    • Welding of glassy metallic materials
    • 玻璃状金属材料的焊接
    • US4115682A
    • 1978-09-19
    • US744658
    • 1976-11-24
    • Sheldon KaveshGerald R. Bretts
    • Sheldon KaveshGerald R. Bretts
    • B23K11/16B23K11/26C21D9/50
    • C21D9/50C21D2201/03C21D2251/00
    • A process is provided for welding metal bodies together, at least one of the metal bodies comprising a metallic material that is at least 50% glassy. The process comprises (a) clamping overlapped portions of the bodies between electrodes and applying a clamping force to the overlapped portions; (b) passing an electrical current having a rapid decay such that at least about 90% of the energy is delivered in less than about 4 .times. 10.sup.-3 sec through the bodies to melt at least a portion of one of the bodies, and (c) extracting heat from the bodies through the electrodes at a rate of at least about 10.sup.5 .degree. C/sec by employing high conductivity electrodes having a thermal conductivity of at least about 0.30 cal/sec/cm.sup.2 /.degree. C to form a weld nugget joining the bodies. The weld nugget so formed has a shear strength which is at least 25% of the tensile strength of the body having the lowest tensile strength.
    • 提供了一种用于将金属体焊接在一起的方法,所述金属体中的至少一个包括至少50%玻璃状的金属材料。 该方法包括(a)将电极的重叠部分夹在电极之间并向重叠部分施加夹紧力; (b)通过具有快速衰减的电流,使得至少约90%的能量以小于约4×10 -3秒的速度输送通过体,以熔化其中一个体的至少一部分,和( c)通过使用具有至少约0.30cal / sec / cm 2 /℃的导热率的高电导率电极,以至少约105℃/秒的速率从所述电极提取热量以形成焊接熔核接合 身体。 如此形成的焊接熔核具有至少具有拉伸强度最低的主体的拉伸强度的25%的剪切强度。