    • Resin composition and injection-molded article
    • 树脂组合物和注塑制品
    • US06426385B2
    • 2002-07-30
    • US09780486
    • 2001-02-12
    • Shigeichi Kobayashi
    • Shigeichi Kobayashi
    • C08L2308
    • C08L23/0815C08L23/06C08L2205/02C08L2666/04
    • A resin composition containing: (A) an ethylene-&agr;-olefin copolymer having a melt flow rate of from 0.5 to 100 g/10 min, a density of from 860 to 920 kg/m3, and a highest melting peak temperature of from 50° C. to 110° C.; (B) an ethylene homopolymer or ethylene-&agr;-olefin copolymer having a melt flow rate of from 0.5 to 100 g/10 min, a density of from 910 to 980 kg/m3, and a highest melting peak temperature of from 110° C. to 135° C.; and (C) a low-density polyethylene having a melt flow rate of from 0.5 to 100 g/10 min, and a swell ratio of from 1.3 to 2.0, provides a molded article superior in mold release properties, flexibility and heat resistance, particularly when used in injection molding.
    • 一种树脂组合物,其含有:(A)熔体流动速率为0.5〜100g / 10分钟,密度为860〜920kg / m 3,最高熔融峰温度为50℃的乙烯-α-烯烃共聚物 (B)熔体流动速率为0.5-100g / 10min,密度为910至980kg / m 3的乙烯均聚物或乙烯-α-烯烃共聚物,和 最高熔融峰温度为110℃至135℃。 和(C)熔体流动速率为0.5〜100g / 10分钟,溶胀比为1.3〜2.0的低密度聚乙烯,提供脱模性,柔软性,耐热性优异的成型体 用于注塑成型。