    • 25. 发明授权
    • Method of making fiber optic coupler
    • 制造光纤耦合器的方法
    • US5078767A
    • 1992-01-07
    • US600613
    • 1990-10-19
    • George E. Berkey
    • George E. Berkey
    • G02B6/28
    • G02B6/2835
    • A method disclosure for making an economical fiber coupler including providing a glass tube having first and second end portions and a midregion, and a longitudinal aperture extending through it. Two suitably prepared glass optical fibers, each having a core and cladding, are disposed within the longitudinal aperture, the fibers extending beyond each end of the tube. The fibers are glued to each end portion. The midregion of the tube is evacuated, heated, collapsed about the fibers, and drawn to reduce the diameter of the resulting composite.
    • 一种用于制造经济的光纤耦合器的方法公开,包括提供具有第一和第二端部和中间区域的玻璃管,以及延伸穿过该玻璃管的纵向孔。 每个具有芯和包层的两个适当制备的玻璃光纤布置在纵向孔内,纤维延伸超过管的每一端。 纤维粘合到每个端部。 管的中间部分围绕纤维抽真空,加热,折叠,并拉伸以减小所得复合材料的直径。
    • 28. 发明授权
    • Conveyor deposition method and apparatus for making optical fiber
preforms
    • 用于制造光纤预制棒的输送机沉积方法和装置
    • US4684384A
    • 1987-08-04
    • US913134
    • 1986-09-29
    • George E. Berkey
    • George E. Berkey
    • C03B37/014C03B37/027
    • C03B37/01413C03B37/0142C03B37/01486C03B2207/42C03B2207/50C03B2207/52C03B2207/60C03B2207/66
    • A plurality of optical waveguide preforms are simultaneously formed by depositing on a plurality of starting members layers of glass soot to build up a coating on each starting member. The soot layers are deposited by traversing a series of burners along the starting members in such a manner that a given one of the burners traverses the first starting member from a first end thereof to a second end thereof to form a layer of soot thereon. The remaining burners of the series similarly traverses the first starting member, a plurality of burners traversing the first starting member at any given time. After the first burner has traversed the first starting member it similarly traverses the second starting member. After the last of the series of burners has begun its traverse along the first starting member, the first of the series of burners completes its traverse of the second starting member and again begins traversing the first starting member immediately following the last of the series of burners.
    • 通过在多个起始构件层上沉积玻璃烟炱同时形成多个光波导预制件,以在每个起始构件上建立涂层。 烟炱层通过沿起始构件横穿一系列燃烧器以使得给定的一个燃烧器从其第一端至其第二端穿过第一起始构件以在其上形成一层烟炱而沉积。 该系列的其余燃烧器类似地在任何给定时间穿过第一起动件,多个燃烧器穿过第一启动件。 在第一燃烧器已经穿过第一启动构件之后,它类似地穿过第二起动构件。 在一系列燃烧器的最后一个已经开始沿着第一启动构件的横移之后,第一系列燃烧器完成其第二启动构件的横移,并且再次开始遍历第一起动构件,紧接在最后的一系列燃烧器 。
    • 29. 发明授权
    • Method of forming a polarization preserving optical waveguide
    • 形成偏振保留光波导的方法
    • US4578097A
    • 1986-03-25
    • US535466
    • 1983-09-26
    • George E. Berkey
    • George E. Berkey
    • C03B37/014C03B25/02
    • C03B37/01486C03B37/01473C03B2203/30
    • A single-mode optical waveguide is constructed in a manner such that the core thereof is subjected to a stress-induced birefringence. A coating of core glass soot is deposited on the surface of a cylindrical mandrel, and a coating of inner cladding glass soot is deposited on the core glass soot. The mandrel is removed and the resultant porous preform is consolidated to form a hollow dense glass preform. The preform aperture is closed at both ends. Diametrically opposed slabs are removed from the inner cladding region of the consolidated preform. The resultant article is evacuated, heated and stretched to close the aperture and form a preform foreproduct having two opposed rounded sides and two opposed flattened sides. The foreproduct is coated with a layer of outer cladding glass soot having a thermal coefficient of expansion which differs from that of the inner cladding glass by at least 1.times.10.sup.-7 /.degree.C. The resultant composite structure is consolidated to form a draw blank which can be drawn into an optical fiber.
    • 单模光波导以这样的方式构造,使得其芯受到应力诱导的双折射。 核心玻璃烟灰的涂层沉积在圆柱形心轴的表面上,并且内包层玻璃烟灰的涂层沉积在芯玻璃烟灰上。 去除心轴,并将得到的多孔预制件固结,形成中空的致密玻璃预制件。 预制孔的两端封闭。 从固结预成型件的内包层区域去除直径相对的板坯。 将所得制品抽真空,加热和拉伸以封闭孔,并形成具有两个相对的圆形侧面和两个相对的平坦侧面的预制件前置产品。 该前产品具有与内包层玻璃的热膨胀系数不同于内包层玻璃的热膨胀系数的一层外包层玻璃烟炱至少1×10 -7 /℃。所得到的复合结构被固结形成一个可以 被拉入光纤。