热词
    • 72. 发明授权
    • Production process for particulate water-absorbent resin
    • 颗粒状吸水树脂的生产工艺
    • US06875511B2
    • 2005-04-05
    • US10443777
    • 2003-05-23
    • Yorimichi DairokuYoshio IrieKenji TadaShinichi FujinoMakoto Nagasawa
    • Yorimichi DairokuYoshio IrieKenji TadaShinichi FujinoMakoto Nagasawa
    • C08J3/12B32B5/16
    • C08J3/12C08J3/122C08J2300/14Y10T428/2982Y10T428/2985Y10T428/2991Y10T428/2998
    • The present invention provides: a production process for a particulate water-absorbent resin with high productivity, which production process is carried out in such a manner that the particulate water-absorbent resin will contain particles with particle diameters of 150 to 850 μm (but excluding 850 μm) in an amount of not smaller than 75 weight % of the particulate water-absorbent resin after the pulverization step or after the pulverization step and the drying step even if the adjustment of the particle diameters is not carried out by the sieving classification procedure; a novel particulate water-absorbent resin having high properties; and a sanitary material comprising this particulate water-absorbent resin. The production process for a particulate water-absorbent resin, according to the present invention, is carried out in such a manner that the particulate water-absorbent resin will contain particles with particle diameters of 150 to 850 μm (but excluding 850 μm) in an amount of not smaller than 75 weight % of the particulate water-absorbent resin after the pulverization step or after the pulverization step and the drying step; with the production process being characterized in that, in the pulverization step, a hydropolymer of a water-absorbent resin having a water content of 10 to 30 weight % is pulverized with a pulverizer.
    • 本发明提供一种高生产率的颗粒状吸水性树脂的制造方法,该制造方法以粒状吸水性树脂含有粒径为150〜850μm的粒子(但不包括 850μm),在粉碎步骤之后或粉碎步骤和干燥步骤之后的颗粒状吸水性树脂的75重量%以上,即使不通过筛分分级程序进行粒径的调整 ; 具有高性能的新型颗粒状吸水性树脂; 以及包含该颗粒状吸水性树脂的卫生材料。 根据本发明的颗粒状吸水性树脂的制造方法,是使颗粒状吸水性树脂含有粒径为150〜850μm(但不包括850μm)的颗粒, 在粉碎步骤之后或粉碎步骤和干燥步骤之后的颗粒状吸水性树脂的75重量%以上的量; 其制造方法的特征在于,在粉碎工序中,用粉碎机粉碎含水率为10〜30重量%的吸水性树脂的氢化聚合物。
    • 74. 发明授权
    • Process for preparing an absorbent resin crosslinked with a mixture of
trimethylolpropane diacrylate and triacrylate
    • 制备用三羟甲基丙烷二丙烯酸酯和三丙烯酸酯的混合物交联的吸收性树脂的方法
    • US5574121A
    • 1996-11-12
    • US262065
    • 1994-06-17
    • Yoshio IrieNobuyuki HaradaKinya NagasunaKohichi HirotaYoshihiko MasudaHideaki NaganoHideyuki Kubo
    • Yoshio IrieNobuyuki HaradaKinya NagasunaKohichi HirotaYoshihiko MasudaHideaki NaganoHideyuki Kubo
    • A61L15/24C08F220/04C08F236/22
    • C08F220/04A61L15/24Y10S526/93
    • A process for preparing an absorbent resin includes the steps of: preparing a first crosslinking agent (A) including at least two polymerizable unsaturated bonds; preparing a second crosslinking agent (B) including at least two polymerizable unsaturated bonds and hydroxyl groups; preparing a crosslinking agent including (A) and (B) with a ratio of (A) to (B) ranging from 95/5 to 50/50; and polymerizing a hydrophilic unsaturated monomer having at least one carboxyl group using the crosslinking agent. The crosslinking agent includes a crosslinking agent which includes a main component at least 90 percent by weight, the main component being an ester having at least two polymerizable unsaturated bonds, wherein the ester is composed of a polyhydroxy alcohol (C) having not more than six carbon atoms and at least three hydroxy groups, and an unsaturated carboxylic acid (D); and a molecular weight ratio of the main component to a standard compound (E) is in the range of from 0.7/1 to less than 1.3/1, (E) being an ester composed of (C) that composes the main component, and (D) that composes the main component, in which all the hydroxy groups in (C) are ester-linked with (D).
    • 制备吸收性树脂的方法包括以下步骤:制备包含至少两个可聚合不饱和键的第一交联剂(A); 制备包含至少两个可聚合不饱和键和羟基的第二交联剂(B); 制备包含(A)和(B)的交联剂,比例为(A)至(B)为95/5至50/50; 并使用交联剂聚合具有至少一个羧基的亲水性不饱和单体。 交联剂包括交联剂,其包含至少90重量%的主要组分,主要组分是具有至少两个可聚合不饱和键的酯,其中该酯由不超过六个的多羟基醇(C)组成 碳原子和至少三个羟基,和不饱和羧酸(D); 并且主成分与标准化合物(E)的分子量比在0.7 / 1〜小于1.3 / 1的范围内,(E)是由构成主成分的(C)构成的酯,和 (D)构成其中(C)中的所有羟基与(D)酯连接的主要组分。