and phenolic type novolac resins; (3) fillers. The benzoxazine resin having highly symmetric molecular structure, and the at least one of naphthol type novolac resins, aniline type novolac resins and phenolic type novolac resins contribute to increase the temperature of glass transition of the varnish composition, while decrease the coefficient of thermal expansion and moisture absorbability due to their small and highly symmetric molecular structures. A copper substrate can meet the requirement of high temperature of glass transition (TMA≧200° C.) and low coefficient of thermal expansion (α1/α≦30/1350(μm/(m° C.). Therefore, the composition of the invention can be widely used as high-performance electronic material.
    • 清漆组合物包括(1)具有高对称分子结构的苯并恶嗪树脂; (2)萘酚型酚醛清漆树脂,苯胺型酚醛清漆树脂和酚醛型酚醛清漆树脂中的至少一种; (3)填料。 具有高对称分子结构的苯并恶嗪树脂和萘酚型酚醛清漆树脂,苯胺型酚醛清漆树脂和酚醛型酚醛清漆树脂中的至少一种有助于提高清漆组合物的玻璃化转变温度,同时降低热膨胀系数, 由于它们的分子结构小而高度对称而具有吸湿性。 铜基材可以满足玻璃化转变温度高(TMA≥200℃)和低热膨胀系数(α1/α≦̸ 30/1350(μm/(m℃))的要求,因此, 本发明可广泛用作高性能电子材料。
    • 4. 发明申请
    • CAPACITIVE TOUCH MODULE AND DISPLAY HAVING CAPACITIVE TOUCH MODULE
    • 电容触摸模块和显示器具有电容触摸模块
    • US20130314623A1
    • 2013-11-28
    • US13612886
    • 2012-09-13
    • Kyaw Kyaw TunChao-Chen WangChi-Cheng Chen
    • Kyaw Kyaw TunChao-Chen WangChi-Cheng Chen
    • G02F1/1343
    • G06F3/044
    • A capacitive touch module includes a first glass layer, a second glass layer, a liquid crystal layer, a first insulating layer, a second insulating layer, a plurality of first electrodes, second electrodes and third electrodes. The liquid crystal layer is arranged between the first glass layer and the second glass layer. The first insulating layer is formed between the first glass layer and the liquid crystal layer. The second insulating layer is formed between the liquid crystal layer and the second glass layer. The plurality of first electrodes are formed between the liquid crystal layer and the first insulating layer along a first axis. The plurality of second electrodes are formed between the second insulating layer and the second glass layer along the first axis. The plurality of third electrodes are formed between the first insulating layer and the first glass layer along a second axis.
    • 电容式触摸模块包括第一玻璃层,第二玻璃层,液晶层,第一绝缘层,第二绝缘层,多个第一电极,第二电极和第三电极。 液晶层布置在第一玻璃层和第二玻璃层之间。 第一绝缘层形成在第一玻璃层和液晶层之间。 第二绝缘层形成在液晶层和第二玻璃层之间。 多个第一电极沿着第一轴线形成在液晶层和第一绝缘层之间。 多个第二电极沿着第一轴线形成在第二绝缘层和第二玻璃层之间。 多个第三电极沿着第二轴线形成在第一绝缘层和第一玻璃层之间。
    • 5. 发明授权
    • Varnish composition with high glass transition temperature for glass fiber laminate
    • 玻璃纤维层压板玻璃化转变温度高的清漆组合物
    • US08536283B2
    • 2013-09-17
    • US13034896
    • 2011-02-25
    • Ming-Jen TzouChi-Cheng ChenMei-Ling Chen
    • Ming-Jen TzouChi-Cheng ChenMei-Ling Chen
    • C08L61/14C08K5/5313
    • C09D179/04C08L61/06C08L61/22C08L61/28
    • A varnish composition includes (1) a benzoxazine resin having highly symmetric molecular structure; (2) at least one of naphthol novolac resins, aniline novolac resins and phenolic novolac resins; (3) fillers. The benzoxazine resin having highly symmetric molecular structure, and the at least one of naphthol novolac resins, aniline novolac resins and phenolic novolac resins contribute to increase the glass transition temperature of the varnish composition, while decrease the coefficient of thermal expansion and moisture absorbability due to their small and highly symmetric molecular structures. A copper substrate can meet the requirement of high glass transition temperature (TMA≧200° C.) and low coefficient of thermal expansion (α1/α≦30/135 (μm/m° C.). Therefore, the composition of the invention can be widely used as high-performance electronic material.
