    • 11. 发明授权
    • Method of manufacturing rolling bearings
    • 制造滚动轴承的方法
    • US6101719A
    • 2000-08-15
    • US242817
    • 1999-02-25
    • Akihiro KiuchiShigeru OkitaKenji Yamamura
    • Akihiro KiuchiShigeru OkitaKenji Yamamura
    • C22C38/22C22C38/24C23C8/22C23C8/80F16C33/30F16C33/62B21K1/02
    • C22C38/24C22C38/22C23C8/22C23C8/80F16C33/30F16C33/62Y10T29/49707Y10T29/49709
    • In manufacturing a rolling bearing, at least one component of an inner ring, an outer ring, and a rolling element is manufactured from an alloy steel comprising 0.05 weight %-0.5 weight % carbon, 0.5 weight %-18 weight % chromium, 1.5 weight % or less silicon, 5 weight % or less molybdenum, 4.0 weight % or less vanadium, 4 weight % or less nickel, and 8 weight % or less tungsten, by subjecting the alloy steel to carburizing, hardening and tempering. The carburizing is carried out by vacuum carburization. In the vacuum carburization, carburizing and diffusion are carried out by introducing an acetylene-based carburizing gas in a hot atmosphere under reduced pressure, followed by hardening and tempering. The use of the vacuum carburization enables carburization with the chromium (Cr) content being 3.0 weight % or more, and even up to 18 weight %, which was difficult to achieve with the conventional gas carburization (pre-oxidation+gas carburizing).
    • PCT No.PCT / JP98 / 03782 Sec。 一九九九年二月二十五日 102(e)1999年2月25日PCT PCT 1998年8月26日PCT公布。 公开号WO99 /​​ 10557 日期1999年3月4日在制造滚动轴承时,由含有0.05重量%-0.5重量%碳,0.5重量%-18重量%的合金钢制成内圈,外圈和滚动元件的至少一个部件 铬,1.5重量%以下的硅,5重量%以下的钼,4.0重量%以下的钒,4重量%以下的镍和8重量%以下的钨,通过对合金钢进行渗碳,淬火和回火 。 渗碳是通过真空渗碳进行的。 在真空渗碳中,通过在减压下在热气氛中引入乙炔系渗碳气体进行渗碳扩散,然后硬化和回火。 使用真空渗碳可以使铬(Cr)含量为3.0重量%以上,甚至高达18重量%的渗碳,这是常规的气体渗碳(预氧化+气体渗碳)难以实现的。
    • 13. 发明授权
    • Rolling member
    • 滚动会员
    • US06358333B1
    • 2002-03-19
    • US09576954
    • 2000-05-24
    • Susumu TanakaKenji YamamuraManabu Obori
    • Susumu TanakaKenji YamamuraManabu Obori
    • C21D936
    • F16C33/62C22C38/001C22C38/18C22C38/22C22C38/44C22C38/52F16C33/30F16C33/32F16C2240/54Y10S148/906Y10S384/912
    • An inexpensive rolling apparatus improved in resistance to fretting, acoustic performance, resistance to corrosion, life and workability is provided. At least one of an outer member, an inner member and rolling elements of the apparatus is formed of an alloy steel containing 1.5% by weight or less of C, 10% to 20% by weight of Cr, 0.1% to 0.8% by weight of Mn, 0.1% to 1.0% by weight of Si and less than 0.2% by weight of N, particularly, at least one of the outer member, the inner member and the rolling elements is formed of a martensitic stainless steel containing 0.6% by weight or less of C, 10% to 14% by weight of Cr, 0.1% to 0.8% by weight of Mn, 0.1% to 1.0% by weight of Si, less than 0.2% by weight of N, 0.5% by weight or less of Mo, 0.2% by weight or less of V, and Fe and inevitable components as the balance, wherein the relationship between the content of C and that of Cr satisfies C %≦−0.05 Cr %+1.41; the relationship between a specific relational equation eq1 indicating the content of elements accelerating the conversion of the raw material to ferrite, taken as (eq1)=Cr %+Si %+1.5 Mo %+3.5V %, and a specific relational equation eq2 indicating the content of elements accelerating the conversion of the raw material to austenite, taken as (eq2)=C %+0.83 N %+0.1 Mn %, satisfies (eq2)≧0.04×(eq1)−0.39, (eq1)≦14.0 and (eq2)≦0.8; and the total content of C and N satisfies C+N≧0.45%.
