    • 62. 发明授权
    • Luminescent glass element, producing method thereof and luminescing method thereof
    • 发光玻璃元件及其制造方法及其发光方法
    • US08217369B2
    • 2012-07-10
    • US13229535
    • 2011-09-09
    • Mingjie ZhouWenbo MaYugang Liu
    • Mingjie ZhouWenbo MaYugang Liu
    • G01N21/64
    • H01J63/04C03C3/062C03C3/095C03C4/12C03C17/09Y10T428/265
    • The present invention relates to a luminescent glass element comprising a luminescent glass substrate, which a metal layer is positioned on a surface thereof. The metal layer is provided with a metal microstructure. The luminescent glass substrate has composite oxides represented as the following formula: aM2O.bY2O3.cSiO2.dPr2O3, wherein M represents alkali metal element, a, b, c and d are, by mol part, 25-60, 1-30, 20-70 and 0.001-10 respectively. The present invention also provides a producing method of the luminescent glass element and a luminescing method thereof. The metal layer is positioned on the luminescent glass substrate, thereby improving luminescence efficiency of the luminescent glass substrate. The luminescent glass element can be used in luminescent devices with ultrahigh brightness or high-speed operation.
    • 本发明涉及包含发光玻璃基板的发光玻璃元件,金属层位于其表面上。 金属层设有金属微结构。 发光玻璃基板具有由下式表示的复合氧化物:aM2O.bY2O3.cSiO2.dPr2O3,其中M表示碱金属元素,a,b,c和d分别为25-60,1-30,20 -70和0.001-10。 本发明还提供了发光玻璃元件的制造方法及其发光方法。 金属层位于发光玻璃基板上,从而提高发光玻璃基板的发光效率。 发光玻璃元件可用于具有超高亮度或高速操作的发光装置。
    • 63. 发明申请
    • Rare Earth Ion Doped Silicate Luminescence Glass and Preparation Method Thereof
    • 稀土离子掺杂硅酸盐发光玻璃及其制备方法
    • US20120061615A1
    • 2012-03-15
    • US13320753
    • 2009-05-19
    • Mingjie ZhouWenbo MaZhaopu ShiYanbo QiaoQingtao Li
    • Mingjie ZhouWenbo MaZhaopu ShiYanbo QiaoQingtao Li
    • C09K11/79
    • C03C4/12C03C3/062C03C3/095
    • A rare earth ion doped silicate luminescence glass and preparation method thereof are provided. The luminescence glass is the material with the following formula: aM2O.bM′2O3.cSiO2.dRE2O3, wherein M is at least one of Na, K and Li, M′ is at least one of Y, Gd, La, Sc and Lu, RE is at least one of Ce, Tm, Tb, Ho, Dy, Er, Nd, Sm, Eu and Pr. The preparation method is: grinding the raw material until mixed uniformly, calcining the raw material at 1200-1500° C. for 1-5 h, cooling to room temperature, annealing at 600-1100° C. for 0.5-24 h, cooling to room temperature again, molding then getting the product. The performance of the product is stable. The product is homogenous, and the luminescence performance is good. The light transmittance is high. The process of the preparation method is simple and with low cost.
    • 提供了一种稀土离子掺杂硅酸盐发光玻璃及其制备方法。 发光玻璃是具有下式的材料:aM2O.bM'2O3.cSiO2.dRE2O3,其中M是Na,K和Li中的至少一种,M'是Y,Gd,La,Sc和Lu中的至少一种 ,RE为Ce,Tm,Tb,Ho,Dy,Er,Nd,Sm,Eu和Pr中的至少一种。 制备方法为:研磨原料直至混合均匀,在1200-1500℃下煅烧原料1-5小时,冷却至室温,在600-1100℃退火0.5-24小时,冷却 再到室温,成型然后得到产品。 产品性能稳定。 产品均匀,发光性能好。 透光率高。 制备方法简单,成本低。