    • Preparation of thermoplastics
    • 热塑性塑料的制备
    • US5910276A
    • 1999-06-08
    • US620310
    • 1996-03-22
    • Norbert GuntherbergJurgen HofmannHilmar OhligElmar MailahnKlaus BusBernhard CzaudernaSven Grabowski
    • Norbert GuntherbergJurgen HofmannHilmar OhligElmar MailahnKlaus BusBernhard CzaudernaSven Grabowski
    • B29B7/88B29B7/48B29B7/58B29C47/40B29C47/76C08G85/00C08J3/20C08J3/205C08L25/04C08L27/06C08L33/04C08L33/12C08L33/18C08L33/20C08L51/00C08L51/04C08L55/02C08L101/00
    • B29C47/767B29C47/40B29C47/6031B29C47/6056B29C47/62B29C47/64B29C47/76C08J3/205C08L51/04C08L55/02B29C47/0011B29C47/0019B29C47/0023B29C47/762
    • Toughened thermoplastics are prepared by mechanically dewatering a water-moist elastomer component A containing up to 60% by weight of residual water and mixing the resulting dewatered elastomer component A' with a thermoplastic polymer B in an extruder, by a process in which the elastomer component A is fed to a twin-screw extruder which has corotating, in each case double-flight, screws and essentially includes, in the transport direction,a metering section in which the elastomer component A is fed to the extruder by a metering means,at least one squeeze section which serves for dewatering and contains at least one retarding element and in each case at least one associated dewatering orifice,at least one section provided with a conveying screw or at least one section provided with mixing, kneading or other plasticating elements or combinations of these elements,at least one section in which the thermoplastic polymer B is introduced as a melt into the extruder,at least one section provided with mixing, kneading or other plasticating elements or combinations of these elements,at least one devolatilization section which is provided with at least one devolatilization orifice and in which the residual water is removed as steam, anda discharge zone,the water emerging from the dewatering orifices being present partially or completely in the liquid phase, and the extruder being operated at a screw speed of from 50 to 600 min.sup.-1 and average shear rates of from 20 to 240 s.sup.-1.
    • 通过机械脱水含有高达60重量%的残余水的水分弹性体组分A并将所得脱水的弹性体组分A'与热塑性聚合物B混合在挤出机中,通过以下方法制备增韧的热塑性塑料,其中弹性体组分 A被输送到双螺杆挤出机,双螺杆挤出机在每个情况下都具有旋转螺旋,并且在输送方向上基本上包括计量部分,其中弹性体组分A通过计量装置进料到挤出机, 至少一个挤压部分,其用于脱水并且包含至少一个延迟元件,并且在每种情况下包括至少一个相关联的脱水孔,设置有输送螺杆的至少一个部分或设置有混合,捏合或其它塑化元件的至少一个部分, 这些元件的组合,将热塑性聚合物B作为熔体引入挤出机中的至少一个部分,至少一个部分 n具有混合,捏合或其它塑化元件或这些元素的组合,至少一个脱挥发段,其设置有至少一个脱挥发分孔,残留水作为蒸汽除去,以及排出区,从 脱水孔部分或完全在液相中存在,挤出机以50至600分钟-1的螺杆速度和20至240s -1的平均剪切速率操作。