    • 14. 发明申请
    • Perfluoroelastomer seal material
    • 全氟弹性体密封材料
    • US20070037922A1
    • 2007-02-15
    • US10572779
    • 2004-09-21
    • Hiroyuki TanakaTsuyoshi Noguchi
    • Hiroyuki TanakaTsuyoshi Noguchi
    • C08L27/12
    • C09K3/1009F16J15/102Y10T428/24355
    • The present invention provides a perfluoroelastomer seal material in which adhesive strength, contamination, corrosion and color change of a contacted surface with a seal material are improved, and an amount of an uncrosslinked polymer component is at most 1% by weight, measured under specific conditions, and a process for preparing the same. The present invention relates to a perfluoroelastomer seal material, wherein a rate of weight decrease is at most 1% by weight when the seal material is immersed into perfluoro(tri-n-butyl)amine at 60° C. for 70 hours and is dried at 90° C. for 5 hours, 125° C. for 5 hours and 200° C. for 10 hours after taken out of the emersion. And, the present invention also relates to a process for preparing a perfluoroelastomer seal material comprising a step of treating with a solvent having at least 50 % of a swelling rate based on said molded article, when said molded article is immersed at 60° C. for 70 hours.
    • 本发明提供了一种全氟弹性体密封材料,其中改善了与密封材料的接触表面的粘合强度,污染物,腐蚀和颜色变化,并且在特定条件下测量的未交联聚合物组分的量为至多1重量% ,及其制备方法。 全氟弹性体密封材料技术领域本发明涉及一种全氟弹性体密封材料,其中当密封材料在60℃下浸入全氟(三正丁基)胺中70小时时,其重量减少率至多为1重量%,并干燥 在90℃,5小时,125℃,5小时和200℃,10分钟后脱出。 另外,本发明还涉及一种全氟弹性体密封材料的制造方法,其特征在于,在将所述成形体浸渍于60℃时,使用具有基于所述成型体的至少50%的溶胀率的溶剂进行处理的工序。 70个小时。
    • 18. 发明授权
    • Molded elastomer
    • 成型弹性体
    • US06515064B1
    • 2003-02-04
    • US09889009
    • 2001-07-06
    • Hiroyuki TanakaMasanori HasegawaTsuyoshi NoguchiKatsuhiko Higashino
    • Hiroyuki TanakaMasanori HasegawaTsuyoshi NoguchiKatsuhiko Higashino
    • C08K304
    • C08J5/00C08J2321/00C08K3/04C08L21/00
    • To provide an elastomer molded article for a semiconductor manufacturing equipment which not only has cleanliness required but also has an excellent plasma resistance and an excellent property of metal-elution inhibition. The elastomer molded article is obtained by crosslinking a crosslinkable elastomer composition comprising a crosslinkable elastomer component and a carbon black filler having an average particle size of not more than 700 &mgr;m and an impurity metal content measured by an ashing analysis method of not more than 300 ppm and has an impurity metal content measured by an ashing analysis method of not more than 100 ppm. An increasing rate of particles generated by irradiating oxygen plasma to the article is not more than 500% or an amount of impurity metals extracted from the article with a 50% aqueous solution of HF is not more than 500 ppb.
    • 为了提供一种用于半导体制造设备的弹性体模塑制品,其不仅需要清洁度,而且具有优异的等离子体电阻和优异的金属洗脱抑制性能。 弹性体成型体是将包含交联性弹性体成分和平均粒径为700μm以下的炭黑填料的交联性弹性体组合物和通过灰化分析法测定的杂质金属含量为300ppm以下, 并且通过灰化分析方法测定的不大于100ppm的杂质金属含量。 通过向制品照射氧等离子体而产生的颗粒的增加率不大于500%,或者用50%的HF水溶液从制品中提取的杂质金属的量不超过500ppb。
    • 19. 发明授权
    • Perfluoroelastomer seal material
    • 全氟弹性体密封材料
    • US07834096B2
    • 2010-11-16
    • US10572779
    • 2004-09-21
    • Hiroyuki TanakaTsuyoshi Noguchi
    • Hiroyuki TanakaTsuyoshi Noguchi
    • C08L27/12
    • C09K3/1009F16J15/102Y10T428/24355
    • The present invention provides a perfluoroelastomer seal material in which adhesive strength, contamination, corrosion and color change of a contacted surface with a seal material are improved, and an amount of an uncrosslinked polymer component is at most 1% by weight, measured under specific conditions, and a process for preparing the same. The present invention relates to a perfluoroelastomer seal material, wherein a rate of weight decrease is at most 1% by weight when the seal material is immersed into perfluoro(tri-n-butyl)amine at 60° C. for 70 hours and is dried at 90° C. for 5 hours, 125° C. for 5 hours and 200° C. for 10 hours after taken out of the emersion. And, the present invention also relates to a process for preparing a perfluoroelastomer seal material comprising a step of treating with a solvent having at least 50 % of a swelling rate based on said molded article, when said molded article is immersed at 60° C. for 70 hours.
    • 本发明提供了一种全氟弹性体密封材料,其中改善了与密封材料的接触表面的粘合强度,污染物,腐蚀和颜色变化,并且在特定条件下测量的未交联聚合物组分的量为至多1重量% ,及其制备方法。 全氟弹性体密封材料技术领域本发明涉及一种全氟弹性体密封材料,其中当密封材料在60℃下浸入全氟(三正丁基)胺中70小时时,其重量减少率至多为1重量%,并干燥 在90℃,5小时,125℃,5小时和200℃,10分钟后脱出。 另外,本发明还涉及一种全氟弹性体密封材料的制造方法,其特征在于,在将所述成形体浸渍于60℃时,使用具有基于所述成型体的至少50%的溶胀率的溶剂进行处理的工序。 70个小时。