    • 提供了耐磨性,声学性能,耐腐蚀性,寿命和可加工性的廉价滚动装置。 该装置的外部构件,内部构件和滚动体中的至少一个由含有1.5重量%以下的C,10重量%〜20重量%的Cr,0.1重量%〜0.8重量% 的Mn,0.1〜1.0重量%的Si和小于0.2重量%的N,特别地,外部构件,内部构件和滚动体中的至少一个由马氏体不锈钢形成,所述马氏体不锈钢含有0.6% 重量以下的C,10〜14重量%的Cr,0.1〜0.8重量%的Mn,0.1〜1.0重量%的Si,小于0.2重量%的N,0.5重量% 少量的Mo,0.2重量%以下的V,Fe和不可避免的成分作为余量,其中C与Cr的含量之间的关系满足C%<= -0.05 Cr%+ 1.41; 以(eq1)= Cr%+ Si%+ 1.5Mo%+ 3.5V%表示加速原料转化为铁素体的元素含量的特定关系式eq1与特定关系式eq2之间的关系, (eq2)= C%+ 0.83N%+ 0.1Mn%,将原料转化为奥氏体的元素的含量满足(eq2)> = 0.04x(eq1)-0.39,(eq1)<= 14.0和(eq2)<= 0.8; C和N的总含量满足C + N> = 0.45%。
    • 14. 发明授权
    • Rolling member
    • 滚动会员
    • US06228184B1
    • 2001-05-08
    • US09576265
    • 2000-05-24
    • Susumu TanakaKenji YamamuraManabu Obori
    • Susumu TanakaKenji YamamuraManabu Obori
    • C22C3818
    • F16C33/62C22C38/001C22C38/18C22C38/22C22C38/44C22C38/52F16C33/30F16C33/32F16C2240/54Y10S148/906Y10S384/912
    • An inexpensive rolling apparatus improved in resistance to fretting, acoustic performance, resistance to corrosion, life and workability is provided. At least one of an outer member, an inner member and rolling elements of the apparatus is formed of an alloy steel containing 1.5% by weight or less of C, 10% to 20% by weight of Cr, 0.1% to 0.8% by weight of Mn, 0.1% to 1.0% by weight of Si and less than 0.2% by weight of N, particularly, at least one of the outer member, the inner member and the rolling elements is formed of a martensitic stainless steel containing 0.6% by weight or less of C, 10% to 14% by weight of Cr, 0.1% to 0.8% by weight of Mn, 0.1% to 1.0% by weight of Si, less than 0.2% by weight of N, 0.5% by weight or less of Mo, 0.2% by weight or less of V, and Fe and inevitable components as the balance, wherein the relationship between the content of C and that of Cr satisfies C %≦−0.05 Cr %+1.41; the relationship between a specific relational equation eq1 indicating the content of elements accelerating the conversion of the raw material to ferrite, taken as (eq1)=Cr %+Si %+1.5 Mo %+3.5 V %, and a specific relational equation eq2 indicating the content of elements accelerating the conversion of the raw material to austenite, taken as (eq2)=C %+0.83 N %+0.12 Mn %, satisfies (eq2)≧0.04×(eq1)−0.39, (eq1)≦14.0 and (eq2)≦0.8; and the total content of C and N satisfies C+N≧0.45%.
