    • 75. 发明申请
    • Methods for controlling migration of particulates in a subterranean formation
    • 控制地层中颗粒迁移的方法
    • US20060219408A1
    • 2006-10-05
    • US11092210
    • 2005-03-29
    • Philip NguyenRichard RickmanRonald DusterhoftJohnny Barton
    • Philip NguyenRichard RickmanRonald DusterhoftJohnny Barton
    • E21B33/138E21B43/22
    • C09K8/5753C09K8/5083C09K8/5086C09K8/5755
    • Methods of controlling particulate migration in a portion of a subterranean formation comprising placing a pre-flush fluid into the portion of the subterranean formation; and then, placing a low-viscosity adhesive substance diluted with an aqueous dissolvable solvent into the portion of the subterranean formation; wherein the portion of a subterranean formation being treated has a regain permeability of at least about 70%. Methods of creating a stabilized region around a portion of a subterranean formation around a well bore having a screen or liner in place in that portion of the subterranean formation comprising placing a pre-flush fluid into the portion of the subterranean formation; and then, placing a low-viscosity adhesive substance diluted with an aqueous dissolvable solvent into that portion of the subterranean formation; wherein the portion of a subterranean formation being treated has regain permeability of at least about 70%.
    • 控制地下地层部分中的微粒迁移的方法,包括将预冲洗流体置于地层的一部分中; 然后将用水溶性溶剂稀释的低粘度粘合剂物质放置到地层的部分中; 其中被处理的地层的部分具有至少约70%的回弹渗透率。 在围绕井眼周围的地下地层的一部分周围形成稳定区域的方法,其中所述地下地层的该部分中具有筛网或衬套就位,包括将预冲洗流体放置到地下地层的该部分中; 然后将用水溶性溶剂稀释的低粘度粘合剂物质放置在该地层的该部分中; 其中被处理的地层的部分重新获得至少约70%的渗透率。
    • 77. 发明申请
    • Methods for preparing slurries of coated particulates
    • 制备涂层颗粒的浆料的方法
    • US20060180307A1
    • 2006-08-17
    • US11397455
    • 2006-04-04
    • Billy SlabaughJimmie WeaverPhilip Nguyen
    • Billy SlabaughJimmie WeaverPhilip Nguyen
    • E21B43/267
    • C09K8/805C09K8/68E21B43/267Y10T428/2998
    • A method of using coated proppant slurries in subterranean applications such as production enhancement and sand control. Some embodiments of the present invention provide methods of creating a stable slurry of coated particulates wherein the slurry is capable of being stored for at least 2 hours before use comprising the steps of: providing resin coated particulates wherein the resin comprises a resin that does not completely cure unless it is at least one of exposed to a temperature above about 175° F. or exposed to an external catalyst; and, substantially suspending the resin coated particulates in a servicing fluid to create a stable resin coated particulate slurry. Other embodiments of the present invention provide methods of creating a stable slurry of coated particulates wherein the slurry is capable of being stored for at least 2 hours before use comprising the steps of: providing tackifyer coated particulates; and, substantially suspending the tackifyer coated particulates in a servicing fluid to create a tackifyer coated particulate slurry.
    • 在地下应用中使用涂覆的支撑剂浆料的方法,例如生产增强和防砂。 本发明的一些实施方案提供了产生涂覆颗粒的稳定淤浆的方法,其中浆料能够在使用前储存至少2小时,包括以下步骤:提供树脂涂覆的颗粒,其中树脂包含不完全的树脂 除非是暴露于高于约175°F或暴露于外部催化剂的温度中的至少一种而固化; 并且将树脂涂覆的颗粒基本上悬浮在维修流体中以产生稳定的树脂涂覆的颗粒浆料。 本发明的其它实施方案提供了产生涂覆颗粒的稳定淤浆的方法,其中浆料能够在使用前储存至少2小时,包括以下步骤:提供增粘剂涂覆的颗粒; 并且将粘合剂涂覆的颗粒基本上悬浮在维修流体中以产生粘合剂涂覆的颗粒浆料。
    • 78. 发明申请
    • Methods for fracturing subterranean wells
    • 压裂地下井的方法
    • US20060157243A1
    • 2006-07-20
    • US11035833
    • 2005-01-14
    • Philip Nguyen
    • Philip Nguyen
    • E21B43/267
    • C09K8/805E21B43/267
    • A method of forming a propped fracture comprising: providing a fracture having a far-well bore area and a near-well bore area; placing first proppant particulates at least partially coated with an adhesive substance; placing a portion of second proppant particulates in the near-well bore area of the fracture so as to form a high porosity propped region in the near-well bore. A method of stimulating a producing interval comprising: hydraulically fracturing to create a fracture having a far-well bore area and a near-well bore area; placing a portion of first proppant particulates at least partially coated with an adhesive substance in the far-well bore area of the fracture; and, placing a portion of second proppant particulates in the near-well bore area of the fracture to form a high porosity propped region in the near-well bore area.
    • 形成支撑断裂的方法,包括:提供具有远井孔面积和近井孔面积的断裂; 将第一支撑剂颗粒至少部分地涂覆有粘合剂物质; 将第二支撑剂颗粒的一部分放置在裂缝的近井孔区域中,以在近井孔中形成高孔隙度支撑区域。 一种刺激产生间隔的方法,包括:水力压裂以产生具有远井孔面积和近井孔面积的断裂; 将第一支撑剂颗粒的一部分至少部分地用粘合剂物质涂覆在所述断裂的远井区域中; 并且将第二支撑剂颗粒的一部分放置在裂缝的近井孔区域中,以在近井孔区域中形成高孔隙度支撑区域。
    • 79. 发明申请
    • Low-quality particulates and methods of making and using improved low-quality particulates
    • 低质量的微粒和制造和使用改进的低质量颗粒物的方法
    • US20060124303A1
    • 2006-06-15
    • US11011394
    • 2004-12-12
    • Philip NguyenJohnny Barton
    • Philip NguyenJohnny Barton
    • E21B43/267
    • C09K8/805Y10S507/924
    • A method of treating a subterranean formation, comprising: at least partially coating particulates with a first layer of a first curable resin and allowing the first curable resin to substantially cure; and then, at least partially coating the particulates with a second layer of a second curable resin; and allowing the second layer of the second curable resin to substantially cure; and then, slurrying the coated particulates into a treatment fluid and placing the slurry into a subterranean formation. Improved particulates suitable for use in subterranean formations, comprising low-quality particulates that have been at least partially coated with a first layer of a first curable resin and then at least partially coated with a second layer of a second curable resin and wherein the first layer of the first curable resin is allowed to substantially cure before the application of the second layer of the second curable resin.
    • 一种处理地层的方法,包括:至少部分地用第一可固化树脂的第一层涂覆微粒,并允许第一可固化树脂基本固化; 然后用第二可固化树脂层至少部分地涂覆微粒; 并允许第二可固化树脂的第二层基本固化; 然后将涂覆的颗粒浆化成处理流体并将浆料置于地层中。 改进的适用于地下地层的颗粒,包括至少部分地涂覆有第一可固化树脂的第一层然后至少部分地涂覆有第二可固化树脂层的低质量颗粒,并且其中第一层 的第一可固化树脂在施加第二可固化树脂的第二层之前被允许基本固化。