    • 清漆组合物包括(1)具有高对称分子结构的苯并恶嗪树脂; (2)萘酚酚醛清漆树脂,苯胺酚醛清漆树脂和苯酚酚醛清漆树脂中的至少一种; (3)填料。 具有高度对称分子结构的苯并嗪树脂,以及萘酚酚醛清漆树脂,苯胺酚醛清漆树脂和酚醛清漆树脂中的至少一种有助于提高清漆组合物的玻璃化转变温度,同时降低由此产生的热膨胀系数和吸湿性 它们的小而高度对称的分子结构。 铜基材可以满足高玻璃化转变温度(TMA> = 200℃)和低热膨胀系数(α1/α@ 30/135(mum / m℃))的要求,因此, 发明可广泛用作高性能电子材料。
    • 6. 发明授权
    • Low dielectric brominated resin with a symmetric or saturated heterocyclic alphatic molecular structure and the preparation thereof
    • 具有对称或饱和杂环脂肪分子结构的低介电溴化树脂及其制备方法
    • US08039560B1
    • 2011-10-18
    • US12752450
    • 2010-04-01
    • Ming Jen TzouChi Cheng ChenChih Hong Chen
    • Ming Jen TzouChi Cheng ChenChih Hong Chen
    • C08L63/04
    • C08G59/08C08G59/1438
    • The present invention provides a brominated epoxy resin, which has a molecular segment of low polarity in the polymer chain, while the molecular segment of low polarity is attributed to the symmetric or saturated cyclic alphatic molecular structure with low “molecular dipole moment” characteristics; making a printed circuit board for high frequency signal transformation applications needs a proper copper clad laminate which processes the properties of a low dielectric constant and of a low dissipation factor; a copper clad laminate can meet above requirements by using the inventive resin as a laminate binder. The inventive resin is prepared by the following steps: 1. Reacting a 2,6-disubstituted mono-phenol compound (A) with an aldehyde or a cyclic diene compound (B), so as to obtain a bisphenol compound (C) having a high symmetry or saturated aliphatic heterocyclic structure; 2. Reacting the resultant symmetric or saturated cyclic diphenol compound (C) with epichlorohydrin for an epoxidation reaction to obtain an epoxy resin (D); and 3. Reacting the resultant epoxy resin (D) with a bromine-containing phenolic compound (E) to obtain the inventive novel brominated epoxy resin (F).
    • 本发明提供了一种溴化环氧树脂,其在聚合物链中具有低极性的分子链段,而低极性的分子链段归因于具有低“分子偶极矩”特性的对称或饱和环状脂肪分子结构; 制造用于高频信号转换应用的印刷电路板需要适当的覆铜层压板,其处理低介电常数和低损耗因子的性质; 通过使用本发明的树脂作为层压粘合剂,覆铜层压板可以满足上述要求。 本发明的树脂通过以下步骤制备:1.用醛或环二烯化合物(B)反应2,6-二取代的单酚化合物(A),以获得具有 高对称性或饱和脂肪杂环结构; 2.用环氧氯丙烷反应所得到的对称或饱和环状二酚化合物(C)进行环氧化反应得到环氧树脂(D); 和3.将得到的环氧树脂(D)与含溴酚化合物(E)反应,得到本发明的新型溴化环氧树脂(F)。