    • 提供了耐磨性,声学性能,耐腐蚀性,寿命和可加工性的廉价滚动装置。 该装置的外部构件,内部构件和滚动体中的至少一个由含有1.5重量%以下的C,10重量%〜20重量%的Cr,0.1重量%〜0.8重量% 的Mn,0.1〜1.0重量%的Si和小于0.2重量%的N,特别地,外部构件,内部构件和滚动体中的至少一个由马氏体不锈钢形成,所述马氏体不锈钢含有0.6% 重量以下的C,10〜14重量%的Cr,0.1〜0.8重量%的Mn,0.1〜1.0重量%的Si,小于0.2重量%的N,0.5重量% 少量的Mo,0.2重量%以下的V,Fe和不可避免的成分作为余量,其中C与Cr的含量之间的关系满足C%<= -0.05 Cr%+ 1.41; 以(eq1)= Cr%+ Si%+ 1.5Mo%+ 3.5V%表示加速原料转化为铁素体的元素的含量的特定关系式eq1与特定关系式eq2之间的关系, (eq2)= C%+ 0.83 N%+ 0.12 Mn%的元素的加入元素的含量满足(eq2)> = 0.04x(eq1)-0.39,(eq1)<= 14.0和(eq2)<= 0.8; C和N的总含量满足C + N> = 0.45%。
    • 15. 发明授权
    • Rolling bearing
    • 滚动轴承
    • US5873956A
    • 1999-02-23
    • US803882
    • 1997-02-21
    • Susumu TanakaKenji YamamuraManabu Ohori
    • Susumu TanakaKenji YamamuraManabu Ohori
    • C21D6/04C21D9/36C21D9/40C22C38/00C22C38/18C22C38/34F16C33/30F16C33/62C23C8/32
    • C21D9/40C22C38/18C22C38/34F16C33/30F16C33/62C21D6/04C21D9/36Y10S148/906
    • In order to provide rolling bearings of high performance using case hardened stainless steels that are superior to the conventional martensite base stainless steels in terms of corrosion resistance, rolling fatigue strength and wear resistance and which also have high core toughness, at least one member of the rolling bearing selected from among the inner race, the outer race and the rolling elements is made of an alloy steel consisting essentially of less than 0.5 wt % C, 8.0 to 20.0 wt % Cr, 0.1 to 1.5 wt % Mn, 0.1 to 2.0 wt % Si and the balance of Fe and incidental impurity elements; the relationship between the C and Cr contents satisfies 0.04 Cr (wt %)-0.39.ltoreq.C (wt %).ltoreq.-0.05 Cr (wt %)+1.41; the bearing also has a surface layer that is formed by nitriding or carbonitriding at a temperature below Ac.sub.1, subsequent heating at a temperature of 900.degree. to 1,200.degree. C., hardening, a subzero treatment and tempering.
    • 为了提供耐腐蚀性,滚动疲劳强度和耐磨性方面优于传统马氏体不锈钢的表面硬化不锈钢的高性能滚动轴承,并且还具有高的芯部韧性,至少有一个部件 从内圈,外圈和滚动体中选择的滚动轴承由基本上由小于0.5重量%C,8.0重量%〜20.0重量%的Cr,0.1〜1.5重量%的Mn,0.1〜2.0重量% %Si和余量的Fe和杂质元素; C和Cr含量之间的关系满足0.04 Cr(wt%) - 0.39(C)(wt%)≤0.05Cr(wt%)+ 1.41; 轴承还具有通过在低于Ac1的温度下氮化或碳氮共渗形成的表面层,随后在900-1200℃的温度下加热,硬化,零度处理和回火。
    • 17. 发明授权
    • Rolling bearing for high-speed rotation at high temperatures
    • 滚动轴承用于在高温下高速旋转
    • US5560787A
    • 1996-10-01
    • US507748
    • 1995-07-26
    • Masaaki TakagiManabu OhoriKyozaburo FurumuraKenji Yamamura
    • Masaaki TakagiManabu OhoriKyozaburo FurumuraKenji Yamamura
    • C21D9/36C21D9/40C23C8/22C23C8/32F16C33/30F16C33/62
    • F16C33/62C21D9/36F16C33/30C21D9/40Y10S148/906
    • One of component parts of an inner race, an outer race and rolling elements of a rolling bearing is composed of a bearing material that is prepared by working a high-speed steel, carburizing or carbonitriding the wrought steel in a temperature range from 800.degree. C. to less than 1200.degree. C. and subsequently hardening and tempering the carburized or carbonitrided steel, the steel composing of 0.2 wt %.ltoreq.C.ltoreq.2.3 wt %, Si.ltoreq.1.0 wt %, Mn.ltoreq.1.0 wt %, 2.0 wt %.ltoreq.Cr.ltoreq.7.0 wt %, 1.5 wt %.ltoreq.W.ltoreq.22.0 wt %, Mo.ltoreq.10.0 wt %, 0.5.ltoreq.V.ltoreq.6.0 wt %, Co.ltoreq.18.0 wt %, the balance Fe and incidental impurities. By carburizing or carbonitriding the steel at low temperatures less than 1,200.degree. C., not only high core toughness is insured but also the dissolved C or N in the surface is compensated to increase the hot strength of the steel and the compressive stress that remains in the surface after heat treatment, so that the rolling bearing that rotate at high speed and high temperatures of more 400.degree. C. extends the service life.
    • 内圈,外圈和滚动轴承的滚动元件的一部分由轴承材料组成,该轴承材料通过在800℃的温度范围内加工高速钢,渗碳或碳氮共渗制备而成 至低于1200℃,随后硬化​​和回火渗碳或碳氮共渗钢,组成0.2wt%C = 2.3wt%的Si,1.0wt%的Mn,1.0wt 重量%,2.0重量%Cr = 7.0重量%,1.5重量%W = 22.0重量%,Mo 10.0重量%,0.5重量%6.0重量% ,Co = 18.0wt%,余量为Fe和杂质。 通过在低于1200℃的低温下对钢进行渗碳或碳氮共渗,不仅保证了高的核心韧性,还补偿了表面中溶解的C或N,以增加钢的热强度和保持在 热处理后的表面,使滚动轴承在高速高温下转动400℃以上,延长使用寿命。
    • 20. 发明授权
    • Rolling member
    • 滚动会员
    • US6086686A
    • 2000-07-11
    • US60810
    • 1998-04-16
    • Susumu TanakaKenji YamamuraManabu Obori
    • Susumu TanakaKenji YamamuraManabu Obori
    • C22C38/00C22C38/18C22C38/22C22C38/44C22C38/52F16C33/30F16C33/32F16C33/34F16C33/62C22C38/02C22C38/04
    • F16C33/62C22C38/001C22C38/18C22C38/22C22C38/44C22C38/52F16C33/30F16C33/32F16C33/34Y10S148/906Y10S384/912
    • An inexpensive rolling apparatus improved in resistance to fretting, acoustic performance, resistance to corrosion, life and workability is provided. At least one of an outer member, an inner member and rolling elements of the apparatus is formed of an alloy steel containing 1.5% by weight or less of C, 10% to 20% by weight of Cr, 0.1% to 0.8% by weight of Mn, 0.1% to 1.0% by weight of Si and less than 0.2% by weight of N, particularly, at least one of the outer member, the inner member and the rolling elements is formed of a martensitic stainless steel containing 0.6% by weight or less of C, 10% to 14% by weight of Cr, 0.1% to 0.8% by weight of Mn, 0.1% to 1.0% by weight of Si, less than 0.2% by weight of N, 0.5% by weight or less of Mo, 0.2% by weight or less of V, and Fe and inevitable components as the balance, wherein the relationship between the content of C and that of Cr satisfies C%.ltoreq.-0.05 Cr%+1.41; the relationship between a specific relational equation eq1 indicating the content of elements accelerating the conversion of the raw material to ferrite, taken as (eq1)=Cr%+Si%+1.5 Mo%+3.5 V%, and a specific relational equation eq2 indicating the content of elements accelerating the conversion of the raw material to austenite, taken as (eq2)=C%+0.83 N%+0.12 Mn%, satisfies (eq2).gtoreq.0.04.times.(eq1)-0.39, (eq1).ltoreq.14.0 and (eq2).ltoreq.0.8; and the total content of C and N satisfies C+N.gtoreq.0.45%.
    • 提供了耐磨性,声学性能,耐腐蚀性,寿命和可加工性的廉价滚动装置。 该装置的外部构件,内部构件和滚动体中的至少一个由含有1.5重量%以下的C,10重量%〜20重量%的Cr,0.1重量%〜0.8重量% 的Mn,0.1〜1.0重量%的Si和小于0.2重量%的N,特别地,外部构件,内部构件和滚动体中的至少一个由马氏体不锈钢形成,所述马氏体不锈钢含有0.6% 重量以下的C,10〜14重量%的Cr,0.1〜0.8重量%的Mn,0.1〜1.0重量%的Si,小于0.2重量%的N,0.5重量% 少量的Mo,0.2重量%以下的V,Fe和不可避免的成分作为余量,其中C与Cr的含量之间的关系满足C%≤0.05Cr%+ 1.41; 以(eq1)= Cr%+ Si%+ 1.5Mo%+ 3.5V%表示加速原料转化为铁素体的元素的含量的特定关系式eq1与特定关系式eq2之间的关系, (eq2)= C%+ 0.83N%+ 0.12Mn%,将原料转化为奥氏体的元素的含量满足(eq2)> / = 0.04×(eq1)-0.39,(eq1)< /=14.0和(eq2) = 0.45%。